共 28 条
Production of (Sm,Zr)(Fe,Co)3 magnets
被引:2
作者:
Saito, Tetsuji
[1
]
机构:
[1] Chiba Inst Technol, Dept Adv Mat Sci & Engn, Narashino, Chiba 2758588, Japan
来源:
关键词:
Sm-Fe alloys;
Melt spinning;
Coercivity;
SM-FE;
INTERMETALLIC COMPOUNDS;
COERCIVITY;
DEMAND;
D O I:
10.1016/j.heliyon.2022.e09612
中图分类号:
O [数理科学和化学];
P [天文学、地球科学];
Q [生物科学];
N [自然科学总论];
学科分类号:
07 ;
0710 ;
09 ;
摘要:
Coercivity This study was aimed at the improvement of SmFe3-based alloys prepared by means of melt-spinning. A systematic study was carried out on (Sm1-xZrx)(Fe0.75Co0.25)(3) (x = 0 -0.4) alloys melt-spun at a wheel speed of 50 m/s and annealed at 773 -1173 K. SmFe3-based melt-spun ribbons with a rhombohedral structure were prepared from the (Sm1-xZrx) (Fe0.75Co0.25)(3) (x = 0 -0.4) alloys. The addition of zirconium increased the coercivity and enhanced the remanence of the melt-spun ribbons. However, the Curie temperature slightly decreased with increasing zirconium content. The optimally annealed alloys, with a composition of (Sm0.7Zr0.3) (Fe0.75Co0.25)(3), achieved a coercivity of 7.8 kOe, a remanence of 6.0 kG, and a Curie temperature of 680K.
引用
收藏
页数:4
相关论文