Development of new bio-based polyol ester from palm oil for potential polymeric drug carrier

被引:7
作者
Tajau, Rida [1 ]
Rohani, Rosiah [1 ]
Isahak, Wan Nor Roslam Wan [1 ]
Salleh, Mek Zah [2 ]
Ghazali, Zulkafli [2 ]
机构
[1] Natl Univ Malaysia, Fac Engn & Built Environm, Dept Chem & Proc Engn, Selangor, Malaysia
[2] Agensi Nuklear Malaysia, Div Radiat Proc Technol, Kajang, Selangor, Malaysia
关键词
biopolymers; drug delivery systems; palm oil; polyesters; polyol; THERMAL-STABILITY; VEGETABLE-OILS; RELEASE; POLYURETHANES; NANOMATERIALS; HYDROGELS; CHITIN; ACID;
D O I
10.1002/adv.22139
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The polyol ester derived from palm oil polymers is a promising material for utilizing it as a polymeric drug carrier due to its natural and biocompatible properties. In this study, the palm oil-based diol is used as a precursor for developing the polyol ester via the transesterification-alcoholysis reaction of the diol with triethanolamine and lithium hydroxide. Preliminary results showed that the polyol ester displayed high hydroxyl value at 182.51 mg KOH/g with the yield reached more than 90%. Meanwhile, its molecular weight was around 5,000 Dalton. The appearances of ester (C-O) between 1,300 and 1,000 cm(-1) in the Fourier transform infrared (FTIR) spectra have confirmed the hydrolyzable ester structure of the polyol ester. Consequently, the delta(H)- and delta(C)-NMR spectra also confirmed the presences of the ester proton (i.e., -COO-CH2-) and the ester carbons (i.e., -CH2CH2CO(O)C-, -CH2COO-, -CH2C(O)OC-). Thermogravimetric analysis of the polyol ester displayed three stages of maximum decomposition temperature (T-max): 203.56 degrees C, 362.79 degrees C, and 481.91 degrees C. Differential scanning chromatography (DSC) analysis indicated that the glass transition temperature (T-g) of the polyol ester was found between -3.27 and 7.5 degrees C. As a result, the analyses affirmed that this polyol ester is a hydrolytically degradable polymer due to the presence of its hydrolyzable ester bonds. Its low molecular weight and low-melting biodegradable properties could show a faster degradation compared to the higher molecular weight synthetic polymers. Thus, the characteristic of the developed polyol ester demonstrates promising physicochemical and good thermal properties, which makes it a potential candidate for a polymeric drug delivery system.
引用
收藏
页码:3552 / 3560
页数:9
相关论文
共 80 条
  • [11] Baharu M.N., 2015, GREEN CHEM LETT REV, V8, P31, DOI DOI 10.1080/17518253.2014.991810
  • [12] Lexicon of lipid nutrition
    Beare-Rogers, J
    Dieffenbacher, A
    Holm, JV
    [J]. PURE AND APPLIED CHEMISTRY, 2001, 73 (04) : 685 - 744
  • [13] Choo YuenMay Choo YuenMay, 2004, Journal of Oil Palm Research, V16, P1
  • [14] Cui Y., 2015, ADV POLYM TECHNOL, V36, P331
  • [15] Synthesis and characterization of interpenetrating polymer networks from transesterified castor oil based polyurethane and polystyrene
    Dave, Vivek J.
    Patel, Hasmukh S.
    [J]. JOURNAL OF SAUDI CHEMICAL SOCIETY, 2017, 21 (01) : 18 - 24
  • [16] From Vegetable Oils to Polyurethanes: Synthetic Routes to Polyols and Main Industrial Products
    Desroches, Myriam
    Escouvois, Maxime
    Auvergne, Remi
    Caillol, Sylvain
    Boutevin, Bernard
    [J]. POLYMER REVIEWS, 2012, 52 (01) : 38 - 79
  • [17] Polylactide-co-glycolide nanoparticles for controlled delivery of anticancer agents
    Dinarvand, R.
    Sepehri, N.
    Manoochehri, S.
    Rouhani, H.
    Atyabi, F.
    [J]. INTERNATIONAL JOURNAL OF NANOMEDICINE, 2011, 6 : 877 - 895
  • [18] Duncan R., 2007, POLYM DRUGS DRUG PRO, P47
  • [19] An Investigation into the Swelling Properties, Dimensional Changes, and Gel Layer Evolution in Chitosan Tablets Undergoing Hydration
    Efentakis, Manuel
    Stamoylis, Konstantinos
    [J]. ADVANCES IN POLYMER TECHNOLOGY, 2009, 28 (01) : 32 - 39
  • [20] Ekkaphan P., 2016, INT J POLYM SCI, V2016, P11