Reaction mechanism and kinetics in Ti3SiC2 synthesised from oxides

被引:1
|
作者
Atasoy, Ahmet [1 ]
机构
[1] Sakarya Univ, Fac Technol, Met & Mat Engn Dept, TR-54287 Sakarya, Turkey
关键词
Ti3SiC2 MAX phase; Aluminothermy; Kinetics; Activation; HIGH-TEMPERATURE SYNTHESIS; MAX PHASES; REDUCTION; COMPOSITES; MIXTURES; NITRIDES; TITANIUM; CARBIDES;
D O I
10.1007/s10973-018-7572-5
中图分类号
O414.1 [热力学];
学科分类号
摘要
The kinetic analysis of the formation of the Ti3SiC2 MAX phase by the aluminothermic reduction of TiO2 and SiO2 in the presence of carbon is being studied for the first time. The mixture was subjected to simultaneous thermogravimetry-differential thermal analysis in an argon atmosphere at different heating rates. It was observed that the aluminothermic reduction of the oxide content took place in two steps followed by formation of binary carbides to obtain nano-layered structure of 312 TiSiC phase. It was suggested that the formation of Ti3SiC2 occurred by the in situ reaction of intermediate phases such as TiSi, Ti2Si3, SiC and TiC. The kinetics parameters, including the activation energy for the Ti3SiC2 phase, were measured using the Kissinger method. The activation energy was found to be - 269 +/- 7 kJ mol(-1). It is also suggested that for preventing any oxidation of Ti3SiC2 phase, a high-grade purity or pre-purified-grade argon should be used.
引用
收藏
页码:363 / 370
页数:8
相关论文
共 50 条
  • [21] Contribution of plastic deformation of Ti3SiC2 to the crack deflection in the Al2O3/Ti3SiC2 composites
    Chin, Yuan-Liang
    Tuan, Wei-Hsing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (7-8): : 3270 - 3274
  • [22] Comparison of corrosion behavior of Ti3SiC2 and Ti3AlC2 in NaCl solutions with Ti
    Zhu, M.
    Wang, R.
    Chen, C.
    Zhang, H. B.
    Zhang, G. J.
    CERAMICS INTERNATIONAL, 2017, 43 (07) : 5708 - 5714
  • [23] Synthesis and properties of TiB2/Ti3SiC2 composites
    Islak, Bilge Yaman
    Candar, Duygu
    CERAMICS INTERNATIONAL, 2021, 47 (01) : 1439 - 1446
  • [24] Sintering of SiC/Ti3SiC2 composites with high SiC contents *
    Chahhou, B.
    Roger, J.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (16) : 7314 - 7325
  • [25] Influence of Cu on the mechanical and tribological properties of Ti3SiC2
    Dang, Wentao
    Ren, Shufang
    Zhou, Jiansong
    Yu, Youjun
    Li, Zhen
    Wang, Lingqian
    CERAMICS INTERNATIONAL, 2016, 42 (08) : 9972 - 9980
  • [26] Pressureless sintering kinetics analysis of Ti3SiC2 and Ti2AlC powdered MAX phases
    Gallego, Jose M. Cordoba
    DISCOVER MATERIALS, 2024, 4 (01):
  • [27] Synthesis of Ti3SiC2 from TiC and Si and its toughening mechanism with incorporated carbon fibers
    Tang, Chen
    Zhao, Kang
    Tang, Yufei
    Li, Fuping
    Meng, Qingnan
    CERAMICS INTERNATIONAL, 2021, 47 (18) : 26293 - 26300
  • [28] Effect of neutron irradiation on defect evolution in Ti3SiC2 and Ti2AlC
    Tallman, Darin J.
    He, Lingfeng
    Garcia-Diaz, Brenda L.
    Hoffman, Elizabeth N.
    Kohse, Gordon
    Sindelar, Robert L.
    Barsoum, Michel W.
    JOURNAL OF NUCLEAR MATERIALS, 2016, 468 : 194 - 206
  • [29] Synthesis and microstructure of the Ti3SiC2 in SiC matrix grown by chemical vapor deposition
    Lin, Tien-Chai
    Hon, Min-Hsiung
    CERAMICS INTERNATIONAL, 2008, 34 (03) : 631 - 638
  • [30] Effect of Ti3SiC2 on the ablation behavior and mechanism of Cf-C-SiC-Ti3SiC2 composites under oxyacetylene torch at 3000 °C
    Yaghobizadeh, Omid
    Sedghi, Arman
    Baharvandi, Hamid Reza
    CERAMICS INTERNATIONAL, 2019, 45 (01) : 777 - 785