Slagging behaviors of high alkali Zhundong coal during circulating fluidized bed gasification

被引:63
作者
Song, Guoliang [1 ]
Qi, Xiaobin [1 ,2 ]
Song, Weijian [1 ,2 ]
Yang, Shaobo [1 ,2 ]
Lu, Qinggang [1 ]
Nowak, Wojciech [3 ]
机构
[1] Chinese Acad Sci, Inst Engn Thermophys, Beijing 100190, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
[3] Czestochowa Tech Univ, Dabrowskiego 73, PL-42200 Czestochowa, Poland
基金
对外科技合作项目(国际科技项目);
关键词
Zhundong coal; High alkali metal; Slagging; Circulating fluidized bed; Gasification; HIGH-TEMPERATURE CORROSION; ASH DEPOSITION; HIGH-SODIUM; SUPERHEATER MATERIALS; COMBUSTION; LIGNITE; TRANSFORMATION; BOILERS; DEFLUIDIZATION; AGGLOMERATION;
D O I
10.1016/j.fuel.2016.08.075
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Slagging behaviors of high alkali Zhundong coal during circulating fluidized bed (CFB) gasification were investigated in a 0.4 t/d CFB test rig for 72 h, with air-cooled ash deposition probes located along the gas flow direction. The microstructure, chemical compositions and mineral crystalline phases of ash were analyzed. Corrosion-reduced slagging and layered slagging were found on the ash deposition probes and the circulating air pipe, respectively. At the initial stage of corrosion-reduced slagging, Fe in the metal surface was transferred to an unsteady state by the corrosion of NaCl. Once corrosion occurred, the corrosion-reduced slagging was accelerated by the presence of sodium iron oxides and alkali sulfates. This type of slagging was greatly influenced by wall temperature, as it was more inclined to occur on the probes only at wall temperature above 495 degrees C. The high density of circulating ash, which was rich in Ca, Na, Fe, S, Si and Mg in the form of low-melting-temperature sulfates and silicates, resulted in slagging on the circulating air pipe. A layered structure was observed on the cross-section of the slags, and its characteristics were determined by the distributions of Ca, S, Na and Fe. With the growth of the slags, the air hole in the circulating air pipe was blocked due to the aggregation of stickier fusant, which might cause unscheduled outages. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:140 / 149
页数:10
相关论文
共 34 条
[1]  
[Anonymous], RES COMBUSTION SLAGG
[2]   Fireside slagging, fouling, and high-temperature corrosion of heat-transfer surface due to impurities in steam-raising fuels [J].
Bryers, RW .
PROGRESS IN ENERGY AND COMBUSTION SCIENCE, 1996, 22 (01) :29-120
[3]   EXTERNAL CORROSION IN COAL-FIRED BOILERS - ASSESSMENT FROM LABORATORY DATA [J].
CUTLER, AJB ;
RAASK, E .
CORROSION SCIENCE, 1981, 21 (11) :789-800
[4]   Inhibition of lignite ash slagging and fouling upon the use of a silica-based additive in an industrial pulverised coal-fired boiler. Part 1. Changes on the properties of ash deposits along the furnace [J].
Dai, Bai-Qian ;
Wu, Xiaojiang ;
De Girolamo, Anthony ;
Zhang, Lian .
FUEL, 2015, 139 :720-732
[5]   Characteristics of Ash Deposits in a Pulverized Lignite Coal-Fired Boiler and the Mass Flow of Major Ash-Forming Inorganic Elements [J].
Dai, Bai-Qian ;
Low, Fiona ;
De Girolamo, Anthony ;
Wu, Xiaojiang ;
Zhang, Lian .
ENERGY & FUELS, 2013, 27 (10) :6198-6211
[6]   Are NaCl and KCl equally corrosive on superheater materials of steam boilers? [J].
Enestam, Sonja ;
Bankiewicz, Dorota ;
Tuiremo, Johanna ;
Makela, Kari ;
Hupa, Mikko .
FUEL, 2013, 104 :294-306
[7]   Combustion performance and sodium transformation of high-sodium ZhunDong coal during chemical looping combustion with hematite as oxygen carrier [J].
Ge, Huijun ;
Shen, Laihong ;
Gu, Haiming ;
Song, Tao ;
Jiang, Shouxi .
FUEL, 2015, 159 :107-117
[8]   ASH FORMATION DURING PULVERIZED SUBBITUMINOUS COAL COMBUSTION .1. CHARACTERIZATION OF COALS, AND INORGANIC TRANSFORMATIONS DURING EARLY STAGES OF BURNOUT [J].
HURLEY, JP ;
SCHOBERT, HH .
ENERGY & FUELS, 1992, 6 (01) :47-58
[9]   Reactions between sodium and silica during gasification of a low-rank coal [J].
Kosminski, A. ;
Ross, D. P. ;
Agnew, J. B. .
FUEL PROCESSING TECHNOLOGY, 2006, 87 (12) :1037-1049
[10]   Reactions between sodium and kaolin during gasification of a low-rank coal [J].
Kosminski, A. ;
Ross, D. P. ;
Agnew, J. B. .
FUEL PROCESSING TECHNOLOGY, 2006, 87 (12) :1051-1062