Shear Bond Strength of Resin Cement to Zirconia Ceramic After Aluminum Oxide Sandblasting and Various Laser Treatments

被引:95
|
作者
Akin, Hakan [1 ]
Ozkurt, Zeynep [2 ]
Kirmali, Omer [1 ]
Kazazoglu, Ender [2 ]
Ozdemir, Ali Kemal [1 ]
机构
[1] Cumhuriyet Univ, Dept Prosthodont, Fac Dent, Sivas, Turkey
[2] Yeditepe Univ, Dept Prosthodont, Fac Dent, Istanbul, Turkey
关键词
FIXED PARTIAL DENTURES; DIFFERENT SURFACE TREATMENTS; IN-VITRO EVALUATION; Y-TZP CERAMICS; ND-YAG LASER; FLEXURAL STRENGTH; ROCATEC SYSTEM; LUTING CEMENTS; AIR ABRASION; DURABILITY;
D O I
10.1089/pho.2011.3039
中图分类号
R61 [外科手术学];
学科分类号
摘要
Objective:The aim of this study was to evaluate the effect of different surface treatments; sandblasting, Er:YAG, Nd:YAG, or CO2 laser irradiation on the shear bond strength (SBS) of zirconia ceramic to dentin. Background data:Zirconia is not properly luted with resin cements. Various surface treatment methods have been suggested for zirconia to obtain high bond strength to resin cements. There is no study that compared the effect of different laser types (Er:YAG, Nd:YAG, CO2) with sandblasting on SBS between zirconia and dentin. Methods:One hundred and twenty human maxillary third molar teeth were sectioned 3mm below the occlusal surfaces, embedded in a metal ring with autopolymerizing acrylic resin, and stored in distilled water at 37(0)C. One hundred and twenty disc-shaped zirconia specimens were fabricated (6mm in diameter and 4mm in thickness), and randomly assigned to six groups (n = 20):Group 1, untreated (control); Group 2, sandblasted; Group 3, Er:YAG laser irradiated; Group 4, Nd:YAG laser irradiated with contact; Group 5, Nd:YAG laser irradiated with non-contact; Group 6, CO2 laser irradiated. They were cemented onto the dentin with dual-cured resin cement (Variolink (R)). After they were stored in distilled water at 37(0)C for 24 h, the SBS test was performed at a crosshead speed of 1mm/min. The fractured specimens were examined under a stereomicroscope to evaluate the fracture pattern. Results:Results of this study did not show statistically significant differences between Groups 1 and 2, or among Groups 3, 4 and 5. The lowest SBS was recorded in Group 6 (CO2 laser), and the highest SBS was recorded in Group 4 (Nd:YAG laser with contact), followed by Group 3 (Er:YAG laser). The adhesive failure mode was predominantly observed in Groups 2, 3, 5, and 6. Group 1 showed 45% mixed failure and Group 4 showed 50% mixed failure. Conclusions:This study shows that Er:YAG and Nd:YAG laser treatment increased the bond strength of zirconia compared to sandbasting and CO2 laser treatment.
引用
收藏
页码:797 / 802
页数:6
相关论文
共 50 条
  • [31] The effect of plasma on shear bond strength between resin cement and colored zirconia
    Park, Chan
    Yoo, Seung-Hwan
    Park, Sang-Won
    Yun, Kwi-Dug
    Ji, Min-Kyung
    Shin, Jin-Ho
    Lim, Hyun-Pil
    JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (02) : 118 - 123
  • [32] Effect of Surface Treatments of Zirconia Ceramics on the Bond Strength to Resin Cement
    Cheung, Guy C. K.
    Botelho, Michael G.
    Matinlinna, Jukka P.
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (01) : 49 - 56
  • [33] Effect of different surface shapes formed by femtosecond laser on zirconia-resin cement shear bond strength
    Akpinar, Yusuf Ziya
    Yavuz, Tevfik
    Aslan, Muhammed Ali
    Kepceoglu, Abdullah
    Kilic, Hamdi Sukur
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2015, 29 (03) : 149 - 157
  • [34] Effect of zirconia etching solution on the shear bond strength between zirconia and resin cement
    Sadid-Zadeh, Ramtin
    Strazzella, Anthony
    Li, Rui
    Makwoka, Steven
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (05) : 693 - 697
  • [35] Influence of silanes on the shear bond strength of resin cements to zirconia
    Goekkaya, Figen Akyelken
    Stawarczyk, Bogna
    Haemmerle, Christoph H. F.
    Sailer, Irena
    QUINTESSENCE INTERNATIONAL, 2013, 44 (08): : 591 - 600
  • [36] Influence of Different Surface Pretreatments on Shear Bond Strength of an Adhesive Resin Cement to Various Zirconia Ceramics
    Colombo, Marco
    Gallo, Simone
    Padovan, Sara
    Chiesa, Marco
    Poggio, Claudio
    Scribante, Andrea
    MATERIALS, 2020, 13 (03)
  • [37] Effect of Sandblasting, Silica Coating, and Erbium: Yttrium-Aluminum-Garnet Laser Treatment on the Shear Bond Strength of Self-adhesive Resin Cement to Alumina Ceramics
    Caglar, I.
    Ates, S. M.
    Boztoprak, Y.
    Aslan, Y. U.
    Duymus, Z. Yesil
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2018, 21 (08) : 1000 - 1007
  • [38] Effect of Er,Cr:YSGG Laser Treatment on Microshear Bond Strength of Zirconia to Resin Cement Before and After Sintering
    Ghasemi, Amir
    Kermanshah, Hamid
    Ghavam, Maryam
    Nateghifard, Afshin
    Torabzadeh, Hassan
    Nateghifard, Ardalan
    Zolfagharnasab, Kaveh
    Ahmadi, Hadi
    JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (04) : 377 - 382
  • [39] Effect of femtosecond laser zirconia surface treatment on cement shear bond strength
    Yegin, Elif
    Yavuz, Tevfik
    Aslan, Muhammed Ali
    Atala, Mustafa Hayati
    Sorensen, John A.
    Kilic, Hamdi Sukur
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2022, 36 (18) : 1951 - 1963
  • [40] Influence of cement thickness on resin-zirconia microtensile bond strength
    Lee, Tae-Hoon
    Ahn, Jin-Soo
    Shim, June-Sung
    Han, Chong-Hyun
    Kim, Sun-Jai
    JOURNAL OF ADVANCED PROSTHODONTICS, 2011, 3 (03) : 119 - 125