Hot deformation behavior and rate-controlling mechanism in dilute Al-Fe-Si alloys with minor additions of Mn and Cu

被引:31
作者
Shakiba, M. [1 ]
Parson, N. [2 ]
Chen, X. -G. [1 ]
机构
[1] Univ Quebec Chicoutimi, Dept Appl Sci, Saguenay, PQ G7H 2B1, Canada
[2] Arvida Res & Dev Ctr, Saguenay, PQ G7S 4K8, Canada
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2015年 / 636卷
基金
加拿大自然科学与工程研究理事会;
关键词
1xxx Aluminum alloys; Hot compressive deformation; Flow stress; Activation energy for hot deformation; Solid solution strengthening; CONSTITUTIVE ANALYSIS; SILICON CONTENT; ALUMINUM; EVOLUTION; CREEP; MICROSTRUCTURE; HOMOGENIZATION; SUBGRAIN; WORKING; GRAIN;
D O I
10.1016/j.msea.2015.04.029
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hot deformation behavior of dilute Al-Fe-Si alloys containing various amounts of Mn (0.1-0.2 wt%) and Cu (0.05-0.31 wt%) was investigated by hot compression tests conducted over a range of deformation temperatures (400-550 degrees C) and strain rates (0.01-10 s(-1)). Both Mn and Cu in a solid solution have a significant influence on the hot workability of dilute Al-Fe-Si alloys. On a wt% basis, Mn exhibits a stronger strengthening effect compared with Cu. The activation energies for hot deformation were calculated from the experimental flow stress data obtained using a hyperbolic sine constitutive equation for all of the alloys.investigated. The activation energy increased from 161 kJ/mol for the low-Fe base alloy to 181 kJ/mol for the alloy containing 0.2 wt% Mn, while the addition of Cu up to 031 wt% only slightly increased the activation energy to 166 kJ/mol. The solute diffusion acted as the deformation rate-controlling mechanism in these dilute alloys. Mn containing alloys have a higher flow stress and higher activation energy due to the considerably lower diffusion rate of Mn in aluminum compared with Cu containing alloys. Dynamic recovery was the sole softening mechanism associated with the hot deformation of all of the alloys was investigated. The addition of Mn and Cu retarded the dynamic recovery and decreased the subgrain size and mean misorientation angle of the grain boundaries. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:572 / 581
页数:10
相关论文
共 40 条
  • [11] Review - Grain and subgrain characterisation by electron backscatter diffraction
    Humphreys, FJ
    [J]. JOURNAL OF MATERIALS SCIENCE, 2001, 36 (16) : 3833 - 3854
  • [12] Solidification Studies of 3003 Aluminium Alloys with Cu and Zr Additions
    Jaradeh, Majed M. R.
    Carlberg, Torbjorn
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (07) : 615 - 627
  • [13] JONAS JJ, 1968, T JPN I MET, VS 9, P257
  • [14] Kaufman J. G., 2000, Introduction to Aluminium Alloys and Tempers
  • [15] Solute drag effects during the dynamic recrystallization of nickel
    Le Gall, R
    Jonas, JJ
    [J]. ACTA MATERIALIA, 1999, 47 (17) : 4365 - 4374
  • [16] Li Y.J., 2010, P 12 INT C AL ALL JA
  • [17] Constitutive descriptions for hot compressed 2124-T851 aluminum alloy over a wide range of temperature and strain rate
    Lin, Y. C.
    Xia, Yu-Chi
    Chen, Xiao-Min
    Chen, Ming-Song
    [J]. COMPUTATIONAL MATERIALS SCIENCE, 2010, 50 (01) : 227 - 233
  • [18] Mcqueen H.J., Aluminum alloys: Their Physical and Mechanical Properties - Proceedings ICAA3, P179
  • [19] Dynamic recovery:: sufficient mechanism in the hot deformation of Al (<99.99)
    McQueen, HJ
    Blum, W
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 290 (1-2): : 95 - 107
  • [20] McQueen HJ, 2011, MANUF ENG MATER PROC, V75, P1