The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel

被引:174
作者
Mohtadi-Bonab, M. A. [1 ]
Szpunar, J. A. [1 ]
Basu, R. [1 ]
Eskandari, M. [1 ]
机构
[1] Univ Saskatchewan, Dept Mech Engn, Saskatoon, SK S7N 5A9, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Hydrogen induced cracking (HIC); Hydrogen charging; Electron backscatter diffraction (EBSD); Energy dispersive spectroscopy (EDS); Grain orientation; Crystallographic texture; STRESS-CORROSION CRACKING; CRYSTALLOGRAPHIC TEXTURE; METALLURGICAL FACTORS; MULTIPHASE STEELS; CARBON-STEEL; EMBRITTLEMENT; BEHAVIOR; MICROSTRUCTURE; IMPACT; DAMAGE;
D O I
10.1016/j.ijhydene.2014.11.057
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Mechanism of failure by hydrogen induced cracking (HIC) in pipeline steel has not been extensively investigated in the past. In the present work, an API X70 pipeline steel was electrochemically charged with hydrogen for different durations in order to find crack nucleation and propagation sites. After 3 h charging, suitable regions for crack initiation and propagation were found. These regions were studied by color metallography, EDS and EBSD techniques. The results brought out that HIC cracks nucleated from regions rich of manganese sulphide inclusions, some complex carbonitride precipitates such as (Ti, Nb, V) (C, N) and further propagated through the segregation area of some elements, such as manganese, carbon, silicon and sulfur. It is worth-mentioning that all these potential sites for crack nucleation and propagation appeared at the center of cross section of the specimens. EBSD measurements were carried out at the center of cross section in as-received and hydrogen-charged specimens in order to find a pattern between microstructural parameters (texture, grain boundary nature and Taylor factor) and probability of HIC cracking. The results showed that fine grain colonies (less than 3.5 mu m in length) with dominant ND parallel to<001> orientations were prone to intergranular HIC crack propagation. The grain boundaries identified between two grains with a mismatch in Taylor factor were more susceptible to intergranular fracture while transgranular fracture occurred in fragmented grains with high and similar Taylor factor that were less likely to yield. HIC cracking occurred in a wide range of orientations such as ND parallel to<123>, ND parallel to<100>, ND parallel to<112>, ND parallel to<110> and even ND parallel to<111>; however, role of high angle grain boundaries and type of fracture would be of great importance in crack propagation. Copyright (C) 2014, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1096 / 1107
页数:12
相关论文
共 40 条
[1]   A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies [J].
Arafin, M. A. ;
Szpunar, J. A. .
CORROSION SCIENCE, 2009, 51 (01) :119-128
[2]  
BEACHEM CD, 1972, METALL TRANS, V3, P437
[3]   The role of hydrogen in microbiologically influenced corrosion and stress corrosion cracking [J].
Biezma, MV .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2001, 26 (05) :515-520
[4]  
Birnbaum H, 1989, NATO C SERIES MAT SC, V5, P20
[5]   Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales [J].
Bridier, F. ;
Villechaise, P. ;
Mendez, J. .
ACTA MATERIALIA, 2008, 56 (15) :3951-3962
[6]   The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking [J].
Carneiro, RA ;
Ratnapuli, RC ;
Lins, VD .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 357 (1-2) :104-110
[7]   Analysis of electrochemical hydrogen permeation through X-65 pipeline steel and its implications on pipeline stress corrosion cracking [J].
Cheng, Y. F. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2007, 32 (09) :1269-1276
[8]  
De AK, 2003, ADV MATER PROCESS, V161, P27
[9]  
DINGLEY DJ, 1995, MICROSCOPY MAT SCI S
[10]   Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking [J].
Dong, C. F. ;
Liu, Z. Y. ;
Li, X. G. ;
Cheng, Y. F. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (24) :9879-9884