Seven-year dentin bond strengths of a total- and self-etch system

被引:29
作者
Burrow, MF [1 ]
Harada, N
Kitasako, Y
Nikaido, T
Tagami, J
机构
[1] Univ Melbourne, Sch Dent Sci, Parkville, Vic 3010, Australia
[2] Tokyo Med & Dent Univ, Grad Sch, Dept Restorat Sci, Tokyo, Japan
[3] Tokyo Med & Dent Univ, COE Program, Tokyo, Japan
关键词
adhesion; dentin bond; durability; self-etching; tensile bond strength;
D O I
10.1111/j.1600-0722.2005.00213.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The aim of this study was to determine the durability of tensile bond strengths of a conventional 3-step bonding system (Superbond D-liner Plus) and a self-etching priming bonding system (Clearfil Liner Bond II) to bovine dentin over a 7 yr period. Superficial bovine dentin finished with 600-grit SiC paper was bonded with one of the two adhesive materials. A 4 mm diameter area was bonded, covered with resin composite and stored in 37 degrees C deionized water containing gypsum chips and 0.4% sodium azide as an antibacterial. Bonds were stressed in tension at a crosshead speed of 1 mm min(-1). Mean bond strengths were observed at 1 d, at 1, 3, and 6 months, and at 1, 2, 3, 6 and 7 yr. Ten specimens were tested for the first 3 yr and 15 specimens were tested for 6 and 7 yr. The bond strength of Superbond D-liner Plus significantly decreased over the 7 yr period, whereas Liner Bond II showed a slight but, insignificant, decrease. The fracture mode changed with time for Superbond D-liner Plus, but not for Liner Bond II. It was concluded that systems which use a strong acid for demineralizing the dentin may show greater deterioration of the bond to dentin compared with a self-etching priming system.
引用
收藏
页码:265 / 270
页数:6
相关论文
共 26 条
[1]  
Armstrong SR, 2003, J ADHES DENT, V5, P47
[2]   THE INFLUENCE OF AGE AND DEPTH OF DENTIN ON BONDING [J].
BURROW, MF ;
TAKAKURA, H ;
NAKAJIMA, R ;
INAI, N ;
TAGAMI, J ;
TAKATSU, T .
DENTAL MATERIALS, 1994, 10 (04) :241-246
[3]   Dentin bond durability after three years using a dentin bonding agent with and without priming [J].
Burrow, MF ;
Satoh, M ;
Tagami, J .
DENTAL MATERIALS, 1996, 12 (5-6) :302-307
[4]  
Burrow Michael F., 1993, Bulletin of Tokyo Medical and Dental University, V40, P173
[5]   Four-year water degradation of total-etch adhesives bonded to dentin [J].
De Munck, J ;
Van Meerbeek, B ;
Yoshida, Y ;
Inoue, S ;
Vargas, M ;
Suzuki, K ;
Lambrechts, P ;
Vanherle, G .
JOURNAL OF DENTAL RESEARCH, 2003, 82 (02) :136-140
[6]   Degradation patterns of different adhesives and bonding procedures [J].
Hashimoto, M ;
Ohno, H ;
Sano, H ;
Kaga, M ;
Oguchi, H .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2003, 66B (01) :324-330
[7]   In vivo degradation of resin-dentin bonds in humans over 1 to 3 years [J].
Hashimoto, M ;
Ohno, H ;
Kaga, M ;
Endo, K ;
Sano, H ;
Oguchi, H .
JOURNAL OF DENTAL RESEARCH, 2000, 79 (06) :1385-1391
[8]   The microtensile strength of bonding resins [J].
Hogan, LC ;
Burrow, MF .
AUSTRALIAN DENTAL JOURNAL, 2001, 46 (03) :194-197
[9]   The effect of thermocycling and dentine pre-treatment on the durability of the bond between composite resin and dentine [J].
Huang, MS ;
Li, MT ;
Huang, FM ;
Ding, SJ .
JOURNAL OF ORAL REHABILITATION, 2004, 31 (05) :492-499
[10]  
Inoue S, 2001, J Adhes Dent, V3, P237