Development of pyrolysis models for charring polymers

被引:50
作者
Li, Jing [1 ,2 ]
Gong, Junhui [3 ]
Stoliarov, Stanislav I. [1 ]
机构
[1] Univ Maryland, Dept Fire Protect Engn, College Pk, MD 20742 USA
[2] Univ New Haven, Dept Fire Sci & Profess Studies, Henry C Lee Coll Criminal Justice & Forens Sci, West Haven, CT 06516 USA
[3] Nanjing Univ Technol, Coll Urban Construct & Safety Engn, Nanjing 210009, Jiangsu, Peoples R China
关键词
Polymer flammability; Burning rate; Thermophysical properties; Intumescence; ThermaKin; FIRE-LIKE ENVIRONMENTS; THERMAL-DEGRADATION; THERMODYNAMICS; KINETICS; HEAT;
D O I
10.1016/j.polymdegradstab.2015.03.003
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Controlled atmosphere, radiation-driven gasification experiments were conducted on a series of synthetic polymers including poly(acrylonitrile butadiene styrene), poly(ethylene terephthalate), poly(methyl methacrylate)-poly(vinyl chloride) alloy (Kydex) and polyetherimide. Mass loss rate and non-radiated surface temperature of coupon-sized material samples were measured simultaneously and recorded as a function of time. These temperature data were combined with the results of broadband radiation absorption measurements and previously conducted thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) to characterize the transport of thermal energy inside the gasifying materials through inverse modeling. Subsequently, complete pyrolysis models, based on the kinetics and thermodynamics of the thermal decomposition derived from the TGA and DSC experiments, were formulated and employed to predict the mass loss rate histories obtained at 30-90 kW m(-2) of external radiant heat flux simulating fire exposure. Satisfactory predictions were obtained for all materials with the exception of polyetherimide, which highly intumescent behavior introduced large uncertainties in the gasification conditions. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:138 / 152
页数:15
相关论文
共 35 条
  • [1] [Anonymous], 2013, E135413 ASTM
  • [2] ATREYA A, 1983, THESIS HARVARD U CAM
  • [3] Fire retardant polymers: recent developments and opportunities
    Bourbigot, Serge
    Duquesne, Sophie
    [J]. JOURNAL OF MATERIALS CHEMISTRY, 2007, 17 (22) : 2283 - 2300
  • [4] Flammability properties for charring materials
    Delichatsios, M
    Paroz, B
    Bhargava, A
    [J]. FIRE SAFETY JOURNAL, 2003, 38 (03) : 219 - 228
  • [5] DIBLASI C, 1993, COMBUST SCI TECHNOL, V90, P315
  • [6] Generalized pyrolysis model for combustible solids
    Lautenberger, Chris
    Fernandez-Pello, Carlos
    [J]. FIRE SAFETY JOURNAL, 2009, 44 (06) : 819 - 839
  • [7] Li J., 2014, PhD thesis
  • [8] Gasification experiments for pyrolysis model parameterization and validation
    Li, Jing
    Gong, Junhui
    Stoliarov, Stanislav I.
    [J]. INTERNATIONAL JOURNAL OF HEAT AND MASS TRANSFER, 2014, 77 : 738 - 744
  • [9] Measurement of kinetics and thermodynamics of the thermal degradation for charring polymers
    Li, Jing
    Stoliarov, Stanislav I.
    [J]. POLYMER DEGRADATION AND STABILITY, 2014, 106 : 2 - 15
  • [10] Measurement of kinetics and thermodynamics of the thermal degradation for non-charring polymers
    Li, Jing
    Stoliarov, Stanislav I.
    [J]. COMBUSTION AND FLAME, 2013, 160 (07) : 1287 - 1297