Effects of dopant materials on the characteristics of the nano-sized Co3O4 powders prepared by spray pyrolysis
被引:0
作者:
Ju, Seo Hee
论文数: 0引用数: 0
h-index: 0
机构:
Konkuk Univ, Dept Chem Engn, Seoul 143701, South KoreaKonkuk Univ, Dept Chem Engn, Seoul 143701, South Korea
Ju, Seo Hee
[1
]
Kang, Yun Chan
论文数: 0引用数: 0
h-index: 0
机构:
Konkuk Univ, Dept Chem Engn, Seoul 143701, South KoreaKonkuk Univ, Dept Chem Engn, Seoul 143701, South Korea
Kang, Yun Chan
[1
]
机构:
[1] Konkuk Univ, Dept Chem Engn, Seoul 143701, South Korea
来源:
JOURNAL OF CERAMIC PROCESSING RESEARCH
|
2010年
/
11卷
/
05期
关键词:
Spray pyrolysis;
Cobalt oxide;
Nano powders;
Gas phase reaction;
Black matrix;
Display material;
NANOPARTICLES;
OXIDATION;
PARTICLES;
ROUTE;
D O I:
暂无
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
Pure and M-doped Co3O4 (M = Cr, Fe, Mg, Zr) powders with a nanometre size and a narrow size distribution were prepared by spray pyrolysis from a spray solution with citric acid and ethylene glycol. The precursor powders with a hollow and thin walled structure were turned to nano-sized Co3O4 powders after post-treatment. The mean size of the pure Co3O4 powders post-treated at a temperature of 600 degrees C was 77 nm. On the other hand, the mean sizes of the doped Co3O4 powders with a doping concentration of 3 mol.% were changed from 24 to 63 nm. The Mg-doped Co3O4 powders had the minimum mean size. The mean sizes of the Mg-doped Co3O4 powders with doping concentrations of 1 and 5 mol.% were 60 and 61 nm. The mean sizes of the Mg-doped Co3O4 powders with a doping concentration of 3 mol.% post-treated at temperatures of 700 and 800 degrees C were 63 to 102 nm.