An investigation on the circumferential surface crack growth in steel pipes subjected to fatigue bending

被引:25
|
作者
Li, Zongchen [1 ]
Jiang, Xiaoli [1 ]
Hopman, Hans [1 ]
Zhu, Ling [2 ,3 ]
Liu, Zhiping [4 ]
机构
[1] Delft Univ Technol, Dept Maritime & Transport Technol, NL-2628 CD Delft, Netherlands
[2] Wuhan Univ Technol, Sch Transportat, Dept Naval Architecture, Wuhan 430063, Peoples R China
[3] Wuhan Univ Technol, Sch Transportat, Dept Ocean & Struct Engn, Wuhan 430063, Peoples R China
[4] Wuhan Univ Technol, Lab Intelligent Manufacture & Control, Wuhan 430063, Peoples R China
关键词
Steel pipes; Circumferential surface crack; Surface crack growth rate; Analytical method; Structural integrity; STRESS;
D O I
10.1016/j.tafmec.2019.102403
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In the present paper, we propose an analytical method to calculate the Stress Intensity Factor (SIF) of circumferential surface cracks in steel pipes subjected to bending. In light of pipe geometry and bending load case, the analytical formula is raised by introducing new bending correction factors and new geometry correction factors on the basis of the Newman-Raju's method. The bending correction factors are deduced based on the bending stress gradient, while the geometry correction factors are determined by parametric studies for internal surface cracks and external surface cracks respectively. Owing to a large data set requirement by the parametric studies, three-dimensional finite element (FE) models of evaluating SIFs of circumferential surface cracks are developed. The FE method is validated to ensure that it could provide accurate SIF estimations. Analytical verification is conducted which shows that the SIF evaluated by the proposed analytical method match well with the results evaluated by the recommended analytical method. Then experimental investigations of external surface crack growth in offshore steel pipe subjected to fatigue bending are implemented to further validate the analytical method of predicting surface crack growth rate. The analytical results match well with the test results and the available experimental data from literature, indicating that the analytical method can be used for practical purposes and facilitate the crack growth evaluation and residual fatigue life prediction of cracked steel pipes.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Experimental Investigation and Finite Element Analysis of Fatigue Crack Growth in Pipes Containing a Circumferential Semi-elliptical Crack Subjected to Bending
    A. R. Shahani
    M. M. Shodja
    A. Shahhosseini
    Experimental Mechanics, 2010, 50 : 563 - 573
  • [2] Experimental Investigation and Finite Element Analysis of Fatigue Crack Growth in Pipes Containing a Circumferential Semi-elliptical Crack Subjected to Bending
    Shahani, A. R.
    Shodja, M. M.
    Shahhosseini, A.
    EXPERIMENTAL MECHANICS, 2010, 50 (05) : 563 - 573
  • [3] Fatigue Crack Growth and Fracture Studies on Stainless Steel Straight Pipes Having Circumferential Surface Crack
    Saravanan, M.
    Vishnuvardhan, S.
    Murthy, A. Ramachandra
    Gandhi, P.
    Mandal, Debasish
    Singh, P. K.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2024, 24 (03) : 1166 - 1180
  • [4] Fatigue crack growth and penetration behaviour in pipes subjected to bending load
    Yoo, YS
    Ahn, SH
    Ando, K
    LIFETIME MANAGEMENT AND EVALUATION OF PLANT, STRUCTURES AND COMPONENTS, 1998, : 159 - 166
  • [5] Circumferential inner fatigue crack growth and penetration behaviour in pipe subjected to a bending moment
    Yoo, YS
    Ando, K
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2000, 23 (01) : 1 - 8
  • [6] Circumferential inner fatigue crack growth and penetration behaviour in pipe subjected to a bending moment
    Yoo, Y.S.
    Ando, K.
    Fatigue and Fracture of Engineering Materials and Structures, 2000, 23 (01): : 1 - 8
  • [7] Fatigue crack growth and fracture studies on straight pipes with circumferential surface notch
    Structural Engineering Research Centre, Council of Scientific, Industrial Research Campus, Chennai-600 113, India
    不详
    J Struct Eng, 2008, 5 (374-379):
  • [8] Effect of surface crack dimension on very low cycle fatigue crack growth behavior of circumferential cracked pipes
    Song, Hyun-Seok
    Hwang, Jin-Ha
    Kim, Yun-Jae
    Kim, Jin-Weon
    THIN-WALLED STRUCTURES, 2023, 191
  • [9] APPROXIMATE CRACK OPENING DISPLACEMENT SOLUTIONS FOR LONG CIRCUMFERENTIAL CRACKS IN PIPES SUBJECTED TO BENDING AND TENSION
    YOO, SH
    PAN, J
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1992, 114 (02): : 178 - 180
  • [10] ESTIMATION OF THE DUCTILE UNSTABLE FRACTURE OF PIPE WITH A CIRCUMFERENTIAL SURFACE CRACK SUBJECTED TO BENDING
    KURIHARA, R
    UEDA, S
    STURM, D
    NUCLEAR ENGINEERING AND DESIGN, 1988, 106 (02) : 265 - 273