Melting of High-Nitrogen Austenitic Steels at Atmospheric Pressure

被引:1
作者
Muradyan, O. S. [1 ]
Muradyan, S. O. [2 ]
机构
[1] ZAO Izhevsk Test Mech Plant, Izhevsk, Russia
[2] Russian Acad Sci, AA Baikov IMET, Moscow, Russia
关键词
high-nitrogen austenitic steels; nitrogen concentration; smelting at atmospheric pressure; nitrogen bubble pressure;
D O I
10.1007/s11015-019-00904-w
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The article considers conditions for nitrogen bubble formation at the crystallization front for iron and stainless steels. Using the results obtained during plasma-arc remelting, a semi-empirical formula is proposed for calculating maximum permissible nitrogen concentrations. It is shown that during steel crystallization with austenite formation at atmospheric pressure it is possible to obtain dense steel ingots with a nitrogen content exceeding its solubility at the liquidus temperature by a factor of 1.4-1.5.
引用
收藏
页码:667 / 671
页数:5
相关论文
共 10 条
  • [1] Melting of High-Nitrogen Austenitic Steels at Atmospheric Pressure
    O. S. Muradyan
    S. O. Muradyan
    Metallurgist, 2019, 63 : 667 - 671
  • [2] Effect of vanadium-alloying on hydrogen embrittlement of austenitic high-nitrogen steels
    Maier, Galina
    Astafurova, Elena
    Moskvina, Valentina
    Melnikov, Evgeny
    Astafurov, Sergey
    Burlachenko, Alexander
    Galchenko, Nina
    ECF22 - LOADING AND ENVIRONMENTAL EFFECTS ON STRUCTURAL INTEGRITY, 2018, 13 : 1053 - 1058
  • [3] Scale-Bridging Analysis on Deformation Behavior of High-Nitrogen Austenitic Steels
    Lee, Tae-Ho
    Ha, Heon-Young
    Hwang, Byoungchul
    Kim, Sung-Joon
    Shin, Eunjoo
    Lee, Jong Wook
    MICROSCOPY AND MICROANALYSIS, 2013, 19 : 77 - 82
  • [4] Work-hardening behavior and evolution of dislocation-microstructures in high-nitrogen bearing austenitic steels
    Kubota, S
    Xia, Y
    Tomota, Y
    ISIJ INTERNATIONAL, 1998, 38 (05) : 474 - 481
  • [5] Correlation of austenite stability and ductile-to-brittle transition behavior of high-nitrogen 18Cr-10Mn austenitic steels
    Hwang, Byoungchul
    Lee, Tae-Ho
    Park, Seong-Jun
    Oh, Chang-Seok
    Kim, Sung-Joon
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (24): : 7257 - 7266
  • [6] Ductile-to-Brittle Transition Behavior of High-Nitrogen 18Cr-10Mn-0.35N Austenitic Steels Containing Ni and Cu
    Hwang, Byoungchul
    Lee, Tae-Ho
    Park, Seong-Jun
    Oh, Chang-Seok
    Kim, Sung-Joon
    PRICM 7, PTS 1-3, 2010, 654-656 : 158 - 161
  • [7] Isothermal aging treatment and its effect on the mechanical properties of Fe-Cr-Mn high-nitrogen austenitic steel
    Ararat, Ozge
    Erisir, Ersoy
    MATERIALS RESEARCH EXPRESS, 2024, 11 (06)
  • [8] Structural stability of austenitic CrMn(Mo)N steels for high-strength, corrosion-resistant retaining rings
    Gavriljuk, VG
    Stein, G
    Berns, H
    STEEL RESEARCH INTERNATIONAL, 2003, 74 (07) : 444 - 452
  • [9] Nitrogen concentration control in diamonds grown in Co-(Fe)-Ti/Al solvents under high-pressure and high-temperature
    Miyakawa, Masashi
    Shinei, Chikara
    Taniguchi, Takashi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2022, 61 (04)