Use of heavy liquid metals (HLM), such as the Lead-Bismuth eutectic (LBE), is foreseen for targets and coolants in the newly designed accelerator driven systems (ADS). However, most of the structural materials suffer severe damage when in contact with the HLM. In particular, the simultaneous presence of load and environment can induce a phenomenon named Liquid Metal Embrittlement (LME) in the reference material (ferritic-martensitic steel T91). This phenomenon could give rise to high crack growth rates and the abrupt collapse of the structural material. In this study the effect of LBE on the crack growth rate of the T91 steel was evaluated. The effect of pre-exposure to flowing LBE was considered and assessed in terms of crack growth rates and fracture surface appearance. It was concluded that if conditions for wetting were reached during exposure in LBE, e.g. by dissolution or rupture of protective oxide layers, LME was likely to occur under stress, at 300 degrees C, regardless of the LBE chemistry. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:21 / 29
页数:9
相关论文
共 16 条
[1]  
Agostini P., 2010, J NUCL MAT UNPUB
[2]   Mechanical properties of martensitic steels after exposure to flowing liquid metals [J].
Aiello, A ;
Agostini, M ;
Benamati, G ;
Long, B ;
Scaddozzo, G .
JOURNAL OF NUCLEAR MATERIALS, 2004, 335 (02) :217-221
[3]   Role of oxidation on LME of T91 steel studied by small punch test [J].
Auger, T. ;
Serre, I. ;
Lorang, G. ;
Hamouche, Z. ;
Gorse, D. ;
Vogt, J. -B. .
JOURNAL OF NUCLEAR MATERIALS, 2008, 376 (03) :336-340
[4]   Effect of contact conditions on embrittlement of T91 steel by lead-bismuth [J].
Auger, T ;
Lorang, G ;
Guérin, S ;
Pastol, JL ;
Gorse, D .
JOURNAL OF NUCLEAR MATERIALS, 2004, 335 (02) :227-231
[5]   Investigation of the sensitivity to EAC of steel T91 in contact with liquid LBE [J].
Di Gabriele, F. ;
Doubkova, A. ;
Hojna, A. .
JOURNAL OF NUCLEAR MATERIALS, 2008, 376 (03) :307-311
[6]  
Gabetta G., CORROSION NACE 2000
[7]   Synergy effect of LBE and hydrogenated helium on resistance to LME of T91 steel grade [J].
Guerin, S ;
Pastol, JL ;
Leroux, C ;
Gorse, D .
JOURNAL OF NUCLEAR MATERIALS, 2003, 318 :339-347
[8]   Temperature effect in the maximum propagation rate of a liquid metal filled crack: The T91 martensitic steel/Lead-Bismuth Eutectic system [J].
Hadjem-Hamouche, Z. ;
Auger, T. ;
Guillot, I. .
CORROSION SCIENCE, 2009, 51 (11) :2580-2587
[9]   Susceptibility to LME of 316L and T91 steels by LBE: Effect of strain rate [J].
Hamouche-Hadjem, Zehoua ;
Auger, Thierry ;
Guillot, Ivan ;
Gorse, Dominique .
JOURNAL OF NUCLEAR MATERIALS, 2008, 376 (03) :317-321
[10]  
James L.A., 1985, PREDICTIVE CAPABILIT, V99, P363