Highly Water-Resistant La-Doped Co3O4 Catalyst for CO Oxidation

被引:188
作者
Bae, Junemin [1 ]
Shin, Dongjae [2 ]
Jeong, Hojin [1 ]
Kim, Beom-Sik [1 ]
Han, Jeong Woo [2 ]
Lee, Hyunjoo [1 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Chem & Biomol Engn, Daejeon 34141, South Korea
[2] Pohang Univ Sci & Technol, Dept Chem Engn, Pohang 37673, Gyeongbuk, South Korea
基金
新加坡国家研究基金会;
关键词
Co3O4; CO oxidation; La doping; water resistance; surface OH; LOW-TEMPERATURE OXIDATION; RARE-EARTH-OXIDES; CARBON-MONOXIDE; MESOPOROUS CO3O4; OXYGEN VACANCY; PERFORMANCE; HYDROPHOBICITY; ADSORPTION; NANOPARTICLES; ORIGIN;
D O I
10.1021/acscatal.9b02920
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Co3O4 is an attractive alternative to precious metal catalyst for CO oxidation due to its low cost and earth abundance, but its high catalytic activity is severely degraded in the presence of water. Here, we show that doping La into Co3O4 surfaces significantly enhances CO oxidation activity under moisture-rich condition. While bare Co3O4 is deactivated under moisture, the La-doped Co3O4 catalysts exhibit greatly improved activity and water resistance. The higher ratio of active Co3+ on the La-doped Co3O4 surface results in the enhanced activity. Especially, the La doping greatly reduces the formation of surface OH on the Co3O4 surface, which causes the poor water resistance. Density functional theory calculations reveal that the La doping suppresses the vacancy-assisted dissociative adsorption of H2O, resulting in less formation of surface OH and thereby mitigating water poisoning on the Co3O4 surface. This work can provide an insight into the surface restructuring for highly active and water-resistant Co3O4 catalysts.
引用
收藏
页码:10093 / 10100
页数:15
相关论文
共 56 条
[1]   Sub-ambient CO oxidation over mesoporous Co3O4: Effect of morphology on its reduction behavior and catalytic performance [J].
Alvarez, A. ;
Ivanova, S. ;
Centeno, M. A. ;
Odriozola, J. A. .
APPLIED CATALYSIS A-GENERAL, 2012, 431 :9-17
[2]   Nanoparticles as recyclable catalysts: The frontier between homogeneous and heterogeneous catalysis [J].
Astruc, D ;
Lu, F ;
Aranzaes, JR .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2005, 44 (48) :7852-7872
[3]  
Azimi G, 2013, NAT MATER, V12, P315, DOI [10.1038/NMAT3545, 10.1038/nmat3545]
[4]   Promotion of lanthanum-supported cobalt-based catalysts for the Fischer-Tropsch reaction [J].
Brabant, Cathy ;
Khodakov, Andrei ;
Griboval-Constant, Anne .
COMPTES RENDUS CHIMIE, 2017, 20 (01) :40-46
[5]   A DFT study on CO oxidation over Co3O4 [J].
Broqvist, P ;
Panas, I ;
Persson, H .
JOURNAL OF CATALYSIS, 2002, 210 (01) :198-206
[6]   Ultrathin, Polycrystalline, Two-Dimensional Co3O4 for Low-Temperature CO Oxidation [J].
Cai, Yafeng ;
Xu, Jia ;
Guo, Yun ;
Liu, Jingyue .
ACS CATALYSIS, 2019, 9 (03) :2558-2567
[7]   Understanding and Tuning the Intrinsic Hydrophobicity of Rare Earth Oxides: A DFT plus U Study [J].
Carchini, Giuliano ;
Garcia-Melchor, Max ;
Lodziana, Zbigniew ;
Lopez, Nuria .
ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (01) :152-160
[8]   Hydrophobic Polymer-Coated Metal Oxide Catalysts for Effective Low-Temperature Oxidation of CO under Moisture-Rich Conditions [J].
Chen, Chun-Hu ;
Njagi, Eric C. ;
Sun, Shih-Po ;
Genuino, Homer ;
Hu, Boxun ;
Suib, Steven L. .
CHEMISTRY OF MATERIALS, 2010, 22 (11) :3313-3315
[9]   INFLUENCE OF DRY OPERATING-CONDITIONS - OBSERVATION OF OSCILLATIONS AND LOW-TEMPERATURE CO OXIDATION OVER CO3O4 AND AU/CO3O4 CATALYSTS [J].
CUNNINGHAM, DAH ;
KOBAYASHI, T ;
KAMIJO, N ;
HARUTA, M .
CATALYSIS LETTERS, 1994, 25 (3-4) :257-264
[10]   Electron-energy-loss spectra and the structural stability of nickel oxide: An LSDA+U study [J].
Dudarev, SL ;
Botton, GA ;
Savrasov, SY ;
Humphreys, CJ ;
Sutton, AP .
PHYSICAL REVIEW B, 1998, 57 (03) :1505-1509