Investigation on scratching force and material removal mechanism of 3D SiCf/C-SiC composites during single grain scratching

被引:31
作者
Zan, Zhuoliang [1 ,2 ]
Guo, Kai [1 ,2 ]
Sun, Jie [1 ,2 ]
Lu, Yuan [1 ,2 ]
Yang, Bin [1 ,2 ]
Jia, Xiujie [1 ,2 ]
Sivalingam, Vinothkumar [1 ,2 ]
Xi, Jianren [3 ]
机构
[1] Shandong Univ, Res Ctr Aeronaut Component Mfg Technol & Equipment, Jinan 250061, Peoples R China
[2] Shandong Univ, Natl Demonstrat Ctr Expt Mech Engn Educ, Sch Mech Engn, Key Lab High efficiency & Clean Mech Manufacture, Jinan 250061, Peoples R China
[3] Shandong Univ, Sch Mat Sci & Engn, Jinan 250061, Peoples R China
关键词
Ceramic -matrix composites (CMCs); Ceramic fibers; Machining; Micro; -mechanics; CERAMIC-MATRIX COMPOSITES; SIC/SIC COMPOSITES; C/SIC COMPOSITES; OPTIMIZATION;
D O I
10.1016/j.jeurceramsoc.2022.05.079
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
As one of the novel fiber-reinforced ceramic matrix composites, SiCf/C-SiC composites are difficult to machine materials and the material removal mechanism is not completely clear yet. Single grain scratching tests with gradual depth have been carried out to analyze the influence of fiber orientation and woven structure on the material removal mechanism and scratching force in three typical scratched surfaces defined by the fiber orientation. Results indicate that the scratching force waveform is affected by the weaving method, fibers orientation, and porosity distribution of the scratched area, resulting in periodic fluctuations. Diamond indenter causes greater damage to the surface of SiCf/C-SiC composites when scratching along transverse fibers, while leaving narrow but deep grooves on the surface when scratching along perpendicular fibers. The dominant mode of material removal of SiCf/C-SiC composites is brittle fracture, and the damage features mainly include direct fiber breakage, matrix fragmentation, fiber pullout, fiber outcropping.
引用
收藏
页码:5366 / 5379
页数:14
相关论文
共 33 条
[1]   Experimental and numerical investigations of single abrasive-grain cutting [J].
Anderson, D. ;
Warkentin, A. ;
Bauer, R. .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2011, 51 (12) :898-910
[2]   Investigations on grinding process of woven ceramic matrix composite based on reinforced fiber orientations [J].
Cao, Xiaoyan ;
Lin, Bin ;
Zhang, Xiaofeng .
COMPOSITES PART B-ENGINEERING, 2015, 71 :184-192
[3]   Transformation of fracture mechanism and damage behavior of ceramic-matrix composites during nano-scratching [J].
Chen, Jie ;
An, Qinglong ;
Chen, Ming .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2020, 130
[4]   Experimental studies on drilling tool load and machining quality of C/SiC composites in rotary ultrasonic machining [J].
Ding, Kai ;
Fu, Yucan ;
Su, Honghua ;
Chen, Yan ;
Yu, Xizhai ;
Ding, Guozhi .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2014, 214 (12) :2900-2907
[5]   New observations of the fiber orientations effect on machinability in grinding of C/SiC ceramic matrix composite [J].
Du, Jinguang ;
Ming, Wuyi ;
Ma, Jun ;
He, Wenbin ;
Cao, Yang ;
Li, Xiaoke ;
Liu, Kun .
CERAMICS INTERNATIONAL, 2018, 44 (12) :13916-13928
[6]   Localized mechanical property assessment of SiC/SiC composite materials [J].
Frazer, D. ;
Abad, M. D. ;
Krumwiede, D. ;
Back, C. A. ;
Khalifa, H. E. ;
Deck, C. P. ;
Hosemann, P. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 70 :93-101
[7]   Hysteresis loop model of unidirectional carbon fiber-reinforced ceramic matrix composites under an arbitrary cyclic load [J].
Gao, Xiguang ;
Fang, Guangwu ;
Song, Yingdong .
COMPOSITES PART B-ENGINEERING, 2014, 56 :92-99
[8]   Some observations in grinding SiC and silicon carbide ceramic matrix composite material [J].
Gong, Yadong ;
Qu, Shuoshuo ;
Yang, Yuying ;
Liang, Chunyou ;
Li, Pengfei ;
She, Yuebing .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 103 (5-8) :3175-3186
[9]  
Hashish M., 2015, INTERTECH 2015 AN IN
[10]   Effects of cyclic tensile loading on the rupture behavior of orthogonal 3-D woven SiC fiber/SiC matrix composites at elevated temperatures in air [J].
Ikarashi, Yoshito ;
Ogasawara, Toshio ;
Aoki, Takuya .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) :806-812