The effect of various sandblasting conditions on surface changes of dental zirconia and shear bond strength between zirconia core and indirect composite resin

被引:59
作者
Su, Naichuan [1 ,2 ]
Yue, Li [3 ]
Liao, Yunmao [1 ]
Liu, Wenjia [2 ]
Zhang, Hai [4 ]
Li, Xin [5 ]
Wang, Hang [1 ,2 ]
Shen, Jiefei [1 ,2 ]
机构
[1] Sichuan Univ, West China Hosp Stomatol, State Key Lab Oral Dis, Chengdu 610041, Peoples R China
[2] Sichuan Univ, West China Sch Stomatol, Dept Prosthodont, Chengdu 610041, Peoples R China
[3] Sichuan Univ, West China Hosp Stomatol, Dept Dent Technol, Chengdu 610041, Peoples R China
[4] Univ Washington, Sch Dent, Dept Restorat Dent, Seattle, WA 98195 USA
[5] Mianyang Cent Hosp, Dept Stomatol, Mianyang, Peoples R China
关键词
All-ceramic; Bond strength; Indirect composite; Sandblasting; Zirconia; FIXED PARTIAL DENTURES; Y-TZP CERAMICS; FLEXURAL STRENGTH; IN-VITRO; VENEERING CERAMICS; RESTORATIONS; ROUGHNESS; CEMENT; PERFORMANCE; FRAMEWORKS;
D O I
10.4047/jap.2015.7.3.214
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
PURPOSE. To measure the surface loss of dental restorative zirconia and the short-term bond strength between an indirect composite resin (ICR) and zirconia ceramic after various sandblasting processes. MATERIALS AND METHODS. Three hundred zirconia bars were randomly divided into 25 groups according to the type of sandblasting performed with pressures of 0.1, 0.2, 0.4 and 0.6 MPa, sandblasting times of 7, 14 and 21 seconds, and alumina powder sizes of 50 and 110 mu m. The control group did not receive sandblasting. The volume loss and height loss on zirconia surface after sandblasting and the shear bond strength (SBS) between the sandblasted zirconia and ICR after 24-h immersion were measured for each group using multivariate analysis of variance (ANOVA) and Least Significance Difference (LSD) test (alpha=.05). After sandblasting, the failure modes of the ICR/zirconia surfaces were observed using scanning electron microscopy. RESULTS. The volume loss and height loss were increased with higher sandblasting pressure and longer sandblasting treatment, but they decreased with larger powder size. SBS was significantly increased by increasing the sandblasting time from 7 seconds to 14 seconds and from 14 seconds to 21 seconds, as well as increasing the size of alumina powder from 50 mu m to 110 mu m. SBS was significantly increased from 0.1 MPa to 0.2 MPa according to the size of alumina powder. However, the SBSs were not significantly different with the sandblasting pressure of 0.2, 0.4 and 0.6 MPa. The possibilities of the combination of both adhesive failure and cohesive failure within the ICR were higher with the increases in bonding strength. CONCLUSION. Based on the findings of this study, sandblasting with alumina particles at 0.2 MPa, 21 seconds and the powder size of 110 mu m is recommended for dental applications to improve the bonding between zirconia core and ICR.
引用
收藏
页码:214 / 223
页数:10
相关论文
共 48 条
[1]   Microtensile bond strength of different components of core veneered all-ceramic restorations [J].
Aboushelib, MN ;
de Jager, N ;
Kleverlaan, CJ ;
Feiler, AJ .
DENTAL MATERIALS, 2005, 21 (10) :984-991
[2]  
Aboushelib Moustafa N, 2008, J Prosthodont, V17, P9
[3]   Reliability and properties of core materials for all-ceramic dental restorations [J].
Ban, Seiji .
JAPANESE DENTAL SCIENCE REVIEW, 2008, 44 (01) :3-21
[4]   Resin-ceramic bonding: a review of the literature [J].
Blatz, MB ;
Sadan, A ;
Kern, M .
JOURNAL OF PROSTHETIC DENTISTRY, 2003, 89 (03) :268-274
[5]   Fracture surface roughness and toughness of Al2O3-platelet reinforced glass matrix composites [J].
Boccaccini, AR ;
Winkler, V .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2002, 33 (01) :125-131
[6]   Pressed ceramics onto zirconia. Part 1: Comparison of crystalline phases present, adhesion to a zirconia system and flexural strength [J].
Choi, Jung Eun ;
Waddell, J. Neil ;
Torr, Brendan ;
Swain, Michael Vincent .
DENTAL MATERIALS, 2011, 27 (12) :1204-1212
[7]  
Çiftçi Y, 2000, INT J ORAL MAX IMPL, V15, P571
[8]  
Craig R., 2004, Dental materials: properties and manipulation, V8a, P578
[9]   Influence of surface treatments and resin cement selection on bonding to densely-sintered zirconium-oxide ceramic [J].
de Oyague, Raquel Castillo ;
Monticelli, Francesca ;
Toledano, Manuel ;
Osorio, Estrella ;
Ferrari, Marco ;
Osorio, Raquel .
DENTAL MATERIALS, 2009, 25 (02) :172-179
[10]  
Dong J K, 1992, Int J Prosthodont, V5, P9