The Microstructures and Tensile Properties of As-Extruded Mg-4Sm-xZn-0.5Zr (x=0, 1, 2, 3, 4 wt %) Alloys

被引:8
作者
Che, Chaojie [1 ,2 ]
Cai, Zhongyi [1 ]
Cheng, Liren [2 ]
Meng, Fanxing [2 ,3 ]
Yang, Zhen [1 ]
机构
[1] Jilin Univ, Roll Forging Res Inst, Changchun 130025, Jilin, Peoples R China
[2] Chinese Acad Sci, Changchun Inst Appl Chem, State Key Lab Rare Earth Resource Utilizat, Changchun 130022, Jilin, Peoples R China
[3] Jilin Univ, Sch Mat Sci & Engn, Changchun 130025, Jilin, Peoples R China
基金
中国国家自然科学基金;
关键词
Mg-Sm-Zn-Zr; dynamic precipitation; microstructure; mechanical property; MECHANICAL-PROPERTIES; MAGNESIUM ALLOYS; HEAT-TREATMENT; DYNAMIC RECRYSTALLIZATION; HOT-WORKING; PRECIPITATION; ZN; EVOLUTION; TEXTURE;
D O I
10.3390/met7070281
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructures and tensile properties of as-cast and as-extruded Mg-4Sm-xZn-0.5Zr (x = 0, 1, 2, 3, 4 wt %) alloys were systematically investigated by optical microscope, X-ray diffractometer (XRD), scanning electron microscope (SEM) and transmission electron microscope (TEM). Numerous nanoscale dynamic precipitates could be observed in the as-extruded alloys containing high content of Zn, and the nanoscale particles were termed as (Mg,Zn)(3)Sm phase. Some basal disc-like precipitates were observed in as-extruded Mg-4Sm-4Zn-0.5Zr alloy, which were proposed to have a hexagonal structure with a = 0.556 nm. The dynamic precipitates effectively pinned the motions of DRXed (dynamic recrystallized) grain boundaries leading to an obvious reduction of DRXed grain size, and the tensile yield strength of as-extruded alloy was improved. The as-extruded Mg-4Sm-4Zn-0.5Zr alloy exhibits the best comprehensive mechanical properties at room temperature among all the alloys, and the yield strength, ultimate tensile strength and elongation are about 246 MPa, 273 MPa and 21% respectively.
引用
收藏
页数:15
相关论文
共 33 条
[1]   Hardening precipitation in a Mg-4Y-3RE alloy [J].
Antion, C ;
Donnadieu, P ;
Perrard, F ;
Deschamps, A ;
Tassin, C ;
Pisch, A .
ACTA MATERIALIA, 2003, 51 (18) :5335-5348
[2]   Influence of grain size on hot working stresses and microstructures in Mg-3Al-lZn [J].
Barnett, MR ;
Beer, AG ;
Atwell, D ;
Oudin, A .
SCRIPTA MATERIALIA, 2004, 51 (01) :19-24
[3]   Recrystallization during and following hot working of magnesium alloy AZ31 [J].
Barnett, MR .
MAGNESIUM ALLOYS 2003, PTS 1 AND 2, 2003, 419-4 :503-508
[4]  
Chen Z.H., 2006, CHEM IND ENG PROG, V25, P7
[5]   Dynamic precipitation in Mg-3Al-1Zn alloy during different plastic deformation modes [J].
Dogan, E. ;
Wang, S. ;
Vaughan, M. W. ;
Karaman, I. .
ACTA MATERIALIA, 2016, 116 :1-13
[6]   Phase equilibria and transformations in ternary Mg-rich Mg-Y-Zn alloys [J].
Groebner, J. ;
Kozlov, A. ;
Fang, X. Y. ;
Geng, J. ;
Nie, J. F. ;
Schmid-Fetzer, R. .
ACTA MATERIALIA, 2012, 60 (17) :5948-5962
[7]   Microstructure and strengthening mechanism of high strength Mg-10Gd-2Y-0.5Zr alloy [J].
He, S. M. ;
Zeng, X. Q. ;
Peng, L. M. ;
Gao, X. ;
Nie, J. F. ;
Ding, W. J. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 427 (1-2) :316-323
[8]   Microstructure, texture and mechanical properties of a hot rolled Mg-6.5Gd-1.3Nd-0.7Y-0.3Zn alloy [J].
Hou, Xiuli ;
Cao, Zhanyi ;
Zhao, Lei ;
Wang, Lidong ;
Wu, Yaoming ;
Wang, Limin .
MATERIALS & DESIGN, 2012, 34 :776-781
[9]  
Humphreys F.J., 2005, RECRYSTALLIZATION RE
[10]   Effect of strain-induced precipitation on dynamic recrystallization in Mg-Al-Sn alloys [J].
Kabir, Abu Syed Hurnaun ;
Sanjari, Mehdi ;
Su, Jing ;
Jung, In-Ho ;
Yue, Stephen .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 616 :252-259