Organic solvent resistant poly(ether-ether-ketone) nanofiltration membranes

被引:129
作者
Burgal, Joao da Silva [1 ]
Peeva, Ludmila G. [1 ]
Kumbharkar, Santosh [1 ]
Livingston, Andrew [1 ]
机构
[1] Univ London Imperial Coll Sci Technol & Med, Dept Chem Engn & Chem Technol, London SW7 2AZ, England
关键词
Poly(ether ether ketone) (PEEK); Organic solvent nanofiltration (OSN); Degree of sulphonation (DS); Chemical resistance; POLY(ETHER ETHER KETONE); SIZE-EXCLUSION CHROMATOGRAPHY; MOLECULAR-MASS DETERMINATION; CHEMICAL MODIFICATION; PEEK SULFONATION; ROOM-TEMPERATURE; SURFACE;
D O I
10.1016/j.memsci.2014.12.035
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
In this work a poly(ether ether ketone) (PEEK) membrane is presented for its suitability for organic solvent nanofiltration (OSN) applications using polar aprotic solvents, such as DMF and THF, high temperatures, and basic/acidic conditions. Four grades of PEEK polymer were tested and it was verified that different grades produced membranes with different performances; the post-phase inversion drying process of membrane fabrication was shown to be crucial in obtaining separation performance in the nanofiltration range. The degree of sulphonation (DS) was also important and was controlled to be in the range of 3.7-6.7 wt%. The tightest membrane, produced from VESTAKEEP (R) 4000P and obtained after drying at 20 degrees C from water, presented a permeance of 0.22 L h(-1) m(-2) bar(-1) and molecular weight cutoff (MWCO) of 400 g mol(-1) in THF, and a permeance of 0.07 L h(-1) m(-2) bar(-1) and a MWCO of around 470 g mol(-1) in DMF. To the best of our knowledge this is the first report on a non-sulphonated and non-modified PEEK membrane capable of separations in the nanofiltration range and resistant to DMF and THE and to basic and acidic aqueous solutions. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:105 / 116
页数:12
相关论文
共 39 条
[1]  
Anneliese G., 1996, European patent, Patent No. [0737,506 (A1), 0737506]
[2]   THE SODIUM-SALTS OF SULFONATED POLY(ARYL-ETHER-ETHER-KETONE) (PEEK) - PREPARATION AND CHARACTERIZATION [J].
BAILLY, C ;
WILLIAMS, DJ ;
KARASZ, FE ;
MACKNIGHT, WJ .
POLYMER, 1987, 28 (06) :1009-1016
[3]  
Beerlage M. A. M., 1994, Polyimide Ultrafiltration Membranes for Non-Aqueous Systems, P211
[4]  
Bishop M.T., 1991, US patent, Patent No. [4,992,485 A, 4992485]
[5]   THE MORPHOLOGY OF POLY(ARYL-ETHER-ETHER-KETONE) [J].
BLUNDELL, DJ ;
OSBORN, BN .
POLYMER, 1983, 24 (08) :953-958
[6]  
Costa LC., 1992, US patent, Patent No. [5,089,192 A, 5089192]
[7]   CHEMICAL MODIFICATION OF POLY(ETHER ETHER KETONE) FOR SIZE-EXCLUSION CHROMATOGRAPHY AT ROOM-TEMPERATURE .2. ON THE RELIABILITY OF THE DERIVATIZATION PROCEDURE FOR PEEK MOLECULAR-MASS DETERMINATION-APPLICATION TO PEEK-CARBON FIBER-COMPOSITE [J].
DAOUST, D ;
GODARD, P ;
DEVAUX, J ;
LEGRAS, R ;
STRAZIELLE, C .
POLYMER, 1994, 35 (25) :5498-5503
[8]   CHEMICAL MODIFICATION OF POLY(ETHER ETHER KETONE) FOR SIZE-EXCLUSION CHROMATOGRAPHY AT ROOM-TEMPERATURE .1. ABSOLUTE MOLECULAR-MASS DETERMINATION FOR SULFONATED PEEK [J].
DAOUST, D ;
GODARD, P ;
DEVAUX, J ;
LEGRAS, R ;
STRAZIELLE, C .
POLYMER, 1994, 35 (25) :5491-5497
[9]   ON THE MOLECULAR-WEIGHT DETERMINATION OF A POLY(ARYL-ETHER-ETHER-KETONE) (PEEK) [J].
DEVAUX, J ;
DELIMOY, D ;
DAOUST, D ;
LEGRAS, R ;
MERCIER, JP ;
STRAZIELLE, C ;
NIELD, E .
POLYMER, 1985, 26 (13) :1994-2000
[10]   Synthesis and Characterization of Poly(ether ether ketone) Derivatives Obtained by Carbonyl Reduction [J].
Diez-Pascual, Ana M. ;
Martinez, Gerardo ;
Gomez, Marian A. .
MACROMOLECULES, 2009, 42 (18) :6885-6892