The production of copper parts using DMLR

被引:87
作者
Pogson, SR [1 ]
Fox, P [1 ]
Sutcliffe, CJ [1 ]
O'Neill, W [1 ]
机构
[1] Univ Liverpool, Mfg Sci & Engn Res Ctr, Dept Engn, Liverpool L69 3BX, Merseyside, England
关键词
lasers; melting; rapid prototypes; copper;
D O I
10.1108/13552540310502239
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The relationship between the major process variables (laser power, laser scan speed, scan length, beam overlap and Q-switch pulse frequency) of direct metal laser re-melting and their effect on the structure of single- and multi-layer copper coupons has been investigated. The work successfully produced selectively fused copper powder layers and simple three-dimensional copper structures with suitable laser parameters being identified for the production of parts, including thin-walled cubic structures. it was shown that the specific energy density needed to melt thick powder beds was less than that to melt multi-layer builds and that the type of substrate material used significantly affected the process parameters. Thus, the substrate and its thermal properties have a significant effect on the melt pool size and freezing rate.
引用
收藏
页码:334 / 343
页数:10
相关论文
共 13 条
[1]  
Amon C, 1993, P SOL FREEF FABR S A, P1
[2]  
ARTHUR G, 1954, J I MET, V83, P329
[3]  
CARTER WT, 1993, SOL FREEF FABR P, P54
[4]  
DAS S, 2001, SOLID FREEFORM FABRI, P85
[5]  
Karapatis NP, 1999, SOL FREEFORM FABRIC, P255
[6]  
Lide D., 2002, HDB CHEM PHYS, P12
[7]   Use of metallic stents and balloons in the esophagus and gastrointestinal tract [J].
Morgan, R ;
Adam, A .
JOURNAL OF VASCULAR AND INTERVENTIONAL RADIOLOGY, 2001, 12 (03) :283-297
[8]   Experimental investigation of nanosecond pulsed Nd:YAG laser re-melted pre-placed powder beds [J].
Morgan, R ;
Sutcliffe, CJ ;
O'Neill, W .
RAPID PROTOTYPING JOURNAL, 2001, 7 (03) :159-172
[9]  
Morgan R., 2001, RAPID PROTOTYPING J
[10]  
STEEN WM, 1998, LASER MAT PROCESSING, P68