Low-temperature sintering, structure transition and dielectrical properties of Ba0.85Ca0.15Ti0.9Zr0.1O3 with Na0.5Bi0.5TiO3 addition

被引:5
作者
Yao, Mouteng [1 ]
Pu, Yongping [1 ]
Gao, Ziyan [1 ]
Zheng, Hanyu [1 ]
机构
[1] Shaanxi Univ Sci & Technol, Sch Mat Sci & Engn, Xian 710021, Peoples R China
基金
中国国家自然科学基金;
关键词
Solid state method; Perovskite; Diffuse phase transition; Ba0.85Ca0.15Ti0.9Zr0.1O3; HIGH PIEZOELECTRIC COEFFICIENT; RELAXOR BEHAVIOR; CERAMICS; RANGE; RAMAN;
D O I
10.1016/j.ceramint.2016.03.226
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Na0.5Bi0.5TiO3-modified Ba0.85Ca0.15Ti0.9Zr0.1O3 ceramics were prepared by solid state route and their structural and dielectric properties were investigated. The sintering temperature of BCTZ ceramics has been significantly decreased from 1460 degrees C to 1280 degrees C with NBT addition. All samples showed a pure perovskite structure and a stable solid solution has been formed between BCTZ and NBT. Some tetragonal phase gradually transformed to rhombohedral or cubic phase with the addition of NBT. Dielectric peak gradually becomes broader, revealing that the diffuser behavior was enhanced. The prominent superimposed loss peaks related to thermally activated relaxation process. The values of activation energy of the relaxation process are 1.034, 1.285, 1.308 and 1353 eV, which could be associated with the migration of oxygen vacancies. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:10922 / 10928
页数:7
相关论文
共 44 条
  • [1] Oxygen-vacancy-related low-frequency dielectric relaxation and electrical conduction in Bi:SrTiO3
    Ang, C
    Yu, Z
    Cross, LE
    [J]. PHYSICAL REVIEW B, 2000, 62 (01) : 228 - 236
  • [2] Phase formation and dielectric study of Bi doped BaTi0.75Zr0.25O3 ceramic
    Badapanda, T.
    Rout, S. K.
    Panigrahi, S.
    Sinha, T. P.
    [J]. CURRENT APPLIED PHYSICS, 2009, 9 (04) : 727 - 731
  • [3] Raman and dielectric investigation of (Ba0.9-xSrxCa0.1)(Ti0.8Zr0.2)O3 ferroelectric ceramics
    Bahri, Fathi
    Khemakhem, Hamadi
    [J]. CERAMICS INTERNATIONAL, 2014, 40 (06) : 7909 - 7913
  • [4] A modified lead-free piezoelectric BZT-xBCT system with higher TC
    Bao, Huixin
    Zhou, Chao
    Xue, Dezhen
    Gao, Jinghui
    Ren, Xiaobing
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2010, 43 (46)
  • [5] Recent progress in relaxor ferroelectrics with perovskite structure
    Bokov, AA
    Ye, ZG
    [J]. JOURNAL OF MATERIALS SCIENCE, 2006, 41 (01) : 31 - 52
  • [6] Chen J. D., 1982, PHYS DIELECTRIC
  • [7] Lead-free (Ba0.85Ca0.15)(Ti0.9Zr0.1)O3-CeO2 ceramics with high piezoelectric coefficient obtained by low-temperature sintering
    Cui, Yerang
    Liu, Xinyu
    Jiang, Minhong
    Zhao, Xiayan
    Shan, Xu
    Li, Wenhua
    Yuan, Changlai
    Zhou, Changrong
    [J]. CERAMICS INTERNATIONAL, 2012, 38 (06) : 4761 - 4764
  • [8] High-field dielectric properties and Raman spectroscopic investigation of the ferroelectric-to-relaxor crossover in BaSnxTi1-xO3 ceramics
    Deluca, Marco
    Stoleriu, Laurentiu
    Curecheriu, Lavinia Petronela
    Horchidan, Nadejda
    Ianculescu, Adelina Carmen
    Galassi, Carmen
    Mitoseriu, Liliana
    [J]. JOURNAL OF APPLIED PHYSICS, 2012, 111 (08)
  • [9] Micro-Raman scattering and dielectric investigations of phase transition behavior in the BaTiO3-BaZrO3 system
    Dobal, PS
    Dixit, A
    Katiyar, RS
    Yu, Z
    Guo, R
    Bhalla, AS
    [J]. JOURNAL OF APPLIED PHYSICS, 2001, 89 (12) : 8085 - 8091
  • [10] The Effect of Electric Poling on the Performance of Lead-Free (1-x)Ba(Zr0.2Ti0.8)O3-x(Ba0.7Ca0.3)TiO3 Piezoceramics
    Ehmke, Matthias C.
    Glaum, Julia
    Hoffman, Mark
    Blendell, John E.
    Bowman, Keith J.
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (12) : 3805 - 3811