Microstructure and compression behavior of chip consolidated magnesium

被引:8
|
作者
Anilchandra, Adamane R. [1 ]
Basu, Ritwik [2 ]
Samajdar, Indradev [2 ]
Surappa, Mirle K. [1 ,3 ]
机构
[1] Indian Inst Sci, Dept Mat Engn, Bengaluru 560012, Karnataka, India
[2] Indian Inst Technol, Dept Met Engn & Mat Sci, Bombay 400076, Maharashtra, India
[3] Indian Inst Technol Ropar, Rupnagar 140001, Punjab, India
关键词
HALL-PETCH PARAMETERS; MECHANICAL-PROPERTIES; MG ALLOY; HOT EXTRUSION; ROOM-TEMPERATURE; MACHINED CHIPS; DEFORMATION; TENSION; ALUMINUM; TEXTURE;
D O I
10.1557/jmr.2011.411
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Chips produced by turning a commercial purity magnesium billet were cold compacted and then hot extruded at four different temperatures: 250, 300, 350, and 400 degrees C. Cast billets, of identical composition, were also extruded as reference material. Chip boundaries, visible even after 49: 1 extrusion at 400 degrees C, were observed to suppress grain coarsening. Although 250 degrees C extruded chip-consolidated product showed early onset of yielding and lower ductility, fully dense material (extruded at 400 degrees C) had nearly 40% reduction in grain size with 22% higher yield strength and comparable ductility as that of the reference. The study highlights the role of densification and grain refinement on the compression behavior of chip consolidated specimens.
引用
收藏
页码:709 / 719
页数:11
相关论文
共 50 条
  • [1] Microstructure and tensile properties of consolidated magnesium chips
    Anilchandra, A. R.
    Surappa, M. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 560 : 759 - 766
  • [2] Microstructure and damping behaviour of consolidated magnesium chips
    Anilchandra, A. R.
    Surappa, M. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 542 : 94 - 103
  • [3] Effect of compression deformation on the microstructure and corrosion behavior of magnesium alloys
    Snir, Y.
    Ben-Hamu, G.
    Eliezer, D.
    Abramov, E.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 528 : 84 - 90
  • [4] Microstructure and tensile behavior of a friction stir processed magnesium alloy
    Mansoor, Bilal
    Ghosh, A. K.
    ACTA MATERIALIA, 2012, 60 (13-14) : 5079 - 5088
  • [5] Evolution of microstructure and texture of AZ80 magnesium alloy under hot torsion with constant decreasing temperature rate
    Yang, Yongbiao
    Guo, Jinxuan
    Wang, Cuiying
    Jiang, Wenxuan
    Zhang, Zhimin
    Wang, Qiang
    Zhang, Xing
    JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (04) : 1619 - 1637
  • [6] Microstructure and texture evolution during warm compression of the magnesium alloy AZ31
    Jiang Jia
    Andy, Godfreyb
    Liu Qing
    SCIENCE IN CHINA SERIES E-TECHNOLOGICAL SCIENCES, 2009, 52 (01): : 186 - 189
  • [7] Asymmetry evolutions in microstructure and strain hardening behavior between tension and compression for AZ31 magnesium alloy
    Wang, Wenke
    Chen, Wenzhen
    Jung, Jaimyun
    Cui, Chao
    Li, Peng
    Yang, Jianlei
    Zhang, Wencong
    Xiong, Renlong
    Kim, Hyoung Seop
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 844
  • [8] Twinning Behavior of VW53 Magnesium Alloy During Compression at RT
    He, Yanda
    Wu, Di
    Zhang, Chengyu
    Pan, Wenyu
    Wang, Jianqiu
    Zhou, Yizhou
    Sun, Xiaofeng
    Li, Jinguo
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (09) : 2604 - 2613
  • [9] Influence of pre-hardening on microstructure evolution and mechanical behavior of AZ31 magnesium alloy sheet
    He, Junjie
    Jiang, Bin
    Yang, Qingshan
    Li, Xin
    Xia, Xiangsheng
    Pan, Fusheng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 621 : 301 - 306
  • [10] Die geometry influence on the texture and microstructure development during extrusion of AZ31 and ZK60 magnesium alloy chips
    Hendriok, Leo
    Nienaber, Maria
    Kurz, Gerrit
    Ben Khalifa, Noomane
    MATERIALS & DESIGN, 2025, 249