Crystal and electronic structure changes during the charge-discharge process of Na4Co3(PO4)2P2O7

被引:28
|
作者
Moriwake, Hiroki [1 ]
Kuwabara, Akihide [1 ]
Fisher, Craig Aj. [1 ]
Nose, Masafumi [2 ]
Nakayama, Hideki [2 ]
Nakanishi, Shinji [2 ]
Iba, Hideki [2 ]
Ikuhara, Yuichi [1 ]
机构
[1] Japan Fine Ceram Ctr, Nanostruct Res Lab, Atsuta Ku, 2-4-1 Mutsuno, Nagoya, Aichi 4568587, Japan
[2] Toyota Motor Co Ltd, Shizuoka 4101193, Japan
关键词
Sodium-ion battery; Positive electrode; Battery voltage; Crystal structure; Charge-discharge process; First-principles calculations; SODIUM-ION BATTERIES; AUGMENTED-WAVE METHOD; CATHODE; LITHIUM; NA; STABILITY; DIFFUSION; VOLTAGE; STORAGE; MN;
D O I
10.1016/j.jpowsour.2016.07.006
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Sodium-ion batteries offer a potential solution to the problem of limited lithium resources, and the newly developed positive electrode material Na4Co3(PO4)(2)P2O7 is attracting significant attention due to its high rate, high capacity, and high voltage compared to other sodium-ion battery materials. However, details of its electronic structure and its charge discharge behavior are still uncertain. Here we report detailed first principles calculations of the desodiation behavior of Na4Co3(PO4)(2)P2O7 using the GGA U formalism of density functional theory. Assuming a stepwise desodiation process, removal of Na down to NaCo3(PO4)(2)P2O7 is found to be accompanied by oxidation of Co2+ to Co3+. Further removal of Na to give Co-3(PO4)(2)P2O7 requires oxidation of oxygen 2p orbitals in the P2O7 polyhedra instead of Co3+ being oxidized to Co4+. The holes thus formed are expected to be strongly self-trapped, rendering them immobile at room temperature. At the same time, a large volume shrinkage is observed during this last desodiation step, constricting the Na migration channels. These two factors may explain the difficulty encountered experimentally in removing all Na from Na4Co3(PO4)(2)P2O7. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:220 / 225
页数:6
相关论文
共 50 条
  • [1] Na4Co3(PO4)2P2O7: A novel storage material for sodium-ion batteries
    Nose, Masafumi
    Nakayama, Hideki
    Nobuhara, Kunihiro
    Yamaguchi, Hiroyuki
    Nakanishi, Shinji
    Iba, Hideki
    JOURNAL OF POWER SOURCES, 2013, 234 : 175 - 179
  • [2] Na4Co3(PO4)2P2O7/NC Composite as a Negative Electrode for Sodium-Ion Batteries
    Dwivedi, Pravin K.
    Sapra, Simranjot K.
    Pati, Jayashree
    Dhaka, Rajendra S.
    ACS APPLIED ENERGY MATERIALS, 2021, 4 (08) : 8076 - 8084
  • [3] Na4Co3(PO4)2P2O7 through Correlative Operando X-ray Diffraction and Electrochemical Impedance Spectroscopy
    Zarrabeitia, Maider
    Jauregui, Maria
    Sharma, Neeraj
    Pramudita, James C.
    Casas-Cabanas, Montse
    CHEMISTRY OF MATERIALS, 2019, 31 (14) : 5152 - 5159
  • [4] CoOx(OH)y/C nanocomposites in situ derived from Na4Co3(PO4)2P2O7 as sustainable electrocatalysts for water splitting
    Odynets, Ievgen V.
    Strutynska, Nataliia Yu.
    Li, Junzhi
    Han, Wei
    Zatovsky, Igor V.
    Klyui, N. I.
    DALTON TRANSACTIONS, 2018, 47 (44) : 15703 - 15713
  • [5] Low-Concentration Electrolyte Enables High-Voltage Positive Electrode Na4Co3(PO4)2P2O7 with Good Cycle Stability
    Zeng, Jingyao
    Guan, Dichang
    Wang, Weigang
    Tan, Xin
    Cao, Yanbing
    Peng, Zhongdong
    Hu, Guorong
    Du, Ke
    ACS APPLIED ENERGY MATERIALS, 2023, 6 (08): : 4238 - 4248
  • [6] Understanding the electrode - electrolyte interphase of high voltage positive electrode Na4Co3(PO4)2P2O7 for rechargeable sodium-ion batteries
    Zarrabeitia, Maider
    Casas-Cabanas, Montse
    Munoz-Marquez, Miguel angel
    ELECTROCHIMICA ACTA, 2021, 372
  • [7] Na4Co3(PO4)2P2O7, A NEW SODIUM COBALT PHOSPHATE CONTAINING A THREE-DIMENSIONAL SYSTEM OF LARGE INTERSECTING TUNNELS.
    Ruiz-Valero, C.
    Gutierrez-Puebla, E.
    Monge, A.
    Amador, U.
    Parada, C.
    Sanz, F.
    ACTA CRYSTALLOGRAPHICA A-FOUNDATION AND ADVANCES, 1996, 52 : C321 - C321
  • [8] Sodium-ion migration in secondary battery cathode material Na4Co3(PO4)2P2O7: A first-principles molecular dynamics study
    Moriwake, Hiroki
    Kuwabara, Akihide
    Fisher, Craig A. J.
    Kohama, Keiichi
    Nose, Masafumi
    Nakanishi, Shinji
    Iba, Hideki
    Ikuhara, Yuichi
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2023, 131 (07) : 279 - 283
  • [9] An Al-doped high voltage cathode of Na4Co3(PO4)2P2O7 enabling highly stable 4 V full sodium-ion batteries
    Liu, Xiaohao
    Tang, Linbin
    Li, Zhi
    Zhang, Jianhua
    Xu, Qunjie
    Liu, Haimei
    Wang, Yonggang
    Xia, Yongyao
    Cao, Yuliang
    Ai, Xinping
    JOURNAL OF MATERIALS CHEMISTRY A, 2019, 7 (32) : 18940 - 18949
  • [10] Electrochemical insertion of potassium ions in Na4Fe3(PO4)2P2O7 mixed phosphate
    Senthilkumar, Baskar
    Murugesan, Chinnasamy
    Sada, Krishnakanth
    Barpanda, Prabeer
    JOURNAL OF POWER SOURCES, 2020, 480