Synthesis by TEA sol-gel method and electrochemical properties of Li4Ti5O12 anode material for lithium-ion battery
被引:100
作者:
Hao, YJ
[1
]
Lai, QY
[1
]
Xu, ZH
[1
]
Liu, XQ
[1
]
Ji, XY
[1
]
机构:
[1] Sichuan Univ, Chem Coll, Chengdu 610064, Peoples R China
关键词:
TEA;
sol-gel method;
Li4Ti5O12;
anode material;
lithium-ion battery;
D O I:
10.1016/j.ssi.2005.02.010
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
Anode material Li4Ti5O12 for lithium-ion batteries have been synthesized by a novel sol-gel method with triethanolamine(TEA) as a chelating agent and LiAc - 2H(2)O and Tetrabutyl titanate [Ti (OC4H9)(4)] as starting materials. Various initial conditions were studied in order to find the optimal conditions for the synthesis of Li4Ti5O12. The as-prepared samples have been characterized by means of XRD, IR and SEM. Its electrochemical behavior was evaluated in a liquid electrolyte in lithium-ion batteries. These analyses indicated that the prepared Li-Ti-O powders belonged to a spinel structure and had a uniform morphology with average particle size from 223 to 105 nm with the increase in TEA content. At 1.55 V (vs. Li), the Li4Ti5O12 electrode with the ratio of TEA to Ti ions 0.8 exhibited an initial discharge capacity of 168 mA h/g and a subsequent charge capacity of 151 mA h/g. The results of cyclic voltammetry for Li4Ti5O12 showed that at the potential range from 1.5 to 1.7 V (vs. Li), there was a pair of reversible redox peaks correspond to the process of Li+ intercalation and deintercalation in the spinel Li-Ti-O oxides. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:1201 / 1206
页数:6
相关论文