Photoinduced transformations in amorphous Se75Ge25 thin film by XeCl excimer-laser exposure

被引:42
|
作者
Lee, HY
Park, SH
Chun, JY
Chung, HB
机构
[1] Kwangwoon Univ, Dept Elect Mat Engn, Nowon Ku, Seoul 139701, South Korea
[2] Kwangwoon Univ, Inst New Technol, Nowon Ku, Seoul 139701, South Korea
关键词
D O I
10.1063/1.367367
中图分类号
O59 [应用物理学];
学科分类号
摘要
The scalar photoinduced changes of the optical absorption edge and the optical constants in amorphous Se75Ge25 chalcogenide thin film have been studied using XeCl excimer laser Light with a wavelength of 306 nm. The glass transition temperature (T-g) of this material is evaluated to be approximately 220 degrees C, at which the as-deposited film is initially annealed. The optical energy gaps E-op of as-deposited and initially annealed Se75Ge25 thin films are 1.90 and 1.84 eV, respectively. When initially annealed films are exposed to a 4.05 eV excimer laser (much greater than E-op) with energy densities of 100, 120 and 180 mJ/cm(2), a photodarkening effect that exhibits a decrease in the optical transmittance (T-op) and E-op and an increase of the refractive index n and the extinction coefficient k in the vicinity of the absorption edge (1.4-3.0 eV) is observed. In particular, in the case of a thin film exposed by 120 mJ/cm(2), E-op and n + ik measured at 673.7 nm(1.84 eV), i.e., an absorption edge of initially annealed thin him, are 160 eV and 2.680 + i0.118 and the changes of Delta E-op and Delta n + i Delta k are 0.24 eV and 0.215 + i0.100, respectively. Furthermore, these photodarkened thin films recovered (bleached) to the initial annealed state by re-annealing at T-g. As a result of the x-ray diffraction analysis, we can conclude that these changes are due to an amorphous to amorphous transition. Therefore, considering that these large changes in Se75Ge25 thin film lead to its structural changes, we could expect high etch selectivity in using this film as a deep ultraviolet lithography resist. (C) 1998 American Institute of Physics.
引用
收藏
页码:5381 / 5385
页数:5
相关论文
共 17 条
  • [1] The characteristics of an amorphous Se75Ge25 thin film as a positive-type resist in focused-ion-beam lithography
    Lee, H
    Chung, HB
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 1998, 32 (02) : 171 - 175
  • [2] Low-energy focused-ion-beam exposure characteristics of an amorphous Se75Ge25 resist
    Lee, HY
    Chung, HB
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1997, 15 (04): : 818 - 822
  • [3] Amorphous Se75Ge25 resist profile simulation of focused-ion-beam lithography
    Lee, HY
    Chung, HB
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1997, 36 (4A): : 2409 - 2414
  • [4] Amorphous Se75Ge25 resist profile simulation of focused-ion-beam lithography
    Kwangwoon Univ, Seoul, Korea, Republic of
    Jpn J Appl Phys Part 1 Regul Pap Short Note Rev Pap, 4 A (2409-2414):
  • [5] Lithographic properties of SiNx and Se75Ge25 thin films as the low-energy ion-beam resist
    Lee, HY
    Chung, HB
    PROCEEDINGS OF THE 5TH INTERNATIONAL CONFERENCE ON PROPERTIES AND APPLICATIONS OF DIELECTRIC MATERIALS, VOLS 1 AND 2, 1997, : 635 - 638
  • [6] Structural characterization and optical properties of pulsed laser deposition of Se75Te25 and Se75Te17Ge8 amorphous thin films
    Salim, S. M.
    Lahmar, A.
    Zayied, H.
    Salem, A. M.
    Sakr, G. B.
    Teleb, N.
    El Marssi, M.
    MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING, 2015, 39 : 172 - 177
  • [7] Improvements in the Device Performance of Amorphous Indium Gallium Zinc Oxide Thin Film Transistors by XeCl Excimer Laser Irradiation
    Ahn, Byung Du
    Shin, Hyun Soo
    Jeong, Woong Hee
    Kim, Gun Hee
    Kim, Hyun Jae
    Choi, Sung-Hwan
    Han, Min-Koo
    2009 SID INTERNATIONAL SYMPOSIUM DIGEST OF TECHNICAL PAPERS, VOL XL, BOOKS I - III, 2009, : 1170 - +
  • [8] BOTTOM-GATE POLY-SI THIN-FILM TRANSISTORS USING XECL EXCIMER-LASER ANNEALING AND ION DOPING TECHNIQUES
    FURUTA, M
    KAWAMURA, T
    YOSHIOKA, T
    MIYATA, Y
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1993, 40 (11) : 1964 - 1969
  • [9] Application of excimer-laser annealing to amorphous, poly-crystal and single-crystal silicon thin-film transistors
    Matsumura, M
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1998, 166 (02): : 715 - 728
  • [10] Application of excimer-laser annealing to amorphous, poly-crystal and single-crystal silicon thin-film transistors
    Matsumura, M.
    Physica Status Solidi (A) Applied Research, 1998, 166 (02): : 715 - 728