Evaluation of interfacial properties by embedded single fibre test in aramid/epoxy composites

被引:0
作者
Kitagawa, K [1 ]
Hayasaki, S
Hamada, H
Maekawa, Z
Ikuta, N
机构
[1] Kyoto Municipal Inst Ind Res, Shimogyo Ku, Kyoto 6008813, Japan
[2] Kyoto Inst Technol, Sakyo Ku, Kyoto 606, Japan
[3] Shonan Inst Technol, Fujisawa, Kanagawa 251, Japan
关键词
interphase; aramid composites; embedded single filament; tensile test; compression test; sizing treatment;
D O I
暂无
中图分类号
TB33 [复合材料];
学科分类号
摘要
An embedded single filament test using aramid fibre has been carried out, not only in tensile mode but also in compressive mode. In the tensile test, all single filaments embedded under various pre-tensions are not fractured until the specimen's break, so that embedded single filament tensile test was not suitable for an evaluation method of the aramid/epoxy interphase. In the compressive test, optical microscope observations indicate the dark zone of/around the embedded single filament after testing. As compressive stress increases, a kink band is generated at first, then kink bands are immediately developed all over the length of the filament and the field becomes clearer. The dark zone first appears after the plastic deformation of the specimen. The intensity of the dark zone measured by image analysis for the micrographs has a linear relationship with the transverse tensile strain which is measured by two strain gauges on the specimen. These results suggest that the dark zone is due to damage of the interface by the transverse tensile strain under longitudinal compressive stress to the specimen. This suggests that it is possible to evaluate the interfacial properties by the measurement of the intensity and the aspect of the dark zone at a constant transverse tensile strain.
引用
收藏
页码:169 / 183
页数:15
相关论文
共 18 条
[1]   FRAGMENTATION OF ARAMID FIBERS IN SINGLE-FIBER MODEL COMPOSITES [J].
ANDREWS, MC ;
YOUNG, RJ .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (22) :5607-5616
[2]   Experimental evaluation of residual stresses in single fibre composites by means of the fragmentation test [J].
Detassis, M ;
Pegoretti, A ;
Migliaresi, C ;
Wagner, HD .
JOURNAL OF MATERIALS SCIENCE, 1996, 31 (09) :2385-2392
[3]   COMPRESSIVE AND TORSIONAL BEHAVIOR OF KEVLAR-49 FIBER [J].
DETERESA, SJ ;
ALLEN, SR ;
FARRIS, RJ ;
PORTER, RS .
JOURNAL OF MATERIALS SCIENCE, 1984, 19 (01) :57-72
[4]   NEW EVALUATION TECHNIQUE OF INTERFACIAL PROPERTIES IN GFRP [J].
HAMADA, H ;
NISHIDA, N ;
MAEKAWA, Z ;
IKUTA, N .
JOURNAL OF MATERIALS SCIENCE, 1994, 29 (02) :352-355
[5]   Evaluation method for the interfacial property by single fibre embedded compression test [J].
Hamada, H ;
Sogabe, K ;
Oya, N ;
Ikuta, N .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1995, 14 (23) :1710-1711
[6]   COMPARISON OF METHODS FOR THE MEASUREMENT OF FIBER MATRIX ADHESION IN COMPOSITES [J].
HERRERAFRANCO, PJ ;
DRZAL, LT .
COMPOSITES, 1992, 23 (01) :2-27
[7]   Evaluation of interfacial mechanical properties of fiber reinforced composites using the microindentation method [J].
Ho, H ;
Drzal, LT .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 1996, 27 (10) :961-971
[8]   EVALUATION OF INTERFACIAL PROPERTIES IN GLASS-FIBER EPOXY-RESIN COMPOSITES - RECONSIDERATION OF AN EMBEDDED SINGLE FILAMENT SHEAR-STRENGTH TEST [J].
IKUTA, N ;
MAEKAWA, Z ;
HAMADA, H ;
ICHIHASHI, M ;
NISHIO, E .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (17) :4663-4666
[9]  
IKUTA N, 1988, INTERFACES POLYM CER, P611
[10]   PHOTO-CROSS-LINKABLE LIQUID-CRYSTALLINE SIDE-CHAIN POLYSILOXANES [J].
KELLER, P .
CHEMISTRY OF MATERIALS, 1990, 2 (01) :3-4