Spectroscopic analysis of Nd3+-doped cadmium-vanadate invert glasses for near-infrared laser applications

被引:20
作者
Soriano-Romero, O. [1 ]
Espinosa-Ceron, M. Y. [1 ]
Carmona-Tellez, S. [2 ]
Lira, A. [3 ]
Caldino, U. [4 ]
Lozada-Morales, R. [1 ]
Meza-Rocha, A. N. [2 ]
机构
[1] Benemerita Univ Autonoma Puebla, Postgrad Fis Aplicada, Fac Ciencias Fisicomatemat, Av San Claudio & Av 18 Sur, Puebla 72570, Pue, Mexico
[2] Benemerita Univ Autonoma Puebla, CONACyT, Fac Ciencias Fisicomatemat, Postgrad Fis Aplicada, Av San Claudio & Av 18 Sur, Puebla 72570, Pue, Mexico
[3] Univ Autonoma Estado Mexico, Fac Ciencias, Dept Fis, Toluca 50000, Mexico
[4] Univ Autonoma Metropolitana Iztapalapa, Dept Fis, Cdmx 09340, Mexico
关键词
Judd-Ofelt analysis; Near infrared laser applications; PHOSPHATE-GLASSES; BORATE GLASSES; OPTICAL-PROPERTIES; ENERGY-TRANSFER; REDDISH-ORANGE; ND3+ IONS; EMISSION; DY3+; TRANSITION; DEPENDENCE;
D O I
10.1016/j.jnoncrysol.2021.121085
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nd3+ activated CdO-V2O5 invert glasses were synthesized by the well-stablished melt quenching technique, using starting proportions of 95.0 and 5.0 mol% of CdO and V2O5, respectively. The XRD patterns revealed that the glass system remains amorphous up to 4.0 mol% of Nd3+. Such fact was mainly attributed to the low V2O5 content, which avoided the segregation of additional phases. The minimal addition of 0.1 mol% of Nd3+ reduced the direct and indirect glass bandgap energies from 2.79 to 2.66 eV, and from 2.48 to 2.13 eV, respectively. For higher Nd3+ contents, the bandgap energy was recovered, reaching values of 2.78 and 2.40 eV for direct and indirect allowed transitions, respectively. This fact was associated with a Burstein-Moss like effect, observed in semiconductors highly doped. The tail of the absorption edge revealed that the Urbach energy systematically grows with the addition of Nd3+, because of the creation of localized states into the bandgap. The Judd-Ofelt (JO) parameters obtained by least-square method from the experimental and theoretical oscillator strengths, were found in the Omega(2) = 5.24-11.04 x 10(-20) cm(2), Omega(4) = 2.26-4.47 x 10(-20) cm(2), and Omega(6) = 2.85-6.28 x 10(-20) cm(2) range. Such values are close to those reported in other popular glass systems. The stimulated emission cross-section peak (sigma(p)) values calculated for the glass sample doped with 2.0 mol% resulted to be 0.26 x 10(-20) cm(2) (Nd3+: F-4(3/2) -> I-4(9/2)) and 0.81 x 10(-20) cm(2) (Nd3+: F-4(3/2) -> I-4(11/2)). The Nd3+ emission spectra, recorded upon 585 nm excitation (Nd3+: I-4(9/2) -> (4)G(5/2) + (2)G(7/2)), showed the near-infrared Nd3+ emission bands at 881 nm (Nd3+: F-4(3/2) -> I-4(9/2)), 1063 nm (Nd3+: F-4(3/2) -> I-4(11/2)) and 1341 nm (Nd3+: F-4(3/2) -> I-4(13/2)), being dominated for that coming from the Nd3+: F-4(3/2) -> I-4(11/2) transition. The overall emission reached the optimum intensity at 2.0 mol% of Nd3+, with a maximum quantum efficiency (eta(QE)) of 0.23. From the emission spectra important laser parameters such as gain bandwidth (sigma(EMI)(lambda(p)) x Delta lambda(em)) and optical gain (sigma(EMI)(lambda(p)) x tau(R)), were determined for the sample with the highest eta(QE) value. The sigma(EMI)(lambda(p)) x Delta lambda(em) values resulted to be 11.3 and 32.0 x 10(-27) cm(3) for the Nd3+: F-4(3/2) -> I-4(9/2), (11/2) transitions, respectively. The sigma(EMI)(lambda(p)) x tau(R) parameter values were 11.1 and 35.3 x 10(-25) cm(2)s for Nd3+: F-4(3/2) -> I-4(9/2,11/2) transitions, respectively. The Inokuti-Hirayama model suggested that the Nd3+ cross-relaxation process might be dominated by an electric dipole-dipole interaction, inside Nd3+-Nd3+ clusters.
