Influence of strain rate and temperature on the compressive deformation of a eutectic Al-Si alloy based composite reinforced with -Si3N4

被引:0
作者
Feng, AH [1 ]
Geng, L [1 ]
Qu, SJ [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150006, Peoples R China
来源
PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5 | 2005年 / 475-479卷
关键词
Si3N4; whisker; aluminum; hot compressive deformation; Zener-Hollomon parameter;
D O I
10.4028/www.scientific.net/MSF.475-479.885
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The compressive properties characterized as a function of the true stress-strain response of alpha-Si3N4 whisker reinforced 4032 aluminum alloy composite were examined at strain rates ranging from 10(-3) to 10(0)s(-1) in the temperature interval 500 similar to 620 degrees C. The effect of compressive deformation parameters such as strain rate and temperature on the mechanical behavior was systematically investigated. The strain rate sensitivity exponent and activation energy were calculated. The activation energy is 126 KJmol(-1) at 500 degrees C to 540 degrees C, close to that for lattice self-diffusion in aluminum (142KJmol(-1)), and is 210 KJmol(-1) at 540 degrees C to 580 degrees C (epsilon =0.37s(-1)). The compressive deformation behavior of the composite can be described quantified by the Zener-Hollomon parameters (Z) for the solid state and the Non Newton-fluid for the semi-solid state of the composite. It is demonstrated that a linear equation of the logarithmic Z fits the flow stress of the composite at elevated temperatures. The compressive deformation mechanisms of the alpha-Si(3)N(4)w/4032Al composite were discussed preliminarily.
引用
收藏
页码:885 / 888
页数:4
相关论文
共 10 条
  • [1] High temperature mechanical behavior and microstructure of α-Si3N4w/4032Al composite fabricated by squeeze casting
    Feng, AH
    Geng, L
    Wang, GS
    [J]. COMPOSITE MATERIALS III, 2003, 249 : 239 - 243
  • [2] FENG AH, UNPUB J MAT PROCESSI
  • [3] EFFECT OF LIQUID-PHASES ON THE TENSILE ELONGATION OF SUPERPLASTIC ALUMINUM-ALLOYS AND COMPOSITES
    HIGASHI, K
    NIEH, TG
    MABUCHI, M
    WADSWORTH, J
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (07): : 1079 - 1084
  • [4] Effects of addition of magnesium on interface structure and high-strain-rate superplasticity in Si3N4-reinforced Al-alloy composites
    Jeong, HG
    Hiraga, K
    Mabuchi, M
    Higashi, K
    [J]. ACTA MATERIALIA, 1998, 46 (17) : 6009 - 6020
  • [5] Superplastic deformation behaviour of friction stir processed 7075Al alloy
    Ma, ZY
    Mishra, RS
    Mahoney, MW
    [J]. ACTA MATERIALIA, 2002, 50 (17) : 4419 - 4430
  • [6] An experimental investigation of a superplastic constitutive equation in Al-Mg-Si alloy composites reinforced with Si3N4 whiskers
    Mabuchi, M
    Higashi, K
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 2001, 17 (03) : 399 - 407
  • [7] Activation energy for superplastic flow in aluminum matrix composites exhibiting high-strain-rate superplasticity
    Mabuchi, M
    Higashi, K
    [J]. SCRIPTA MATERIALIA, 1996, 34 (12) : 1893 - 1897
  • [8] Microstructural modeling of metadynamic recrystallization in hot working of IN 718 superalloy
    Medeiros, SC
    Prasad, YVRK
    Frazier, WG
    Srinivasan, R
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 293 (1-2): : 198 - 207
  • [9] A RHEOLOGICAL VIEW OF HIGH-STRAIN-RATE SUPERPLASTICITY IN ALLOYS AND METAL-MATRIX COMPOSITES
    NIEH, TG
    WADSWORTH, J
    IMAI, T
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (05): : 703 - 708
  • [10] On the mechanical behavior of commercial-purity aluminum deformed under axisymmetric compression conditions
    Puchi, ES
    Staia, MH
    Villalobos, C
    [J]. INTERNATIONAL JOURNAL OF PLASTICITY, 1997, 13 (8-9) : 723 - 742