Characteristic changes of deuterium retention on tungsten surfaces due to low-energy helium plasma pre-exposure

被引:61
|
作者
Nishijima, D
Sugimoto, T
Iwakiri, H
Ye, MY
Ohno, N
Yoshida, N
Takamura, S
机构
[1] Nagoya Univ, Grad Sch Engn, Dept Energy Engn & Sci, Chikusa Ku, Nagoya, Aichi 4648603, Japan
[2] Kyushu Univ, RI AM, Kasuga, Fukuoka, Japan
关键词
deuterium retention; helium; NAGDIS-II; tungsten;
D O I
10.1016/j.jnucmat.2004.10.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Deuterium retention in tungsten increases substantially when it is pre-exposed to low-energy He plasma at a high temperature (1600 K), while it decreases when pre-exposed at a low temperature (700 K). The increase of deuterium retention could be attributed to the submicron-sized He bubbles and secondary interstitial defects formed on the tungsten surface. Occupation of trap sites by He atoms during the He pre-exposure at low temperature could decreases the effective number of available trap sites for deuterium atoms, which would decreases the deuterium retention on the tungsten surface. (c) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:927 / 931
页数:5
相关论文
共 50 条
  • [1] Suppression of blister formation and deuterium retention on tungsten surface due to mechanical polishing and helium pre-exposure
    Nishijima, D
    Iwakiri, H
    Amano, K
    Ye, MY
    Ohno, N
    Tokunaga, K
    Yoshida, N
    Takamura, S
    NUCLEAR FUSION, 2005, 45 (07) : 669 - 674
  • [2] Deuterium retention in tungsten exposed to low-energy pure and helium-seeded deuterium plasmas
    Ogorodnikova, O. V.
    Schwarz-Selinger, T.
    Sugiyama, K.
    Alimov, V. Kh.
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (01)
  • [3] Deuterium supersaturation in low-energy plasma-loaded tungsten surfaces
    Gao, L.
    Jacob, W.
    von Toussaint, U.
    Manhard, A.
    Balden, M.
    Schmid, K.
    Schwarz-Selinger, T.
    NUCLEAR FUSION, 2017, 57 (01)
  • [4] Surface blistering and deuterium retention in tungsten exposed to low-energy deuterium plasma at different temperatures
    Qin, Shaoyang
    Wang, Jinliang
    Gao, Liang
    Cheng, Long
    Yuan, Yue
    Jacob, Wolfgang
    Lu, Guang-Hong
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2019, 450 (210-214): : 210 - 214
  • [5] Deuterium retention in plasma sprayed tungsten exposed to low energy deuterium plasma
    Rusinov, Aleksandr
    Sakamoto, Mizuki
    Zushi, Hideki
    Ohyama, Ryohei
    Honda, Koichiro
    Tanabe, Tetsuo
    Yoshida, Naoaki
    Plasma and Fusion Research, 2013, 8 (2013)
  • [6] Deuterium retention in plasma spray tungsten coatings exposed to low-energy, high flux D plasma
    Alimov, V. Kh.
    Nakamura, H.
    Tyburska-Pueschel, B.
    Ogorodnikova, O. V.
    Roth, J.
    Isobe, K.
    Yamanishi, T.
    JOURNAL OF NUCLEAR MATERIALS, 2011, 414 (03) : 479 - 484
  • [7] Temperature dependence of blistering and deuterium retention in tungsten exposed to high-flux and low-energy deuterium plasma
    Shu, W. M.
    Isobe, K.
    Yamanishi, T.
    FUSION ENGINEERING AND DESIGN, 2008, 83 (7-9) : 1044 - 1048
  • [8] Deuterium accumulation in tungsten under low-energy high-flux plasma exposure
    Grigorev P.Y.
    Dubinko V.I.
    Terentyev D.A.
    Bakaev A.V.
    Zhurkin E.E.
    Journal of Surface Investigation, 2014, 8 (02): : 234 - 238
  • [9] Surface morphology and deuterium retention in tungsten exposed to low-energy, high flux pure and helium-seeded deuterium plasmas
    Alimov, V. Kh
    Shu, W. M.
    Roth, J.
    Sugiyama, K.
    Lindig, S.
    Balden, M.
    Isobe, K.
    Yamanishi, T.
    PHYSICA SCRIPTA, 2009, T138
  • [10] Deuterium retention in chemically vapor deposited tungsten carbide coatings and hot-rolled tungsten exposed to low-energy deuterium plasma
    Vladimir Kh. Alimov
    Joachim Roth
    Tungsten, 2022, 4 : 10 - 19