Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel

被引:21
作者
Sun, Qi [1 ,2 ]
Wang, Jian [1 ,2 ]
Li, Hua-bing [3 ]
Li, Yue [1 ,2 ]
Hu, Ya-di [1 ,2 ]
Bai, Jin gang [4 ]
de Han, Pei [1 ,2 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030021, Shanxi, Peoples R China
[2] Taiyuan Univ Technol, Key Lab Interface Sci & Engn Adv Mat, Taiyuan 030021, Shanxi, Peoples R China
[3] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[4] Technol Ctr Taiyuan Iron & Steel Grp Co Ltd, Taiyuan 030003, Shanxi, Peoples R China
基金
中国国家自然科学基金; 高等学校博士学科点专项科研基金;
关键词
duplex stainless steel; short-term aging; chi phase; pitting corrosion; selective corrosion; grain size; SIGMA-PHASE; DELETERIOUS PHASES; PRECIPITATION; TRANSFORMATION; RESISTANCE;
D O I
10.1016/S1006-706X(16)30159-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Correlation between pitting corrosion behavior and chi (chi) phase formed after a short-term aging (5, 10 and 15 min) at 850 degrees C of 2205 duplex stainless steel (DSS) was investigated using potentiodynamic polarization tests, optical microscopy, and scanning electron microscopy equipped with energy-dispersive spectrum system. Results showed that after aging for 5 min, the chi phase initially precipitated at ferrite grain boundaries, developed and then became linked with prolonging aging time. The chi phase was rich in Cr and Mo, resulting in formation of depleted zones nearby. The chi phase could reduce corrosion resistance of DSS and slightly influence its stability, but the specimens still displayed the capacity for repassivation. Some lines of evidence showed that stable pitting corrosion initiated at the boundaries of precipitates. The chi phase was selectively corroded during the first stage of corrosion and then the depleted zones nearby were attacked. In addition, the grain size and volume of precipitates also affected pit nucleation and progress, and suitable size and distribution of chi phase could aggravate pit initiation at precipitate boundaries. The chi phase with considerably low volume fraction and small size was not sensitive position for pit initiation.
引用
收藏
页码:1071 / 1079
页数:9
相关论文
共 50 条
  • [41] HOT DEFORMATION BEHAVIOR OF 2205 DUPLEX STAINLESS STEEL
    Chen Lei
    Wang Longmei
    Du Xiaojian
    Liu Xiao
    ACTA METALLURGICA SINICA, 2010, 46 (01) : 52 - 56
  • [42] Electrochemical corrosion behavior of 2205 duplex stainless steel in hot concentrated seawater under vacuum conditions
    Yang, Yong
    Zeng, Hongtao
    Xin, Sensen
    Hou, Xueling
    Li, Moucheng
    CORROSION SCIENCE, 2020, 165
  • [43] Phase transformation and mechanical behavior in annealed 2205 duplex stainless steel welds
    Badji, Riad
    Bouabdallah, Mabrouk
    Bacroix, Brigitte
    Kahloun, Charlie
    Belkessa, Brahim
    Maza, Halim
    MATERIALS CHARACTERIZATION, 2008, 59 (04) : 447 - 453
  • [44] Influence of sigma-phase formation on the localized corrosion behavior of a duplex stainless steel
    Adhe, KN
    Kain, V
    Madangopal, K
    Gadiyar, HS
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1996, 5 (04) : 500 - 506
  • [45] Electrochemical and Corrosion Behavior of 2205 Duplex Stainless Steel in Simulated Concrete Pore Solution
    Li, Baosong
    Zhang, Weiwei
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (09): : 8432 - 8446
  • [46] Phase Transformation and Its Effects on Mechanical Properties and Pitting Corrosion Resistance of 2205 Duplex Stainless Steel
    ZOU De-ning1
    2. State Key Laboratory for Mechanical Behavior of Metal Materials
    3. State Key Laboratory of Advanced Stainless Steel Materials
    Journal of Iron and Steel Research(International), 2010, 17 (11) : 67 - 72
  • [47] Phase Transformation and Its Effects on Mechanical Properties and Pitting Corrosion Resistance of 2205 Duplex Stainless Steel
    De-ning Zou
    Ying Han
    Wei Zhang
    Guang-wei Fan
    Journal of Iron and Steel Research International, 2010, 17 : 67 - 72
  • [48] Corrosion Properties and Impact Toughness of 2205 Duplex Stainless Steel after TIG Welding
    Basyigit, Aziz Baris
    Kurt, Adem
    MATERIALS TESTING, 2014, 56 (10) : 786 - 794
  • [49] Effect of hydrogen on the pitting corrosion of 2205 duplex stainless steel welded joints
    Zheng, Qing
    Zhang, Houwei
    Wang, Dengyun
    Xu, Lining
    Li, Gang
    Qiao, Lijie
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2024, 59 (02) : 104 - 119
  • [50] Effect of Temperature on Resistance to Pitting Corrosion in Duplex Stainless Steel 2205 Welds
    Y. Martinez-Galvan
    L. Dzib-Perez
    M. Garcia-Renteria
    O. Bilyy
    V. Lopez-Morelos
    J. Gonzalez-Sanchez
    Materials Science, 2023, 58 (6) : 755 - 761