Core loss of ultra-rapidly annealed Fe-rich nanocrystalline soft magnetic alloys

被引:41
作者
Parsons, R. [1 ]
Zang, B. [1 ]
Onodera, K. [2 ]
Kishimoto, H. [2 ]
Shoji, T. [2 ]
Kato, A. [2 ]
Suzuki, K. [1 ]
机构
[1] Monash Univ, Dept Mat Sci & Engn, Clayton, Vic 3800, Australia
[2] Toyota Motor Co Ltd, Susono, Shizuoka 4101193, Japan
基金
澳大利亚研究理事会;
关键词
Rapid annealing; Core loss; Anomaly factor; HiB-nanoperm; Soft magnetic materials; Nanocrystalline; HIGH SATURATION MAGNETIZATION; ZR-B; CRYSTALLIZATION; MICROSTRUCTURE;
D O I
10.1016/j.jmmm.2018.12.053
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ultra-rapidly annealed (heating rate > 10(4) K/s, annealing time < 1 s) Fe-rich nanocrystalline soft magnetic materials with a nominal composition of Fe100-xBx and Fe87-yB13My where x = 12, 13, 14, y = 1, 2 and M = Cu, Ni (HiB-Nanoperm) have recently been demonstrated with a saturation magnetic polarization (J(s)) up to 1.92 T and a low coercivity (H-c) of less than 8 A/m. In this study the AC core loss (P-cm) is estimated for HiB-Nanoperm at 50, 400 and 1000 Hz and is compared with existing amorphous, nanocrystalline and conventionally crystalline (Fe-Si) materials. The P-cm of HiB-Nanoperm at 1.5 T, 50 Hz is demonstrated to be 5-15% that of Fe-3 wt% Si. In specific, Fe86B13Cu1 displays losses that are 30% that of Fe-6.5 wt% Si steel while also possessing a 5% larger J(s). For maximum magnetic polarization (J(m)) values greater than 1.5 T this same composition also exhibits some of the lowest core losses seen from all Fe-based nanocrystalline alloys across the frequencies tested in this study. Core loss separation and an estimation of the anomaly factor (eta) for selected HiB-Nanoperm alloys is also undertaken and compared with a Fe-based amorphous alloy. The eta of HiB-Nanoperm is seen to be lower than that of Fe-based amorphous alloy and is also observed to be positively correlated with saturation magnetostriction. The low core loss of HiB-Nanoperm is attributed to a reduced anomalous loss which may be brought about by the moderate magnetostriction of this alloy.
引用
收藏
页码:142 / 148
页数:7
相关论文
共 33 条
[1]  
HASEGAWA R, 1978, J APPL PHYS, V49, P4174, DOI 10.1063/1.325328
[2]   SOFT-MAGNETIC NANOCRYSTALLINE MATERIALS [J].
HERZER, G .
SCRIPTA METALLURGICA ET MATERIALIA, 1995, 33 (10-11) :1741-1756
[3]   GRAIN-STRUCTURE AND MAGNETISM OF NANOCRYSTALLINE FERROMAGNETS [J].
HERZER, G .
IEEE TRANSACTIONS ON MAGNETICS, 1989, 25 (05) :3327-3329
[4]  
HERZER G, 1994, J MAGN MAGN MATER, V133, P250
[5]   Temperature dependence of refractive index and electronic polarizability of KNbGeO5 glass and its nanocrystallized glasses [J].
Honma, Tsuyoshi ;
Ito, Noriko ;
Dimitrov, Vesselin ;
Komatsu, Takayuki .
JOURNAL OF APPLIED PHYSICS, 2009, 105 (05)
[6]   THE MICROSTRUCTURE EVOLUTION OF A FE73.5SI13.5B9NB3CU1 NANOCRYSTALLINE SOFT MAGNETIC MATERIAL [J].
HONO, K ;
HIRAGA, K ;
WANG, Q ;
INOUE, A ;
SAKURAI, T .
ACTA METALLURGICA ET MATERIALIA, 1992, 40 (09) :2137-2147
[7]   Electron confinement and heating in microwave-sustained argon microplasmas [J].
Hoskinson, Alan R. ;
Gregorio, Jose ;
Parsons, Stephen ;
Hopwood, Jeffrey .
JOURNAL OF APPLIED PHYSICS, 2015, 117 (16)
[8]   MAGNETOSTRICTION AND MAGNETIC CORE LOSS AT HIGH-FREQUENCY IN AMORPHOUS FE-NB-SI-B ALLOYS [J].
INOMATA, K ;
HASEGAWA, M ;
KOBAYASHI, T ;
SAWA, T .
JOURNAL OF APPLIED PHYSICS, 1983, 54 (11) :6553-6557
[9]  
JFE, 2016, JFE STEEL CORPORATIO
[10]   CRYSTALLIZATION OF HIGHLY UNDERCOOLED METALLIC MELTS AND METALLIC GLASSES AROUND THE GLASS-TRANSITION TEMPERATURE [J].
KOSTER, U ;
MEINHARDT, J .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 178 (1-2) :271-278