Relation between microstructure, composition, and hot cracking in Ti-stabilized austenitic stainless steel weldments

被引:33
作者
Shankar, V [1 ]
Gill, TPS
Terrance, ALE
Mannan, SL
Sundaresan, S
机构
[1] Indira Gandhi Ctr Atom Res, Mat Dev Grp, Kalpakkam 603102, Tamil Nadu, India
[2] Indira Gandhi Ctr Atom Res, Mat Characterizat Grp, Kalpakkam 603102, Tamil Nadu, India
[3] Indian Inst Technol, Dept Met Engn, Madras 600036, Tamil Nadu, India
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2000年 / 31卷 / 12期
关键词
D O I
10.1007/s11661-000-0090-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A stabilized, fully austenitic alloy D9, a 15Cr-15Ni-2Mo stainless steel with a titanium addition corresponding to UNS 38660, is a candidate material for the fuel-clad and wrapper applications of the Prototype Fast Breeder Reactor (PFBR). The fully austenitic microstructure and the presence of titanium in this alloy lead to high susceptibility to hot cracking during welding. The fusion-zone and the heat-affected zone (HAZ) cracking susceptibility of alloy D9 was studied at three titanium levels, 0.22, 0.32, and 0.42 pet. all other elements remaining constant. The longitudinal and transverse Varestraint (Transvarestraint) hot-cracking tests were used to evaluate fusion-zone and HAZ cracking. The results showed that titanium increases cracking in the fusion zone by 15 to 20 pet in the range of Ti levels studied. The microanalysis of fusion-zone hot cracks using electron probe microanalysis (EPMA) showed an enrichment of Ti, C, N, and S along cracks and in the interdendritic regions. The corresponding phases were identified as TiC, TiC0.3N0.7, and the carbosulfides Ti2CS and Ti4C2S2, which are believed to form eutectics with austenite to produce cracking. The amounts of these phases increased with increasing Ti content. In the HAZ, a similar relation between titanium level and cracking was found. The comparison of the weldability of the D9 with an FA mode type 321 revealed that Ti-bearing eutectics were responsible for a high degree of cracking irrespective of the solidification mode. The results show that in the D9, the ratio of Ti to C and N must be controlled to minimize cracking.
引用
收藏
页码:3109 / 3122
页数:14
相关论文
共 35 条
[1]  
Arata Y., 1977, Trans JWRI, V6, P105
[2]  
BROOKS JA, 1974, WELD J, V53, pS517
[3]  
CIESLAK MJ, 1991, WELD J, V70, pS49
[4]  
CULLEN TM, 1963, T ASME, V85, P151
[5]  
EGNELL L, 1970, P C WELDING CREEP RE, P144
[6]   VARIATION OF MC-CARBIDE GEOMETRY WITH LOCAL SOLIDIFICATION TIME IN CAST INCONEL 713-C ALLOY [J].
FEGAN, SC ;
KATTAMIS, TZ ;
MORRAL, JE ;
BHAMBRI, AK .
JOURNAL OF MATERIALS SCIENCE, 1975, 10 (07) :1266-1270
[7]  
Folkhard E., 1988, WELDING METALLURGY S
[8]  
GILL TPS, 1982, J MATER SCI, V17, P1513, DOI 10.1007/BF00752268
[9]  
GILL TPS, 1983, T INDIAN I METALS, V36, P269
[10]   DISLOCATION-CONTROLLED PRECIPITATION OF TIC PARTICLES AND THEIR RESISTANCE TO COARSENING [J].
KESTERNICH, W .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1985, 52 (04) :533-548