摘要
The ability to monitor corrosion on a nanometer scale is a powerful tool for a fundamental understanding of surface chemical processes. Nanoscale chemical images of individual bare and alumina-coated zinc oxide nanowires (NWs) were recorded using tip-enhanced second harmonic generation (SHG) spectroscopy before and after exposure to carbon dioxide and water vapor. Images were collected for the same bare nanowire after each successive two-day exposure period. Corrosion of the bare ZnO NW to zinc carbonate was evident from far-field and near-field SHG images and simultaneously recorded atomic force microscopy (AFM) data. The expected zinc carbonate corrosion product is SHG inactive. The AFM profile of the NW showed vertical and lateral expansion in different regions of the nanowire. The lower resolution far-field SHG signal decreased gradually and uniformly. The near-field SHG signal provided a profile of the evolving NW with a spatial resolution approaching 100 nm. In contrast, exposed alumina-coated ZnO NWs showed reduced, but still observable, degradation. The 3 nm thick alumina protective layer may have been insufficient to fully protect the NW, or the coating may have been incomplete. Thicker coatings preclude the tip-enhanced method. Further nanometer-scale imaging should lead to the discovery of protective layers to prevent or delay ZnO degradation.
引用
收藏
页码:10405 / 10414
页数:10
相关论文
共 35 条
[1]   Field-effect transistors based on single semiconducting oxide nanobelts [J].
Arnold, MS ;
Avouris, P ;
Pan, ZW ;
Wang, ZL .
JOURNAL OF PHYSICAL CHEMISTRY B, 2003, 107 (03) :659-663
[2]   Broadband ZnO single-nanowire light-emitting diode [J].
Bao, Jiming ;
Zimmler, Mariano A. ;
Capasso, Federico ;
Wang, Xiaowei ;
Ren, Z. F. .
NANO LETTERS, 2006, 6 (08) :1719-1722
[3]   Formation of Branched ZnO Nanowires from Solvothermal Method and Dye-Sensitized Solar Cells Applications [J].
Cheng, Hsin-Ming ;
Chiu, Wei-Hao ;
Lee, Chia-Hua ;
Tsai, Song-Yeu ;
Hsieh, Wen-Feng .
JOURNAL OF PHYSICAL CHEMISTRY C, 2008, 112 (42) :16359-16364
[4]   Chemical imaging of corrosion: Sum frequency generation imaging microscopy of cyanide on gold at the solid-liquid interface [J].
Cimatu, Katherine ;
Baldelli, Steven .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2008, 130 (25) :8030-8037
[5]   Novel nanostructures of functional oxides synthesized by thermal evaporation [J].
Dai, ZR ;
Pan, ZW ;
Wang, ZL .
ADVANCED FUNCTIONAL MATERIALS, 2003, 13 (01) :9-24
[6]   The role of carbon dioxide in the atmospheric corrosion of zinc - A laboratory study [J].
Falk, T ;
Svensson, JE ;
Johansson, LG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (01) :39-44
[7]   The influence of CO2 and NaCl on the atmospheric corrosion of zinc -: A laboratory study [J].
Falk, T ;
Svensson, JE ;
Johansson, LG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (09) :2993-2999
[8]   Electrostatic surface charge at aqueous/α-Al2O3 single-crystal interfaces as probed by optical second-harmonic generation [J].
Fitts, JP ;
Shang, XM ;
Flynn, GW ;
Heinz, TF ;
Eisenthal, KB .
JOURNAL OF PHYSICAL CHEMISTRY B, 2005, 109 (16) :7981-7986
[9]   Frequency doubling and autocorrelation studies of 20-fs pulses using polycrystalline zinc oxide thin films [J].
Griebner, U ;
Kaindl, RA ;
Elsaesser, T ;
Seeber, W .
APPLIED PHYSICS B-LASERS AND OPTICS, 1998, 67 (06) :757-760
[10]   Active site nature of pyrogenic alumina/silica and water bound to surfaces [J].
Gunko, VM ;
Turov, VV ;
Zarko, VI ;
Voronin, EF ;
Tischenko, VA ;
Dudnik, VV ;
Pakhlov, EM ;
Chuiko, AA .
LANGMUIR, 1997, 13 (06) :1529-1544