Effects of Ni nanoparticles addition on the microstructure, electrical and mechanical properties of Sn-Ag-Cu alloy

被引:45
作者
Gain, Asit Kumar [1 ]
Zhang, Liangchi [1 ]
机构
[1] Univ New South Wales, Sch Mech & Mfg Engn, Lab Precis & Nano Proc Technol, Sydney, NSW 2052, Australia
关键词
SAC305-0.5Ni composite solder; SAC305; Cu-substrate; Microstructure; Electrical resistivity; Mechanical properties; LEAD-FREE SOLDER; INTERFACIAL REACTIONS; DAMPING PROPERTIES; SHEAR-STRENGTH; JOINTS; BI; TEMPERATURE; GROWTH; CREEP; WETTABILITY;
D O I
10.1016/j.mtla.2019.100234
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of Ni nanoparticles addition on the microstructure, electrical resistivity and mechanical properties such as elastic/shear moduli, microhardness and creep of Sn-3.0Ag-0.5Cu (SAC305; in wt.%) electronic interconnect materials have been investigated. Microstructure analysis of Sn-3.0Ag-0.5Cu-0.5 Ni nanoparticles (in wt.%) solder revealed that adding Ni nanoparticles has promoted the formation and growth of (Cu, Ni)-Sn intermetallic compound (IMC) in the bulk phase of the samples and the structure of composite material resulted refined. This finer structure and (Cu, Ni)-Sn IMC5 in a composite solder resulted in improved mechanical and electrical properties with respect to the Sn-3Ag-0.5Cu reference alloy. Indeed, a comparison between the reference alloy and composite material doped with 0.5 wt.% Ni nanoparticles indicates that the improvement in elastic and shear modulus was 8% and 11.2%, respectively, whereas the microhardness value was increased about 16.7%. Moreover, in the electronic interconnect systems on organic solderability preservative (OSP)-Cu pad, a scallop-shaped Cu6Sn5 IMC was detected at their interfaces at early stage reaction. Increasing the reaction time, the growth of the Cu6Sn5 and the formation of a very thin Cu3Sn IMC layer was observed. However, in Sn-3.0Ag-0.5Cu-0.5 Ni nanoparticles composite material, a very stable (Cu, Ni)-Sn IMC grew at the interface between composite solder and (OSP)-Cu pad in absence of Cu3Sn IMC. In addition, a relatively fine Ag3Sn and (Cu, Ni)-Sn IMC appeared to be evenly dispersed in beta-Sn matrix and the fine microstructure surely affect the overall properties of solder joints.
引用
收藏
页数:9
相关论文
共 44 条
[1]   EVALUATION OF LEAD-FREE SOLDER JOINTS IN ELECTRONIC ASSEMBLIES [J].
ARTAKI, I ;
JACKSON, AM ;
VIANCO, PT .
JOURNAL OF ELECTRONIC MATERIALS, 1994, 23 (08) :757-764
[2]   Reinforcements at nanometer length scale and the electrical resistivity of lead-free solders [J].
Babaghorbani, P. ;
Nai, S. M. L. ;
Gupta, M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 478 (1-2) :458-461
[3]   Failure mechanisms of solder interconnects under current stressing in advanced electronic packages [J].
Chan, Y. C. ;
Yang, D. .
PROGRESS IN MATERIALS SCIENCE, 2010, 55 (05) :428-475
[4]   Effects of fullerenes reinforcement on the performance of 96.5Sn-3Ag-0.5Cu lead-free solder [J].
Chen, Guang ;
Wu, Fengshun ;
Liu, Changqing ;
Xia, Weisheng ;
Liu, Hui .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 636 :484-492
[5]   Effects of Ce Addition on the Microstructure and Mechanical Properties of Sn-58Bi Solder Joints [J].
Chuang, Tung-Han ;
Wu, Hsing-Fei .
JOURNAL OF ELECTRONIC MATERIALS, 2011, 40 (01) :71-77
[6]   Impression creep characterization of rapidly cooled Sn-3.5Ag solders [J].
Dutta, I ;
Park, C ;
Choi, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 379 (1-2) :401-410
[7]   Improved strength of Ni and Zn-doped Sn-2.0Ag-0.5Cu lead-free solder alloys under controlled processing parameters [J].
El-Daly, A. A. ;
El-Taher, A. M. .
MATERIALS & DESIGN, 2013, 47 :607-614
[8]   Synthesis and melting behaviour of Bi, Sn and Sn-Bi nanostructured alloy [J].
Frongia, F. ;
Pilloni, M. ;
Scano, A. ;
Ardu, A. ;
Cannas, C. ;
Musinu, A. ;
Borzone, G. ;
Delsante, S. ;
Novakovic, R. ;
Ennas, G. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 623 :7-14
[9]   The effects of TiO2 nanoparticles addition on the thermal shock resistance, shear strength and IMC layer growth of SAC305 alloy [J].
Gain, Asit Kumar ;
Zhang, Liangchi .
MATERIALIA, 2018, 3 :64-73
[10]   Growth nature of in-situ Cu6Sn5-phase and their influence on creep and damping characteristics of Sn-Cu material under high-temperature and humidity [J].
Gain, Asit Kumar ;
Zhang, Liangchi .
MICROELECTRONICS RELIABILITY, 2018, 87 :278-285