INTERNAL REVERSIBLE HYDROGEN EMBRITTLEMENT AND HYDROGEN GAS EMBRITTLEMENT OF AUSTENITIC STAINLESS STEELS BASED ON TYPE 316

被引:0
|
作者
Imade, Masaaki [1 ]
Zhang, Lin [1 ]
Wen, Mao [1 ]
Iijima, Takashi [1 ]
Fukuyama, Seiji [1 ]
Yokogawa, Kiyoshi [1 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Tsukuba, Ibaraki 3058565, Japan
来源
PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, VOL 6, PTS A AND B | 2010年
关键词
STRESS-CORROSION CRACKING; HIGH-PRESSURE HYDROGEN; LOW-TEMPERATURES; ENVIRONMENT EMBRITTLEMENT; BEHAVIOR; DEFORMATION; MARTENSITE; GROWTH;
D O I
暂无
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The internal reversible hydrogen embrittlement (IRHE) of austenitic Fe(10-20)Ni17Cr2Mo alloys based on type 316 stainless steel was investigated by tests using the slow strain rate technique from 80 to 300 K in comparison with its effect on the hydrogen gas embrittlement (HGE) of the alloys in hydrogen at a pressure of 1 MPa. The IRHE and HOE of the alloys in 70 MPa hydrogen at room temperature was also investigated. At low temperatures, IRHE occurred below a Ni content of 15% (Ni equivalent (Ni-eq):29%), increased with decreasing temperature, reached a maximum at 200 K, and decreased with further decreasing temperature, similarly to the temperature dependence of HOE. At room temperature, IRHE and HOE were observed below a Ni content of 14% (Ni-eq:28%) and decreased with increasing Ni content (Ni-eq). The dependence of HGE on hydrogen pressure increased with decreasing Ni content (Ni-eq). Hydrogen-induced fracture closely related to the strain-induced alpha' martensite structure and twin boundaries mainly occurred for both IRHE and HGE. Dimple ruptures caused by hydrogen segregation occurred in only IRHE at 150 K. The content of strain-induced alpha' martensite increased with decreasing temperature and Ni content (Ni-eq). Thus, the susceptibility to IRHE and HOE depended on Ni content (Ni-eq). It was concluded that both IRHE and HOE were controlled by the amount of strain-induced alpha' martensite above 200 K, whereas they were controlled by the hydrogen transport below 200 K.
引用
收藏
页码:205 / 213
页数:9
相关论文
共 50 条
  • [21] HYDROGEN EMBRITTLEMENT OF ULTRAFINE-GRAINED AUSTENITIC STAINLESS STEELS
    Astafurova, E. G.
    Astafurov, S., V
    Maier, G. G.
    Moskvina, V. A.
    Melnikov, E., V
    Fortuna, A. S.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2018, 54 (01) : 25 - 45
  • [22] STUDY OF HYDROGEN EMBRITTLEMENT OF UNSTABLE AUSTENITIC STAINLESS-STEELS
    BRICOUT, JP
    MISSIAEN, R
    AZOU, PF
    FIDELLE, JP
    BAVAY, JC
    MEMOIRES ET ETUDES SCIENTIFIQUES DE LA REVUE DE METALLURGIE, 1986, 83 (02): : 105 - 118
  • [23] Nitrogen effect on hydrogen diffusivity and hydrogen embrittlement behavior in austenitic stainless steels
    Kim, Kyung-Shik
    Kang, Jee-Hyun
    Kim, Sung-Joon
    SCRIPTA MATERIALIA, 2020, 184 (184) : 70 - 73
  • [24] Mechanism of hydrogen embrittlement of austenitic steels
    Shivanyuk, V.
    Gavriljuk, V.
    Foct, J.
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 4249 - +
  • [25] HYDROGEN EMBRITTLEMENT OF AUSTENITIC STAINLESS STEEL
    WHITEMAN, MB
    TROIANO, AR
    CORROSION, 1965, 21 (02) : 53 - &
  • [26] Hydrogen embrittlement of additively manufactured austenitic stainless steel 316 L
    Bertsch, K. M.
    Nagao, A.
    Rankouhi, B.
    Kuehl, B.
    Thoma, D. J.
    CORROSION SCIENCE, 2021, 192
  • [27] HYDROGEN EMBRITTLEMENT OF SUS 316 AUSTENITIC STAINLESS STEEL WELDMENTS.
    Matsuda, Fukuhisa
    Ushio, Masao
    Nakagawa, Hiroji
    Nakata, Kazuhiro
    Transactions of JWRI (Japanese Welding Research Institute), 1985, 14 (01): : 63 - 67
  • [28] Abnormal effect of nitrogen on hydrogen gas embrittlement of austenitic stainless steels at low temperatures
    Zhou, Chengshuang
    Hong, Yuanjian
    Zhang, Lin
    An, Bai
    Zheng, Jinyang
    Chen, Xingyang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (31) : 13777 - 13785
  • [29] Influence of low temperature prestrain on hydrogen gas embrittlement of metastable austenitic stainless steels
    Zhang, Lin
    Li, Zhiyuan
    Zheng, Jinyang
    Zhao, Yongzhi
    Xu, Ping
    Liu, Xianxin
    Zhou, Chilou
    Li, Xiao
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2013, 38 (25) : 11181 - 11187
  • [30] Stress Induce Martensitic Transformations in Hydrogen Embrittlement of Austenitic Stainless Steels
    Rozenak, Paul
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (01): : 162 - 178