Temperature dependence of pitting potentials for austenitic stainless steels above their critical pitting temperature

被引:135
|
作者
Laycock, NJ
Newman, RC
机构
[1] Mat Performance Technol, Lower Hutt, New Zealand
[2] UMIST, Ctr Corros & Protect, Manchester M60 1QD, Lancs, England
关键词
stainless steel; anodic polarisation; pitting corrosion;
D O I
10.1016/S0010-938X(98)00020-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fitting potentials of austenitic stainless steels decrease slowly with increasing temperature above the critical pitting temperature. Fitting potentials have been measured in 1 M NaCl for 304, 316 and 904L stainless steels between 20 and 90 degrees C, and narrow diameter artificial pit electrodes of 302 stainless steel have been used to study dissolution kinetics over the same temperature range. The transition potential, E-T, between activation/ohmic control and diffusion control of the dissolution has been mapped as functions of limiting current density and temperature, and the results interpreted using a simple model of dissolution kinetics within the pit. The dependence of E-T on temperature is strikingly similar to the dependence of the pitting potential, and the model has been used to differentiate between the contributions of activation and solution resistance overpotentials; the observed effects are due mostly to a decrease in the activation overpotential with increasing temperature. (C) 1998 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:887 / 902
页数:16
相关论文
共 50 条
  • [31] Pitting corrosion and crevice corrosion behaviors of high nitrogen austenitic stainless steels
    Li, Hua-bing
    Jiang, Zhou-hua
    Yang, Yan
    Cao, Yang
    Zhang, Zu-rui
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2009, 16 (05) : 517 - 524
  • [32] Electrochemical investigation of the influence of nitrogen alloying on pitting corrosion of austenitic stainless steels
    Jargelius-Pettersson, RFA
    CORROSION SCIENCE, 1999, 41 (08) : 1639 - 1664
  • [33] Pitting Corrosion of Thermally Aged Duplex Stainless Steels at Different Temperature for Long Time
    Wang, Yongqiang
    Sun, Hao
    Li, Junliang
    Li, Dandan
    Li, Na
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2019, 22 (06):
  • [34] Pitting corrosion of duplex stainless steels
    Siow, KS
    Song, TY
    Qiu, JH
    ANTI-CORROSION METHODS AND MATERIALS, 2001, 48 (01) : 31 - 36
  • [35] Pitting corrosion behaviour of PM austenitic stainless steels sintered in nitrogen-hydrogen atmosphere
    Garcia, C.
    Martin, F.
    de Tiedra, P.
    Cambronero, L. Garcia
    CORROSION SCIENCE, 2007, 49 (04) : 1718 - 1736
  • [36] Effects of molybdenum on the pitting of ferritic- and austenitic-stainless steels in bromide and chloride solutions
    Kaneko, M
    Isaacs, HS
    CORROSION SCIENCE, 2002, 44 (08) : 1825 - 1834
  • [37] Deterioration in critical pitting temperature of 904L stainless steel by addition of sulfate ions
    Moayed, M. H.
    Newman, R. C.
    CORROSION SCIENCE, 2006, 48 (11) : 3513 - 3530
  • [38] Correlation between critical pitting temperature and degree of sensitisation on alloy 2205 duplex stainless steel
    Ebrahimi, N.
    Momeni, M.
    Moayed, M. H.
    Davoodi, A.
    CORROSION SCIENCE, 2011, 53 (02) : 637 - 644
  • [39] Analysis of current transients and morphology of metastable and stable pitting on stainless steel above pitting potential
    Moayed, MH
    Newman, RC
    IRANIAN JOURNAL OF SCIENCE AND TECHNOLOGY, 2002, 26 (B1): : 21 - 30
  • [40] Pitting corrosion of laser welded stainless offshore steels
    Kujanpää, V
    Kyröläinen, A
    Torvinen, T
    Storbacka, H
    20TH ICALEO 2001, VOLS 92 & 93, CONGRESS PROCEEDINGS, 2001, : 448 - 454