Long term anneal study and composition variation for reducing residual Bi2Sr2CaCu2Ox (2212) in (Bi, Pb)2Sr2Ca2Cu3Ox (2223) wires

被引:1
作者
Jiang, J
Cai, XY
Yuan, Y
Polyanskii, AA
Hellstrom, EE
Larbalestier, DC
Maroni, VA
Holesinger, TG
Huang, Y
机构
[1] Univ Wisconsin, Ctr Appl Superconduct, Madison, WI 53706 USA
[2] Argonne Natl Lab, Argonne, IL 60439 USA
[3] Los Alamos Natl Lab, Los Alamos, NM 87545 USA
[4] Amer Superconductor Corp, Westborough, MA 01581 USA
关键词
composition; critical current density; superconductor; 2212; 2223;
D O I
10.1109/TASC.2005.847516
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Recent experiments showed that Bi2Sr2CaCu2Ox (2212) intergrowths are a major current limiting mechanism in (Bi,Pb)(2)Sr2Ca2Cu3Ox (2223) wires and that reduced Bi2Sr2CaCu2Ox (2212) correlates to enhanced critical current density J(C). We performed a final 500 h post heat treatment on commercial 2223 wire to study whether an extended heat treatment would reduce the 2212 phase content. This heat treatment did not change the 2212 content or J(C), indicating the fully processed 2223 wires were already very close to their terminal phase state. In an attempt to reduce the 2212 content, we slightly modified the standard composition in the Ca and Cu rich directions, investigating: Ca-rich; Cu-rich; Ca plus Cu-rich; Sr-poor; and Ca substitution for Sr. Although the 2212 content was not reduced by modifying the composition, the result further confirmed the correlation between J(C) and residual 2212 in 2223 wires.
引用
收藏
页码:2526 / 2529
页数:4
相关论文
共 15 条
[1]   Transmission electron microscopy investigation of Bi-2223/Ag tapes [J].
Andersen, LG ;
Bals, S ;
Van Tendeloo, G ;
Poulsen, HF ;
Liu, YL .
PHYSICA C, 2001, 353 (3-4) :251-257
[2]   Investigation of a multi-set-point first heat treatment methodology for the silver-sheathed (Bi, Pb)2Sr2Ca2Cu3Ox composite conductor [J].
Baurceanu, RM ;
Maroni, VA ;
Merchant, NM ;
Fischer, AK ;
McNallan, MJ ;
Parrella, RD .
SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2002, 15 (07) :1167-1175
[4]   Observation of the Bi,Pb(2223) reaction mechanism and alternative ways of producing tapes with new filament configurations [J].
Flükiger, R ;
Huang, Y ;
Marti, F ;
Dhallé, M ;
Giannini, E ;
Passerini, R ;
Bellingeri, E ;
Grasso, G ;
Grivel, JC .
IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1999, 9 (02) :2430-2435
[5]   Structural and compositional defects in high-Jc, Bi-2223 tapes [J].
Holesinger, TG ;
Bingert, JF ;
Willis, JO ;
Li, Q ;
Parrella, RD ;
Teplitsky, MD ;
Rupich, MW ;
Riley, GN .
IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1999, 9 (02) :2440-2445
[6]  
HUANG YB, 2002, ADV CRYOGEN ENG, V48, P717
[7]   Critical current limiting factors in post annealed (Bi, Pb)2Sr2Ca2Cu3Ox tapes [J].
Jiang, J ;
Cai, XY ;
Chandler, JG ;
Patnaik, S ;
Polyanskii, AA ;
Yuan, Y ;
Hellstrom, EE ;
Larbalestier, DC .
IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2003, 13 (02) :3018-3021
[8]   Evolution of core density of Ag-Clad Bi-2223 tapes during process [J].
Jiang, J ;
Cai, XY ;
Chandler, JG ;
Rikel, MO ;
Hellstrom, EE ;
Parrella, RD ;
Yu, DA ;
Li, Q ;
Rupich, MW ;
Riley, GN ;
Larbalestier, DC .
IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2001, 11 (01) :3561-3564
[9]   Through-process study of factors controlling the critical current density of Ag-sheathed (Bi,Pb)2Sr2Ca2Cu3Ox tapes [J].
Jiang, J ;
Cai, XY ;
Polyanskii, AA ;
Schwartzkopf, LA ;
Larbalestier, DC ;
Parrella, RD ;
Li, Q ;
Rupich, MW ;
Riley, GN .
SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2001, 14 (08) :548-556
[10]   Direct atomic scale imaging of grain boundaries and defects in Bi-2223/Ag high-Tc superconducting tapes [J].
Kishida, K ;
Browning, ND .
PHYSICA C, 2001, 351 (03) :281-294