Isothermal oxidation behavior of Nb-bearing austenitic cast steels at 950°C

被引:6
作者
Zhao, Hailong [1 ]
Li, Longfei [1 ]
Feng, Qiang [1 ]
机构
[1] Univ Sci & Technol Beijing, Beijing Adv Innovat Ctr Mat Genome Engn, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
关键词
austenitic cast steels; isothermal oxidation; primary Nb(C; N); internal oxidation; Cr depletion; HIGH-TEMPERATURE OXIDATION; LONG-TERM OXIDATION; A-DEGREES-C; STAINLESS-STEEL; CREEP-BEHAVIOR; MICROSTRUCTURAL CHARACTERIZATION; SMALL ADDITIONS; SILICON CONTENT; ALLOYS; NI;
D O I
10.1007/s12613-021-2314-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The oxidation behaviors of three austenitic cast steels with different morphologies of primary carbides at 950 degrees C in air were investigated using scanning electron microscopy, energy dispersive spectroscopy, and focused ion beam/transmission electron microscopy. Their oxidation kinetics followed a logarithmic law, and the oxidation rate can be significantly decreased as long as a continuous silica layer formed at the scale/substrate interface. When the local Si concentration was inadequate, internal oxidation occurred beneath the oxide scale. The spallation of oxides during cooling can be inhibited with the formation of internal oxidation, owing to the reduced mismatch stress between the oxide scale and the substrate. The "Chinese-script" primary Nb(C,N) was superior to the dispersed primary Nb(C,N) in suppressing the oxidation penetration in the interdendritic region by supplying a high density of quick-diffusion Cr channels. In addition, the innermost and outermost oxidation layers were enriched with Cr, whereas the Cr evaporation in the outermost layer was significant when the water vapor concentration in the environment was high enough. These findings further the understanding regarding the oxidation behavior of austenitic cast steels and will promote the alloy development for exhaust components.
引用
收藏
页码:814 / 824
页数:11
相关论文
共 40 条
  • [1] [Anonymous], 2003, Nippon Steel Technical Report
  • [2] EFFECT OF ALLOY GRAIN-SIZE AND SILICON CONTENT ON THE OXIDATION OF AUSTENITIC FE-CR-NI-MN-SI ALLOYS IN PURE O2
    BASU, SN
    YUREK, GJ
    [J]. OXIDATION OF METALS, 1991, 36 (3-4): : 281 - 315
  • [3] A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C
    Behnamian, Yashar
    Mostafaei, Amir
    Kohandehghan, Alireza
    Amirkhiz, Babak Shalchi
    Serate, Dominic
    Sun, Yifei
    Liu, Subiao
    Aghaie, Ermia
    Zeng, Yimin
    Chmielus, Markus
    Zheng, Wenyue
    Guzonas, David
    Chen, Weixing
    Luo, Jing Li
    [J]. CORROSION SCIENCE, 2016, 106 : 188 - 207
  • [4] INFLUENCE OF SURFACE ION-IMPLANTATION UPON THE OXIDATION BEHAVIOR OF A 20-PERCENT CR-25-PERCENT NI, NIOBIUM STABILIZED AUSTENITIC STAINLESS-STEEL, IN CARBON-DIOXIDE, AT 825-DEGREES-C
    BENNETT, MJ
    DEARNALEY, G
    HOULTON, MR
    HAWES, RWM
    GOODE, PD
    WILKINS, MA
    [J]. CORROSION SCIENCE, 1980, 20 (01) : 73 - &
  • [5] Long-Term Oxidation of Candidate Cast Iron and Stainless Steel Exhaust System Alloys from 650 to 800 A°C in Air with Water Vapor
    Brady, M. P.
    Muralidharan, G.
    Leonard, D. N.
    Haynes, J. A.
    Weldon, R. G.
    England, R. D.
    [J]. OXIDATION OF METALS, 2014, 82 (5-6): : 359 - 381
  • [6] Thermal and microstructural characterization of a novel ductile cast iron modified by aluminum addition
    Celik, Gulsah Aktas
    Tzini, Maria-Ioanna T.
    Polat, Seyda
    Atapek, S. Hakan
    Haidemenopoulos, Gregory N.
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2020, 27 (02) : 190 - 199
  • [7] Silicon and chromium depletion during the long-term oxidation of thin-sectioned austenitic steel
    Evans, HE
    Donaldson, AT
    [J]. OXIDATION OF METALS, 1998, 50 (5-6): : 457 - 475
  • [8] MODELING OXIDE SPALLATION
    EVANS, HE
    [J]. MATERIALS AT HIGH TEMPERATURES, 1994, 12 (2-3) : 219 - 227
  • [9] ROLE OF SILICON IN DETERMINING OXIDATION RESISTANCE OF AN AUSTENITIC STEEL
    FRANCIS, JM
    JUTSON, JA
    [J]. MATERIALS SCIENCE AND ENGINEERING, 1969, 4 (2-3): : 84 - &
  • [10] The effects of small additions of yttrium on the high-temperature oxidation resistance of a Si-containing austenitic stainless steel
    Fujikawa, H
    Morimoto, T
    Nishiyama, Y
    Newcomb, SB
    [J]. OXIDATION OF METALS, 2003, 59 (1-2): : 23 - 40