Evolution of aluminum particle-involved phase transformation and pore structure in an elemental Fe-Mn-Al-C powder compact during vacuum sintering

被引:15
作者
Xu, Zhigang [1 ,3 ,4 ]
Du, Jingheng [1 ,4 ]
Zhuang, Chuanbing [2 ]
Huang, Shangyu [2 ,5 ]
Wang, Chuanbin [3 ]
Shen, Qiang [3 ]
机构
[1] Wuhan Univ Technol, Hubei Key Lab Adv Technol Automot Components, Wuhan 430070, Peoples R China
[2] Wuhan Univ Technol, Sch Mat Sci & Engn, Wuhan 430070, Peoples R China
[3] Wuhan Univ Technol, State Key Lab Adv Technol Mat Synth & Proc, Wuhan 430070, Peoples R China
[4] Wuhan Univ Technol, Hubei Collaborat Innovat Ctr Automot Components T, Wuhan 430070, Peoples R China
[5] Wuhan Univ Technol, Hubei Engn Res Ctr Green Precis Mat Forming, Wuhan 430070, Peoples R China
基金
中国国家自然科学基金;
关键词
Powder metallurgy; Aluminum particle-involved diffusion/reaction; Vacuum sintering; Phase transformation; Pore-formation mechanism; STAINLESS-STEEL FOAMS; POROUS CARBON-STEEL; MECHANICAL-PROPERTIES; DEFORMATION-BEHAVIOR; FABRICATION; POROSITY; METALLURGY; SYSTEM; ALLOYS; STATE;
D O I
10.1016/j.vacuum.2020.109289
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, a quaternary elemental Fe-Mn-Al-C powder compact was sintered at various temperatures (<= 700 degrees C) in vacuum, in order to clarify Al particle-involved pore evolution. This is an essential part of work to thoroughly understand the pore-forming process of the porous high-Mn and high-Al FeMnAl steels. The phase compositions, porosities and microstructure of the sintered samples were comprehensively investigated. It was found that phase transformations started at similar to 550 degrees C, where brand-new FeAl, Fe2Al5, Al8Mn5 and Al11Mn4 phases were generated depending on sintering temperature. Residual elemental Al particles still existed after sintering at 660 degrees C, and it disappeared completely when the temperature reached 700 degrees C. Al particle-involved diffusion/reactions played a key role in the increase of porosities, especially open porosity. No change in porosities occurred if the sintering temperature was <= 500 degrees C. Afterwards, the porosities increased steadily with the increase of the sintering temperature. The total and open porosity of the 700 degrees C-sintered compacts significantly increased by similar to 144% and 235% with respect to the green compacts. It was also found that isothermal holding time had limited impact on phase transitions and pore evolution.
引用
收藏
页数:10
相关论文
共 63 条
[21]   Experimental Investigation on Steel Foams Fabricated by Sintering-Dissolution Process [J].
Guo, Kunshan ;
Li, Mingchao ;
Gong, Quan ;
Li, Congshan ;
Li, Chunhui ;
Zhong, Hao ;
Zhou, Yun .
MATERIALS AND MANUFACTURING PROCESSES, 2016, 31 (12) :1597-1602
[22]   Influence of Al content and precipitation state on the mechanical behavior of austenitic high-Mn low-density steels [J].
Gutierrez-Urrutia, I. ;
Raabe, D. .
SCRIPTA MATERIALIA, 2013, 68 (06) :343-347
[23]   AN ASSESSMENT OF THE FE-MN SYSTEM [J].
HUANG, WM .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 1989, 13 (03) :243-252
[24]   Fabrication of lotus-type porous carbon steel by unidirectional solidification in nitrogen atmosphere [J].
Kashihara, M ;
Hyun, SK ;
Yonetani, H ;
Kobi, T ;
Nakajima, H .
SCRIPTA MATERIALIA, 2006, 54 (04) :509-512
[25]   Fabrication of lotus-type porous carbon steel via continuous zone melting and its mechanical properties [J].
Kashihara, M. ;
Yonetani, H. ;
Kobi, T. ;
Hyun, S. K. ;
Suzuki, S. ;
Nakajima, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 524 (1-2) :112-118
[26]   Deformation behavior of open-cell stainless steel foams [J].
Kaya, A. C. ;
Fleck, C. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 615 :447-456
[27]   Strain hardening reduces energy absorption efficiency of austenitic stainless steel foams while porosity does not [J].
Kaya, Ali Can ;
Zaslansky, Paul ;
Ipekoglu, Mehmet ;
Fleck, Claudia .
MATERIALS & DESIGN, 2018, 143 :297-308
[28]   Tensile failure observations in sintered steel foam struts revealed by sub-micron contrast-enhanced microtomography [J].
Kaya, Ali Can ;
Zaslansky, Paul ;
Nikolaus, Anneke ;
Fleck, Claudia .
MATERIALS & DESIGN, 2016, 105 :190-200
[29]   Filtering Properties of Porous Materials Made of Thin Stainless Steel Fibers [J].
Kirichenko, O. V. ;
Klimenko, V. N. ;
Shapoval, I. V. ;
Valeeva, I. K. .
POWDER METALLURGY AND METAL CERAMICS, 2015, 54 (3-4) :151-155
[30]   Magnetic properties of mechanically alloyed Mn-Al-C powders [J].
Kohmoto, O. ;
Kageyama, N. ;
Kageyama, Y. ;
Haji, H. ;
Uchida, M. ;
Matsushima, Y. .
2ND INTERNATIONAL SYMPOSIUM ON ADVANCED MAGNETIC MATERIALS AND APPLICATIONS (ISAMMA 2010), 2011, 266