共 50 条
[41]
Micro-cracking mechanism of RENE 108 thin-wall components built by laser powder bed fusion additive manufacturing
[J].
MATERIALS TODAY COMMUNICATIONS,
2022, 30
[42]
Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High ?' CoNi-Base Superalloy
[J].
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
2023, 54 (05)
:1744-1757
[44]
Effect of pre-welding condition on liquation cracking characteristics of K439B superalloy laser welding
[J].
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T,
2025, 36
:7950-7962
[47]
Effects of the Hot Isostatic Pressing Process on Crack Healing of the Laser Repair-Welded CM247LC Superalloy
[J].
METALS,
2016, 6 (10)
[49]
Susceptibility to environmentally induced cracking of laser-welded NiTi wires in Hanks' solution at open-circuit potential
[J].
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,
2012, 544
:38-47