Surface structure and quenching effects in BiFeO3-BaTiO3 ceramics

被引:24
作者
Wang, Bing [1 ]
Li, Yizhe [1 ]
Hall, David A. [1 ]
机构
[1] Univ Manchester, Dept Mat, Manchester M13 9PL, Lancs, England
关键词
ferroelectricity; ferroelectric materials; lead-free ceramics; piezoelectric materials; properties; quenching effects; PIEZOELECTRIC PROPERTIES; TEMPERATURE; MECHANISMS; INTERPLAY; CONSTANT; STRAIN;
D O I
10.1111/jace.18188
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The structure and properties of Mn-doped 0.67BiFeO(3)-0.33BaTiO(3) ceramics are systematically investigated with respect to the effects of annealing prior to rapid cooling by quenching in air. Air-quenching induces a change in crystal structure from pseudo-cubic to rhombohedral, with higher quenching temperatures leading to an increased rhombohedral distortion. These structural changes are correlated with the appearance of more well-defined ferroelectric domain configurations. It is shown that the surface preparation procedures for XRD measurements can induce significant changes in the peak profiles, indicating differences in crystal structure between the surface and bulk regions. Frequency dispersion in the temperature-dependent relative permittivity for the as-sintered sample is significantly reduced after quenching, accompanied by enhancement of the Curie point and improved temperature-stability of piezoelectric properties. It is proposed that the formation of defect clusters by A-site cation diffusion during cooling is circumvented by quenching, leading to the observed modification of structural distortion and ferroelectric properties.
引用
收藏
页码:1265 / 1275
页数:11
相关论文
共 55 条
[11]   Normal to relaxor ferroelectric transformations in lanthanum-modified tetragonal-structured lead zirconate titanate ceramics [J].
Dai, XH ;
Xu, Z ;
Viehland, D .
JOURNAL OF APPLIED PHYSICS, 1996, 79 (02) :1021-1026
[12]  
Dinnebier RE, 2008, POWDER DIFFRACTION: THEORY AND PRACTICE, P1, DOI 10.1039/9781847558237
[13]  
Dinnebier R, 2019, RIETVELD REFINEMENT: PRACTICAL POWDER DIFFRACTION PATTERN ANALYSIS USING TOPAS, pV, DOI 10.1515/9783110461381-201
[14]   Persistence of ferroelectricity above the Curie temperature at the surface of Pb(Zn1/3Nb2/3)O3-12%PbTiO3 [J].
Domingo, N. ;
Bagues, N. ;
Santiso, J. ;
Catalan, G. .
PHYSICAL REVIEW B, 2015, 91 (09)
[15]  
Erhart J, 2017, TOP MINING METAL MAT, P119, DOI 10.1007/978-3-319-42481-1_4
[16]   Large electric-field-induced strain and enhanced piezoelectric constant in CuO-modified BiFeO3-BaTiO3 ceramics [J].
Gao, Weiwei ;
Lv, Jing ;
Lou, Xiaojie .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2018, 101 (08) :3383-3392
[17]   Structural changes of relaxor ferroelectric Sr0.52Ba0.48Nb2O6 (SBN52) on quenching and reheating [J].
Graetsch, Heribert A. .
ACTA CRYSTALLOGRAPHICA SECTION B-STRUCTURAL SCIENCE CRYSTAL ENGINEERING AND MATERIALS, 2017, 73 :820-826
[18]   Phase evolution and origin of the high piezoelectric properties in lead-free BiFeO3-BaTiO3 ceramics [J].
Habib, Muhammad ;
Lee, Myang Hwan ;
Kim, Da Jeong ;
Choi, Hai In ;
Kim, Myong-Ho ;
Kim, Won-Jeong ;
Song, Tae Kwon .
CERAMICS INTERNATIONAL, 2020, 46 (14) :22239-22252
[19]   Structural, spectroscopic, and dielectric characterizations of Mn-doped 0.67BiFeO3-0.33BaTiO3 multiferroic ceramics [J].
Hang, Qiming ;
Zhou, Wenke ;
Zhu, Xinhua ;
Zhu, Jianmin ;
Liu, Zhiguo ;
Al-Kassab, Talaat .
JOURNAL OF ADVANCED CERAMICS, 2013, 2 (03) :252-259
[20]  
Hardtl K. H., 1982, Ceramics International, V8, P121, DOI 10.1016/0272-8842(82)90001-3