High-temperature oxidation of NiCrAlY/(ZrO2-Y2O3 and ZrO2-CeO2-Y2O3) composite coatings

被引:12
作者
Lee, DB [1 ]
Lee, C
机构
[1] Sungkyunkwan Univ, Ctr Adv Plasma Surface Technol, Suwon 440746, South Korea
[2] Hanyang Univ, Div Mat Sci & Engn, Seoul 133791, South Korea
关键词
air plasma spray; coating; NiCrAlY; zirconia; oxidation;
D O I
10.1016/j.surfcoat.2004.08.140
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Metal/ceramic coatings of Ni-22Cr-10Al-1Y/ZrO2-8Y(2)O(3) and Ni-22Cr-10Al-1Y/ZrO2-25CeO(2)-2.5Y(2)O(3), which were prepared by the air plasma spray method, were oxidized at 900, 1000, and 1100 degrees C in air. The major oxidation product was alpha-Al2O3, which was formed by the reaction of inwardly penetrating oxygen ions with Al at the metal/ceramic phase boundaries. The oxidation of Ni and, moreover, Cr also occurred to a certain extent. (c) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:239 / 242
页数:4
相关论文
共 50 条
[41]   ZrO2 and Y2O3-stablized ZrO2 coatings deposited using an arc ion plating technique [J].
Wang, Qi Min ;
Gong, Jun ;
Sun, Chao ;
Lee, Hyung Woo ;
Kim, Kwang Ho .
JOURNAL OF CERAMIC PROCESSING RESEARCH, 2011, 12 (03) :259-264
[42]   Synthesis and microstructure of Y2O3-doped ZrO2-CeO2 composite nanoparticles by hydrothermal process [J].
Lee, Woo Seok ;
Kim, Sun Woog ;
Koo, Bon Heon ;
Bae, Dong Sik .
COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2008, 313 :100-104
[43]   Thermal expansion coefficient and residual stress of porous Ni/ZrO2-Y2O3 cermet [J].
Kawashima, T ;
Hishinuma, M .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1998, 106 (07) :682-687
[44]   Effect of lauric acid on the grain growth of CeO2-ZrO2-Y2O3-La2O3 in different periods [J].
Li, Mengchen ;
Deng, Jie ;
Yin, Xinyi ;
Wang, Wei ;
Zhao, Yi ;
Xu, Haidi ;
Wang, Jianli ;
Chen, Yaoqiang .
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 894
[45]   High-temperature oxidation resistance of (Al2O3-Y2O3)/(Y2O3-stabilized ZrO2) laminated coating on 8Nb-TiAl alloy prepared by a novel spray pyrolysis [J].
Yao, Junqi ;
He, Yedong ;
Wang, Deren ;
Lin, Junpin .
CORROSION SCIENCE, 2014, 80 :19-27
[46]   High-temperature internal friction and diffusion in Y2O3- and CaO-Stabilised ZrO2 [J].
Kilo, M ;
Weller, M ;
Borchardt, G .
DEFECTS AND DIFFUSION IN CERAMICS: AN ANNUAL RETROSPECTIVE IV, 2002, 206-2 :159-162
[47]   PHASE-TRANSFORMATION OF ZRO2-8-PERCENT-Y2O3 DURING ANNEALING AT HIGH-TEMPERATURE [J].
PAN, M ;
QIU, FX ;
JIA, SC ;
SHAO, GQ ;
LUO, ZP .
JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 1995, 10 (01) :23-29
[48]   Assessment of thermodynamic parameters in the system ZrO2-Y2O3-Al2O3 [J].
Fabrichnaya, O ;
Aldinger, F .
ZEITSCHRIFT FUR METALLKUNDE, 2004, 95 (01) :27-39
[49]   Liquidus Surface of the ZrO2-Y2O3-Eu2O3 Phase Diagram [J].
Andrievskaya, E. R. ;
Kovylyaev, V. V. ;
Lopato, L. M. ;
Shevchenko, A. V. ;
Frolov, A. A. .
POWDER METALLURGY AND METAL CERAMICS, 2014, 53 (5-6) :312-322
[50]   Phase stability and transport characteristics of (ZrO2)1-x(Sc2O3)x(CeO2)y and (ZrO2)1-x-y-z(Sc2O3)x(CeO2)y(Y2O3)z solid solution crystals [J].
Agarkov, D. A. ;
Borik, M. A. ;
Bublik, V. T. ;
Chislov, A. S. ;
Kulebyakin, A., V ;
Kuritsyna, I. E. ;
Kolotygin, V. A. ;
Lomonova, E. E. ;
Milovich, F. O. ;
Myzina, V. A. ;
Osiko, V. V. ;
Tabachkova, N. Yu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 791 :445-451