Effect of La2O3 on microstructure and properties of Fe-based alloy coatings by laser cladding

被引:21
作者
Wang, Qiang [1 ,2 ]
Yang, Ju [1 ,2 ]
Niu, Wenjuan [1 ,2 ]
Li, Yangyang [1 ,2 ]
Mao, Xuan [1 ,2 ]
Wang, Yonggang [1 ,2 ]
Zhang, Kang [1 ,2 ]
机构
[1] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710055, Peoples R China
[2] Shaanxi Res Ctr Met Engn, Xian 710055, Peoples R China
来源
OPTIK | 2021年 / 245卷
关键词
Laser cladding; Fe-based alloy; Microstructure; Tribological properties; La2O3; HIGH-TEMPERATURE OXIDATION; WEAR-RESISTANCE; HEAT-TREATMENT; CORROSION; Y2O3; BEHAVIOR; HARDNESS;
D O I
10.1016/j.ijleo.2021.167653
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
One of the challenges limiting the application of laser cladded Fe-based coatings is the coarse columnar grains formed during the process. In order to improve the microstructure homogeneity of laser cladded coatings, Fe-based alloy (Fe78.5Cr15.6Ni4.0Si0.7) composite coatings with different La2O3 additions were prepared on the surface of 45-steel substrate by laser cladding. The effect of La2O3 content on the microstructure and properties composite coatings were systematically studied. X-ray diffractometer (XRD) and scanning electron microscope (SEM) were used to analyze the phase structure and microstructural evolution of Fe-based alloy composite coatings, and the hardness and tribological properties were measured by the microhardness tester and ball on disc wear tester, respectively. The results show that the addition of La2O3 plays the role of grain refinement, and certain amount of addition can completely eliminate the coarse columnar grains. Due to the fine-grain strengthening and dispersion strengthening of La2O3, the hardness and wear resistance of Fe-based alloy composite coatings have been improved. Especially, when the content of La2O3 is 1 wt%, the hardness increases to 3.1 times and the wear loss decreases to 27.7%, compared with the substrate material. The wear surface of composite coating with 1 wt% La2O3 suffered minor damage, and the wear mechanism is slightly abrasive wear. In contrast, higher amount of 2 wt% La2O3 addition has less effective grain refining where some columnar grains appear on the interface, and the hardness and wear resistance of composite coatings decrease as well. Meanwhile, the wear mechanism is transformed into a mixed mode of abrasive wear and adhesive wear.
引用
收藏
页数:10
相关论文
共 36 条
  • [1] Laser cladding of Inconel 625 wire for corrosion protection
    Abioye, T. E.
    McCartney, D. G.
    Clare, A. T.
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 217 : 232 - 240
  • [2] Formation mechanisms of Ni-Al intermetallics during heat treatment of Ni coating on 6061 Al substrate
    Adabi, Mohsen
    Amadeh, Ahmad Ali
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (12) : 3959 - 3966
  • [3] Effect of nano-CeO2 on microstructure and wear resistance of Co-based coatings
    Ding, Lin
    Hu, Shengsun
    [J]. SURFACE & COATINGS TECHNOLOGY, 2015, 276 : 565 - 572
  • [4] Influence of La2O3 addition on nano indentation hardness and residual stress of Stellite 6 coating prepared by plasma cladding
    Fang, Yongchao
    Cui, Xiufang
    Cai, Zhaobing
    Wang, Chang
    Jin, Guo
    [J]. JOURNAL OF RARE EARTHS, 2018, 36 (08) : 873 - 878
  • [5] Laser cladding assisted by induction heating of Ni-WC composite enhanced by nano-WC and La2O3
    Farahmand, Parisa
    Liu, Shuang
    Zhang, Zhe
    Kovacevic, Radovan
    [J]. CERAMICS INTERNATIONAL, 2014, 40 (10) : 15421 - 15438
  • [6] Investigation on microstructure and wear characteristic of laser cladding Fe-based alloy on wheel/rail materials
    Fu, Z. K.
    Ding, H. H.
    Wang, W. J.
    Liu, Q. Y.
    Guo, J.
    Zhu, M. H.
    [J]. WEAR, 2015, 330 : 592 - 599
  • [7] Effects of sulfur impurity on the scale adhesion behavior of a desulfurized Ni-based superalloy aluminized by chemical vapor deposition
    Lee, WY
    Zhang, Y
    Wright, IG
    Pint, BA
    Liaw, PK
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1998, 29 (03): : 833 - 841
  • [8] Enhanced corrosion and wear resistance properties of carbon fiber reinforced Ni-based composite coating by laser cladding
    Lei, Jianbo
    Shi, Chuan
    Zhou, Shengfeng
    Gu, Zhenjie
    Zhang, Lai-Chang
    [J]. SURFACE & COATINGS TECHNOLOGY, 2018, 334 : 274 - 285
  • [9] Effects of La2O3 on the microstructure and property of laser cladding Ni-based ceramic coating
    Li, Meiyan
    Han, Bin
    Wang, Yong
    Pu, Kejin
    [J]. OPTIK, 2017, 130 : 1032 - 1037
  • [10] Effects of heterogeneity and coarse secondary phases on mechanical properties of 7050-T7451 aluminum alloy friction stir welding joint
    Liu, Yong
    Deng, Caiyan
    Gong, Baoming
    Bai, Yanan
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 764