Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel

被引:22
作者
Sun, Qi [1 ,2 ]
Wang, Jian [1 ,2 ]
Li, Hua-bing [3 ]
Li, Yue [1 ,2 ]
Hu, Ya-di [1 ,2 ]
Bai, Jin gang [4 ]
de Han, Pei [1 ,2 ]
机构
[1] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030021, Shanxi, Peoples R China
[2] Taiyuan Univ Technol, Key Lab Interface Sci & Engn Adv Mat, Taiyuan 030021, Shanxi, Peoples R China
[3] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[4] Technol Ctr Taiyuan Iron & Steel Grp Co Ltd, Taiyuan 030003, Shanxi, Peoples R China
基金
中国国家自然科学基金; 高等学校博士学科点专项科研基金;
关键词
duplex stainless steel; short-term aging; chi phase; pitting corrosion; selective corrosion; grain size; SIGMA-PHASE; DELETERIOUS PHASES; PRECIPITATION; TRANSFORMATION; RESISTANCE;
D O I
10.1016/S1006-706X(16)30159-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Correlation between pitting corrosion behavior and chi (chi) phase formed after a short-term aging (5, 10 and 15 min) at 850 degrees C of 2205 duplex stainless steel (DSS) was investigated using potentiodynamic polarization tests, optical microscopy, and scanning electron microscopy equipped with energy-dispersive spectrum system. Results showed that after aging for 5 min, the chi phase initially precipitated at ferrite grain boundaries, developed and then became linked with prolonging aging time. The chi phase was rich in Cr and Mo, resulting in formation of depleted zones nearby. The chi phase could reduce corrosion resistance of DSS and slightly influence its stability, but the specimens still displayed the capacity for repassivation. Some lines of evidence showed that stable pitting corrosion initiated at the boundaries of precipitates. The chi phase was selectively corroded during the first stage of corrosion and then the depleted zones nearby were attacked. In addition, the grain size and volume of precipitates also affected pit nucleation and progress, and suitable size and distribution of chi phase could aggravate pit initiation at precipitate boundaries. The chi phase with considerably low volume fraction and small size was not sensitive position for pit initiation.
引用
收藏
页码:1071 / 1079
页数:9
相关论文
共 29 条
[1]   Electrochemical characterization of three corrosion-resistant alloys after processing for heating-element sheathing [J].
Bellezze, T ;
Roventi, G ;
Fratesi, R .
ELECTROCHIMICA ACTA, 2004, 49 (17-18) :3005-3014
[2]  
Bhattacharya A., 2007, CORROSION
[3]   Measuring Secondary Phases in Duplex Stainless Steels [J].
Calliari, I. ;
Brunelli, K. ;
Dabala, M. ;
Ramous, E. .
JOM, 2009, 61 (01) :80-83
[4]   Effect of Secondary Phase Precipitation on the Corrosion Behavior of Duplex Stainless Steels [J].
Chan, Kai Wang ;
Tjong, Sie Chin .
MATERIALS, 2014, 7 (07) :5268-5304
[5]   The effect of high-temperature exposure on the microstructural stability and toughness property in a 2205 duplex stainless steel [J].
Chen, TH ;
Weng, KL ;
Yang, JR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 338 (1-2) :259-270
[6]   Effects of solution treatment and continuous cooling on σ-phase precipitation in a 2205 duplex stainless steel [J].
Chen, TH ;
Yang, JR .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 311 (1-2) :28-41
[7]   Assessment of electrochemical methods used on corrosion of superduplex stainless steel [J].
de Assis, Kioshy S. ;
de Sousa, Flavio V. V. ;
Miranda, Marcelo ;
Margarit-Mattos, Isabel C. P. ;
Vivier, Vincent ;
Mattos, Oscar R. .
CORROSION SCIENCE, 2012, 59 :71-80
[8]   Evaluation of localized corrosion in duplex stainless steel aged at 850°C with critical pitting temperature measurement [J].
Deng, Bo ;
Wang, Zhiyu ;
Jiang, Yiming ;
Wang, Hao ;
Gao, Juan ;
Li, Jin .
ELECTROCHIMICA ACTA, 2009, 54 (10) :2790-2794
[9]   Detection of deleterious phases in duplex stainless steel by weak galvanostatic polarization in alkaline solution [J].
Dominguez-Aguilar, M. A. ;
Newman, R. C. .
CORROSION SCIENCE, 2006, 48 (09) :2560-2576
[10]  
Dos Santos D.C., 2013, CORROSION, V69, P900