Dissimilar transient liquid phase bonding of Ti-6Al-4V and Co-Cr-Mo biomaterials using a Cu interlayer: Microstructure and mechanical properties

被引:20
|
作者
Vazirian, S. [1 ]
Farzadi, A. [1 ]
机构
[1] Amirkabir Univ Technol, Dept Mat & Met Engn, Polytech Tehran, Hafez Ave, Tehran 1591634311, Iran
关键词
Diffusion brazing; Bonding time; Joining; Shear strength; Intermetallic compound; ASTM F-75 Co-based alloy; COMMERCIALLY PURE TITANIUM; 316L STAINLESS-STEEL; INTERFACIAL MICROSTRUCTURE; TENSILE-STRENGTH; MARTENSITIC-TRANSFORMATION; CORROSION-RESISTANCE; ALLOY; EVOLUTION; JOINTS; TI;
D O I
10.1016/j.jallcom.2020.154510
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In order to construct a bimetallic device for the medical application, the selection of the joining process is essential. Transient liquid phase (TLP) bonding of two biomaterials of Ti-6Al-4V and Co-Cr-Mo (ASTM F-75) alloys with a Cu interlayer was investigated at the bonding time of 5, 15, 30, and 45 min at the bonding temperature of 920 degrees C. To evaluate the microstructure, the interfacial brazing zone (IBZ) was studied using an optical microscope (OM), field emission scanning electron microscope (FE-SEM), and energy dispersive spectroscopy (EDS). The results showed that the microstructure of Ti-6Al-4V/Cu/Co-Cr-Mo was composed of CoCr(Ti, Mo), Ti(Cu, Co), Ti2Cu, alpha-Ti and beta-Ti. By raising the bonding time and increasing the diffusion of Cu into base metals, the transformation of Ti(Cu, Co) into Ti2Cu was done. Then, the thickness of the Ti(Cu, Co) intermetallic compound (IMC) reduced. With increasing bonding time from 30 to 45 min, the morphology of Ti2Cu IMC changed from tiny to blocky. Shear strength, microhardness, and fractographic assessment were used to investigate the mechanical properties of the bonding zone. It is found that with increasing the bonding time, the shear strength of the brazed joints increased. The maximum shear strength of 316 MPa occurred at 45 min. The microhardness test also demonstrated that the CoCr(Ti, Mo) in the diffusion layer with the hardness value of 839 HV was the hardest phase. The formation of IMCs changed the fracture mode. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Effect of bonding temperature on microstructure and mechanical properties of dissimilar joint between Ti-6Al-4V and Co-Cr-Mo biomaterials
    Vazirian, S.
    Farzadi, A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 792
  • [2] Transient liquid phase bonding of Al 2024 to Ti-6Al-4V alloy using Cu-Zn interlayer
    Samavatian, Majid
    Halvaee, Ayoub
    Amadeh, Ahmad Ali
    Khodabandeh, Alireza
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (03) : 770 - 775
  • [3] Microstructure evolution and mechanical properties of transient liquid phase bonded Ti-6Al-4V joint with copper interlayer
    Deng, Yongqiang
    Sheng, Guangmin
    Wang, Fangli
    Yuan, Xinjian
    An, Qi
    MATERIALS & DESIGN, 2016, 92 : 1 - 7
  • [4] Transient liquid phase bonding of stainless steel 316L to Ti-6Al-4V using Cu/Ni multi-interlayer: microstructure, mechanical properties, and fractography
    Surendar, A.
    Lucas, Andrew
    Abbas, Mazhar
    Rahim, Robbi
    Salmani, Mohammad
    WELDING IN THE WORLD, 2019, 63 (04) : 1025 - 1032
  • [5] NONWOVEN WHEEL POLISHING OF TI-6AL-4V AND CO-CR-MO ALLOYS
    Wang, Yancheng
    Yan, Bing
    Shih, Albert J.
    PROCEEDINGS OF THE ASME 9TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, 2014, VOL 2, 2014,
  • [6] Processing of IN718/Ti-6Al-4V bimetallic joint using transient liquid phase bonding: effect of bonding temperature on the microstructure and mechanical properties
    Binesh, B.
    Aghaie-Khafri, M.
    Fayegh, A.
    PHILOSOPHICAL MAGAZINE, 2022, 102 (09) : 745 - 772
  • [7] Joining dental biomaterials of Ti-6Al-4V alloy and cp-Ti using transient liquid phase bonding: Metallurgical and mechanical assessment
    Vazirian, S.
    Farzadi, A.
    Solouk, A.
    MATERIALS TODAY COMMUNICATIONS, 2022, 32
  • [8] Effect of bonding temperature on the microstructure and mechanical properties of Ti-6Al-4V to AISI 304 transient liquid phase bonded joint
    Norouzi, Ehsan
    Atapour, Masoud
    Shamanian, Morteza
    Allafchian, Alireza
    MATERIALS & DESIGN, 2016, 99 : 543 - 551
  • [9] Microstructure and Mechanical Properties of Al2024/Ti-6Al-4V Transient Liquid Phase Bonded Joint
    Samavatian, M.
    Halvaee, A.
    Amadeh, A.
    Zakipour, S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (06) : 2526 - 2534
  • [10] Microstructure and Mechanical Properties of Al2024/Ti-6Al-4V Transient Liquid Phase Bonded Joint
    M. Samavatian
    A. Halvaee
    A. Amadeh
    S. Zakipour
    Journal of Materials Engineering and Performance, 2015, 24 : 2526 - 2534