Cold rolled texture and microstructure in types 304 and 316L austenitic stainless steels

被引:36
|
作者
Wasnik, DN [1 ]
Gopalakrishnan, IK
Yakhmi, JV
Kain, V
Samajdar, I
机构
[1] Indian Inst Technol, Dept Met Engn & Mat Sci, Bombay 400076, Maharashtra, India
[2] Bhabha Atom Res Ctr, Novel Mat & Struct Chem Div, Bombay 400085, Maharashtra, India
[3] Bhabha Atom Res Ctr, Tech Phys & Prototype Engn Div, Bombay 400085, Maharashtra, India
[4] Bhabha Atom Res Ctr, Div Mat Sci, Bombay 400085, Maharashtra, India
关键词
deformation; texture; microstructure; microtexture; strain localizations; strain induced martensite; austenitic stainless steel; twin; Taylor Models;
D O I
10.2355/isijinternational.43.1581
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Two grades of austenitic stainless steel (ASS), types 304 (UNS S 30400) and 316L (UNS S 31603), were cold rolled to different reductions by unidirectional and by cross-rolling. The steels had reasonable difference in stacking fault energy (estimated respectively as 15 and 61 mJ/m(2) in types 304 and 316L) and also in starting (or pre-deformation) crystallographic texture-being relatively weak and reasonably strong in types 304 and 316L respectively. The cold rolling increased texturing in type 304, but not in type 316L ASS. The more significant effect of cold rolled texture development was in the relative increase of Brass ({011}<211>) against Copper ({112}<111>) and S ({231}<346>) orientations. In type 304 the increase in Brass was significant, while in type 316L the increase in Copper and S was stronger. This effect could be captured by Taylor type deformation texture simulations considering stronger twinning contributions in type 304-for example the respective 'best-fits' (in terms of matching the changes in the volume fractions of Brass against Copper and S) were obtained by full constraint Taylor model with 1 : 100 and 1 : 10 slip: twin activities in types 304 and 316L ASS respectively. Microstructural developments during cold rolling were generalized as strain induced martensite formation and developments of dislocation substructure. The former, as estimated by vibrating sample magnetometer (VSM), increased with cold reduction, being significantly more in type 304 and was also noticeably stronger in both grades under cross-rolling. The most significant aspect of substructural developments was the formation of strain localizations. These were observed as dense dislocation walls (DDWs), micro-bands (MBs) and twin lamellar structures (TLS). The TLS contribution gained significance at higher reductions and during cross-rolling, especially in type 304. Large misorientation development and the accompanying grain splittings were always associated with such strain localizations. Efforts to relate Taylor factor (M) and textural softening (dM/depsilon) values (of ideal texture components) with relative misorientation developments was, however, unsuccessful. No consistent trend could be established for any unique combination(s) of slip-twin in the respective alloys.
引用
收藏
页码:1581 / 1589
页数:9
相关论文
共 50 条
  • [21] Investigation of crack propagation resistance of 304L, 316L and 316L(N) austenitic steels in liquid sodium
    Barkia, B.
    Courouau, J. L.
    Perrin, E.
    Lorentz, V.
    Rivollier, M.
    Robin, R.
    Nicolas, L.
    Cabet, C.
    Auger, T.
    JOURNAL OF NUCLEAR MATERIALS, 2018, 507 : 15 - 23
  • [22] Strengthened microstructure and mechanical properties of austenitic 316L stainless steels by grain refinement and solute segregation
    Wang, Yurong
    Xiao, Buwei
    Liang, Xiaoyu
    Pen, Huabei
    Zhou, Jun
    Lin, Feng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 34 : 552 - 565
  • [23] Effect of Gadolinium Addition on Microstructure, Mechanical Properties and Corrosion Resistance of 316L Austenitic Stainless Steels
    H. Wang
    T. Wang
    J. Peng
    Physics of Metals and Metallography, 2021, 122 : 1640 - 1647
  • [24] Effect of Gadolinium Addition on Microstructure, Mechanical Properties and Corrosion Resistance of 316L Austenitic Stainless Steels
    Wang, H.
    Wang, T.
    Peng, J.
    PHYSICS OF METALS AND METALLOGRAPHY, 2021, 122 (14): : 1640 - 1647
  • [25] Hardness Indentation Size Effect Analysis of 316L Austenitic Stainless Steels during Cold Working
    Xue H.
    Li K.
    Wang S.
    Zhao K.
    Zhongguo Jixie Gongcheng/China Mechanical Engineering, 2019, 30 (01): : 105 - 112
  • [26] Influence of the microstructure on the corrosion resistance of plasma-nitrided austenitic stainless steel 304L and 316L
    Biehler, J.
    Hoche, H.
    Oechsner, M.
    Kaestner, P.
    Bunk, K.
    Braeuer, G.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2014, 45 (10) : 930 - 946
  • [27] Current status of AISI types 304 LN and 316 LN austenitic stainless steels
    Raj, B
    Mudali, UK
    Vasudevan, M
    Shankar, P
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2002, 55 (04): : 131 - 147
  • [28] Considerations for the weldability of types 304L and 316L stainless steel
    Korinko P.S.
    Malene S.H.
    Practical Failure Analysis, 2001, 1 (4) : 61 - 68
  • [29] Characteristics of Mechanical Properties and Microstructure for 316L Austenitic Stainless Steel
    Song Ren-bo
    Xiang Jian-ying
    Hou Dong-po
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 (11) : 53 - 59