Hot corrosion behavior and near-surface microstructure of a "low-temperature high-activity Cr-aluminide" coating on inconel 738LC exposed to Na2SO4, Na2SO4 + V2O5 and Na2SO4 + V2O5 + NaCl at 900 °C

被引:36
|
作者
Doolabi, M. Salehi [1 ]
Ghasemi, B. [1 ]
Sadrnezhaad, S. K. [2 ]
Habibollahzadeh, A. [1 ]
Jafarzadeh, K. [3 ]
机构
[1] Semnan Univ, Fac Mat Sci & Engn, POB 35131-19111, Semnan, Iran
[2] Sharif Univ Technol, Dept Mat Sci & Engn, Azadi Ave,POB 11365-9466, Tehran, Iran
[3] Maleke Ashtar Univ Technol, Mat Dept, Tehran, Iran
关键词
Metal coating; Superalloys; Molten salts; Hot corrosion; CYCLIC OXIDATION BEHAVIOR; NI-BASED SUPERALLOY; BASE SUPERALLOY; NICKEL; ALLOYS; ENVIRONMENT;
D O I
10.1016/j.corsci.2017.09.004
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hot corrosion is a serious problem in gas turbines due to poor quality fuels which contain Na, V, S and Cl. To resolve the problem, Cr-aluminide was coated on IN-738LC superalloy with a two steps pack cementation process. Oxidation behavior and near-surface microstructure of the coating showed consecutive increase in destruction by exposition to Na2SO4, 75Na(2)SO(4) + 25 V2O5 and 70Na(2)SO(4) + 25 V2O5 + 5NaCl (wt.%). Kinetic studies indicated parabolic corrosion rate in salt-less samples due to diffusion. Similar expression for salt-covered samples was assessed for oxide dissolution. Plate-like, broken-plate-like and cauliflower-like morphologies attributed to the corrosion products were observed after exposition to above three salts, respectively.
引用
收藏
页码:42 / 53
页数:12
相关论文
共 50 条
  • [41] Hot corrosion behaviour of plasma-sprayed functionally graded thermal barrier coatings in the presence of Na2SO4 + V2O5 molten salt
    Vakilifard, Hamide
    Ghasemi, Reza
    Rahimipour, Mohammadreza
    SURFACE & COATINGS TECHNOLOGY, 2017, 326 : 238 - 246
  • [42] Effect of Ca(OH)2, NaCl, and Na2SO4 on the corrosion and electrochemical behavior of rebar
    Jin Zuquan
    Zhao Xia
    Zhao Tiejun
    Hou Baorong
    Liu Ying
    CHINESE JOURNAL OF OCEANOLOGY AND LIMNOLOGY, 2017, 35 (03) : 681 - 692
  • [43] Hot Corrosion Resistance of Hot-Dip-Aluminized AISI 321 Stainless Steel in a Salt Mixture of 60%V2O5 + 40% Na2SO4 at 700 °C
    Prashant Huilgol
    K. Rajendra Udupa
    K. Udaya Bhat
    Transactions of the Indian Institute of Metals, 2019, 72 : 1613 - 1616
  • [44] Hot corrosion behavior of AlCuFeCr quasicrystalline coating on titanium alloy with the mixture of NaCl and Na2SO4 deposit
    Wang, Fengfeng
    Zhou, Chungen
    Gong, Shengkai
    Xu, Huibin
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 2313 - +
  • [45] Corrosion behavior of the NiCrAlY and NiSiAlY alloys with salt mixtures of NaCl/Na2SO4
    Zheng, Haiyang
    Cui, Tiancheng
    Zhu, Bing
    Yu, Xiaopeng
    Yu, Miao
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2024, 42 (02):
  • [46] Hot Corrosion Behavior of ZrB2-SiC-Graphite Composite in NaCl and Na2SO4 Molten Salts
    Liu, X.
    Wang, G.
    Liu, L.
    Wang, Z.
    Wu, Z.
    Liu, M.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2018, 9 (03): : 309 - 317
  • [47] EFFECTS OF SO3, SO2 AND O2 GASSES ON HOT CORROSION OF NI AND NI-CR ALLOYS IN MOLTEN NA2SO4
    HARA, M
    HISAICHI, T
    ITOH, K
    SHINATA, Y
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1991, 55 (11) : 1207 - 1215
  • [48] Na2SO4 Induced Hot Corrosion of Aluminized Low Carbon Steel at 700 °C
    Badaruddin, Mohammad
    ADVANCES IN APPLIED MECHANICS AND MATERIALS, 2014, 493 : 761 - 766
  • [49] Hot Corrosion Resistance of CeO2-Doped Cr3C2–NiCr Coatings on Austenite Steel Against Molten Salt (Na2SO4–60%V2O5) Environment
    Singh H.
    Chatha S.S.
    Sidhu B.S.
    Journal of Bio- and Tribo-Corrosion, 2023, 9 (01)
  • [50] Cyclic oxidation and hot corrosion performance of direct metal laser sintered and wrought alloy 718 at 800°C in air and molten salts containing Na2SO4, V2O5 and NaCl
    Muthu, S. M.
    Veeman, Dhinakaran
    Paul, Shiladithya
    Kumar, M. Prem
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2023, 58 (07) : 631 - 644