Hot deformation behavior and rate-controlling mechanism in dilute Al-Fe-Si alloys with minor additions of Mn and Cu

被引:31
作者
Shakiba, M. [1 ]
Parson, N. [2 ]
Chen, X. -G. [1 ]
机构
[1] Univ Quebec Chicoutimi, Dept Appl Sci, Saguenay, PQ G7H 2B1, Canada
[2] Arvida Res & Dev Ctr, Saguenay, PQ G7S 4K8, Canada
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2015年 / 636卷
基金
加拿大自然科学与工程研究理事会;
关键词
1xxx Aluminum alloys; Hot compressive deformation; Flow stress; Activation energy for hot deformation; Solid solution strengthening; CONSTITUTIVE ANALYSIS; SILICON CONTENT; ALUMINUM; EVOLUTION; CREEP; MICROSTRUCTURE; HOMOGENIZATION; SUBGRAIN; WORKING; GRAIN;
D O I
10.1016/j.msea.2015.04.029
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The hot deformation behavior of dilute Al-Fe-Si alloys containing various amounts of Mn (0.1-0.2 wt%) and Cu (0.05-0.31 wt%) was investigated by hot compression tests conducted over a range of deformation temperatures (400-550 degrees C) and strain rates (0.01-10 s(-1)). Both Mn and Cu in a solid solution have a significant influence on the hot workability of dilute Al-Fe-Si alloys. On a wt% basis, Mn exhibits a stronger strengthening effect compared with Cu. The activation energies for hot deformation were calculated from the experimental flow stress data obtained using a hyperbolic sine constitutive equation for all of the alloys.investigated. The activation energy increased from 161 kJ/mol for the low-Fe base alloy to 181 kJ/mol for the alloy containing 0.2 wt% Mn, while the addition of Cu up to 031 wt% only slightly increased the activation energy to 166 kJ/mol. The solute diffusion acted as the deformation rate-controlling mechanism in these dilute alloys. Mn containing alloys have a higher flow stress and higher activation energy due to the considerably lower diffusion rate of Mn in aluminum compared with Cu containing alloys. Dynamic recovery was the sole softening mechanism associated with the hot deformation of all of the alloys was investigated. The addition of Mn and Cu retarded the dynamic recovery and decreased the subgrain size and mean misorientation angle of the grain boundaries. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:572 / 581
页数:10
相关论文
共 40 条
  • [1] [Anonymous], 1993, Aluminum and Aluminum Alloys
  • [2] [Anonymous], 2004, Recrystallization and Related Annealing Phenomena
  • [3] Constitutive equations for elevated temperature flow behavior of commercial purity aluminum
    Ashtiani, H. R. Rezaei
    Parsa, M. H.
    Bisadi, H.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 545 : 61 - 67
  • [4] High temperature deformation behavior of Al-Cu-Mg alloys micro-alloyed with Sn
    Banerjee, Sanjib
    Robi, P. S.
    Srinivasan, A.
    Kumar, Lakavath Praveen
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (10-11): : 2498 - 2503
  • [5] Benedictus R., 1998, P 6 INT C AL ALL ICA, P1577
  • [6] AN INTERNAL VARIABLE CONSTITUTIVE MODEL FOR HOT-WORKING OF METALS
    BROWN, SB
    KIM, KH
    ANAND, L
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 1989, 5 (02) : 95 - 130
  • [7] Microstructure evolution during homogenization of Al-Mn-Fe-Si alloys: Modeling and experimental results
    Du, Q.
    Poole, W. J.
    Wells, M. A.
    Parson, N. C.
    [J]. ACTA MATERIALIA, 2013, 61 (13) : 4961 - 4973
  • [8] Fleischer R., 1963, RELATION STRUCTURE M
  • [9] Substructure evolution during different hot deformation processes of commercial non-heat treatable aluminium alloys
    Furu, T
    Orsund, R
    Nes, E
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 214 (1-2): : 122 - 132
  • [10] Haasen P., 1996, PHYS METALLURGY, V3, P2009