引用
收藏
页数:8
相关论文
共 40 条
[1]   Characterization of Invert Soda Lime Silica Glasses Containing High Titania Content Together with their Glass Ceramics [J].
Abdelghany, A. M. ;
Ghoneim, N. A. ;
ElBatal, H. A. .
SILICON, 2018, 10 (03) :1035-1043
[2]   Dependence of the structure, optical, and dynamic properties of novel cadmium phosphate glass on vanadium content [J].
AbuShanab, Waheed Sami ;
Moustafa, Essam B. ;
Hammad, Ahmed H. .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (06) :14178-14189
[3]   Structural and radiation shielding properties of chromium oxide doped borosilicate glass [J].
Aktas, B. ;
Yalcin, S. ;
Dogru, K. ;
Uzunoglu, Z. ;
Yilmaz, D. .
RADIATION PHYSICS AND CHEMISTRY, 2019, 156 :144-149
[4]   Optical Properties of Soda-Lime-Silica Glasses Doped with Eggshell Powder [J].
Aktas, B. ;
Albaskara, M. ;
Yalcin, S. ;
Dogru, K. .
ACTA PHYSICA POLONICA A, 2017, 132 (03) :442-444
[5]   Erbium-doped fluorotellurite titanate glasses for near infrared broadband amplifiers [J].
Algarni, H. ;
Al-Assiri, M. S. ;
Reben, M. ;
Kityk, I. V. ;
Burtan-Gwizdala, B. ;
Hegazy, H. H. ;
Umar, Ahmad ;
Yousef, E. ;
Lisiecki, R. .
OPTICAL MATERIALS, 2018, 83 :257-262
[6]   Composition dependence of the crystalline-to-amorphous phase transformation of vanadate compounds in the CdO-V2O5 binary system [J].
Aquino-Meneses, L. ;
Lozada-Morales, R. ;
Lopez-Calzada, G. ;
Jimenez-Sandoval, S. ;
Zayas, Ma. E. ;
Zelaya-Angel, O. ;
Becerril, M. ;
Carmona-Rodriguez, J. ;
Sanchez-Mora, E. ;
Serrano, L. E. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2015, 408 :26-31
[7]   Preparation and characterization of invert glasses with high CdO content [J].
Azooz, M. A. ;
Ouis, M. A. ;
ElBatal, H. A. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2019, 515 :82-87
[8]   Development of sodium-zinc phosphate glasses doped with Dy3+, Eu3+ and Dy3+/Eu3+ for yellow laser medium, reddish-orange and white phosphor applications [J].
Caldino, U. ;
Lira, A. ;
Meza-Rocha, A. N. ;
Camarillo, I. ;
Lozada-Morales, R. .
JOURNAL OF LUMINESCENCE, 2018, 194 :231-239
[9]   Energy transfer in CaF2 doped with Ce3+, Eu 2+ and Mn2+ ions [J].
Caldiño, U.G. .
2003, Institute of Physics Publishing (15) :7127-7137
[10]   ELECTRONIC ENERGY LEVELS IN TRIVALENT LANTHANIDE AQUO IONS .I. PR3+ ND3+ PM3+ SM3+ DY3+ HO3+ ER3+ AND TM3+ [J].
CARNALL, WT ;
FIELDS, PR ;
RAJNAK, K .
JOURNAL OF CHEMICAL PHYSICS, 1968, 49 (10) :4424-&