Impact breakage of pharmaceutical tablets

被引:22
作者
Hare, C. [1 ,2 ]
Bonakdar, T. [1 ]
Ghadiri, M. [1 ]
Strong, J. [3 ]
机构
[1] Univ Leeds, Sch Chem & Proc Engn, Leeds, W Yorkshire, England
[2] Univ Surrey, Dept Chem & Proc Engn, Guildford, Surrey, England
[3] AbbVie, N Chicago, IL USA
关键词
Tablets; Breakage; Impact; Indentation; Fracture; Friability; TENSILE-STRENGTH; INDENTATION TOUGHNESS; MECHANICAL STRENGTH; PARTICULATE SOLIDS; ATTRITION; COMPRESSION; COMPACTION; MODEL;
D O I
10.1016/j.ijpharm.2017.11.066
中图分类号
R9 [药学];
学科分类号
1007 ;
摘要
Tablets are the most common solid dosage form of pharmaceutical active ingredients due to their ease of use. Their dissolution behaviour depends on the particle size distribution and physicochemical properties of the formulation, and the compression process, which need to be optimised for producing consistently robust tablets, as weaker tablets are often prone to breakage during production, transport and end use. Tablet strength is typically determined by diametric compression and friability tests. The former gives rise to propagation of a crack on a plane along the compression axis, whilst the latter, carried out in a rotating drum, incurs surface damage and produces chips and debris. These tests produce different measures of strength, neither of which have been correlated with mechanical properties that are accountable for breakage, i.e. hardness, elastic modulus and fracture toughness. We propose a new method based on single tablet impact testing, following the work of Ghadiri and Zhang, 2002, who analysed particle damage by propagation of sub-surface lateral cracks and identified the fundamental form accountable for impact surface damage to be a lumped parameter related to hardness and fracture toughness. Microindentation, carried out separately, to determine fracture toughness led to complete failure of the tablets, hence an unreliable measurement of fracture toughness and no correlation with the experimental trend. In addition, by assuming the fracture toughness to be proportional to the square root of Young's modulus, the indentation measurements do not correlate well with the impact breakage. The discrepancy between the impact and indentation methods is expected to be due to mechanical property variation across the tablet surface, and with strain rate. The impact method is a more suitable test to describe tablet propensity for attrition as it directly represents the failure mode tablets may experience during processing under well-defined conditions. In contrast, the friability test subjects tablets to a similar breakage mechanism but under less well-defined conditions, whilst the compression test represents a different failure mode that is not representative of stresses incurred during processing.
引用
收藏
页码:370 / 376
页数:7
相关论文
共 30 条
[11]  
Lawn B, 1993, FRACTURE BRITTLE SOL
[12]   Roll compaction/dry granulation: Suitability of different binders [J].
Mangal, Haress ;
Kirsolak, Mehmet ;
Kleinebudde, Peter .
INTERNATIONAL JOURNAL OF PHARMACEUTICS, 2016, 503 (1-2) :213-219
[13]   Determination of the tensile strength of elongated tablets [J].
Pitt, Kendal G. ;
Heasley, Matthew G. .
POWDER TECHNOLOGY, 2013, 238 :169-175
[14]   THE MATERIAL TENSILE-STRENGTH OF CONVEX-FACED ASPIRIN TABLETS [J].
PITT, KG ;
NEWTON, JM ;
RICHARDSON, R ;
STANLEY, P .
JOURNAL OF PHARMACY AND PHARMACOLOGY, 1989, 41 (05) :289-292
[15]   Methods for the practical determination of the mechanical strength of tablets-From empiricism to science [J].
Podczeck, Fridrun .
INTERNATIONAL JOURNAL OF PHARMACEUTICS, 2012, 436 (1-2) :214-232
[16]  
PONTON CB, 1989, MATER SCI TECH SER, V5, P865, DOI 10.1179/026708389790222852
[17]   Break force and tensile strength relationships for curved faced tablets subject to diametrical compression [J].
Shang, C. ;
Sinka, I. C. ;
Jayaraman, B. ;
Pan, J. .
INTERNATIONAL JOURNAL OF PHARMACEUTICS, 2013, 442 (1-2) :57-64
[18]   The effect of processing parameters on pharmaceutical tablet properties [J].
Sinka, I. C. ;
Motazedian, F. ;
Cocks, A. C. F. ;
Pitt, K. G. .
POWDER TECHNOLOGY, 2009, 189 (02) :276-284
[19]   The effect of wall friction in the compaction of pharmaceutical tablets with curved faces: a validation study of the Drucker-Prager Cap model [J].
Sinka, IC ;
Cunningham, JC ;
Zavaliangos, A .
POWDER TECHNOLOGY, 2003, 133 (1-3) :33-43
[20]  
Sinka IC, 2007, HANDB POWD TECHNOL, V12, P941, DOI 10.1016/S0167-3785(07)12025-X