共 66 条
Effect of support on hydrogen production from chemical looping steam reforming of ethanol over Ni-based oxygen carriers
被引:58
作者:
Wang, Kaiqiang
[1
]
Dou, Binlin
[1
,2
]
Jiang, Bo
[1
]
Zhang, Qian
[1
]
Li, Min
[1
]
Chen, Haisheng
[3
]
Xu, Yujie
[3
]
机构:
[1] Dalian Univ Technol, Sch Energy & Power Engn, Key Lab Ocean Energy Utilizat & Energy Conservat, Minist Educ, Dalian 116023, Peoples R China
[2] Univ Shanghai Sci & Technol, Sch Energy & Power Engn, Shanghai 200093, Peoples R China
[3] Chinese Acad Sci, Inst Engn Thermophys, Beijing 100190, Peoples R China
关键词:
Chemical looping steam reforming;
Oxygen carriers;
Support structure;
Fixed-bed reactor;
MESOPOROUS SBA-15;
CARBON FORMATION;
CATALYSTS;
METHANE;
GLYCEROL;
SILICA;
BIOMASS;
NANOPARTICLES;
SIZE;
DRY;
D O I:
10.1016/j.ijhydene.2016.07.261
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
The Ni-based oxygen carriers (OCs) with different supports including alloy Ni/Al2O3, lamellar Ni/MMT, mesoporous Ni/Al-MCM-41 and mesoporous Ni/SBA-15 were synthesized. The effect of support on hydrogen production from chemical looping steam reforming (CLSR) of ethanol was investigated in a fixed-bed reactor. The oxygen carriers were characterized by some techniques, including N-2 adsorption-desorption, XRD, TEM, ICP-OES, H-2 pulse chemisorption, H-2-TPR, and TG-DTG. It was observed that Ni/SBA-15 exhibited most efficient confinement effect followed by Ni/Al-MCM-41, Ni/MMT and Ni/Al2O3 via: 1) small nickel particle size and high dispersion as well as strengthened metal-support interaction; 2) sintering resistance due to spatial restriction of support; 3) anti-coke capability derived from small nickel particles and ordered diffusion routes for reactants and products. In addition, the silica supported OCs were conductive to promote water gas shift (WGS) reaction but the supports containing Al atoms were prone to coke deposition due to the formation of acid sites. The 'dead time' and oxygen transfer capacity reflected that the redox performance of oxygen carriers was listed in the following order: Ni/SBA-15, Ni/Al-MCM-41, Ni/MMT and Ni/Al2O3. Ni/Al-MCM-41 exhibited excellent activity in initial cycle of CLSR but the collapse of the Ni/Al-MCM-41 structure for its weak thermo stability leaded to the deactivation and sintering of active phase. The Ni/SBA-15 and lamellar Ni/MMT OCs exhibited superior activity and stability but the performance of Ni/Al2O3 OCs was mediocre. (C) 2016 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.