Wear resistance of Polymethyl Methacrylate (PMMA) with the Addition of Bone Ash, Hydroxylapatite and Keratin

被引:5
作者
Emre, G. [1 ]
Akkus, A. [1 ]
Karamis, M. B. [2 ]
机构
[1] Cumhuriyet Univ, Dept Railway Syst, TR-58140 Sivas, Turkey
[2] Erciyes Univ, Dept Mech Engn, TR-38039 Kayseri, Turkey
来源
9TH INTERNATIONAL CONFERENCE ON TRIBOLOGY (BALKANTRIB'17) | 2018年 / 295卷
关键词
Polymethyl Methacrylate (PMMA); Bone Ash; Hydroxylapatite; Keratin; Wear Resistance;
D O I
10.1088/1757-899X/295/1/012004
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study mechanichal and tribological properties of keratin, bone ash and hydroxylapatite by adding to PMMA (known as the main prosthesis material) were investigated. Hydroxylapatite, bone ash, and keratin materials were added as PMMA in to the content of PMMA, in the proportions of %1, %3 and %5, respectively. The resulting mixtures were put into the molds and solidified in order to obtain samples to be used in the wear experiments. Each experiment was conducted by preparing three experimental samples. The wear data were compared according to the average values of the experimental samples. In the wear test, the results were also evaluated according to the average values obtained from each group and the results of the control group. It was observed that, the wear resistance of the PMMA including 3%, 5% bone ash and PMMA including 5% keratin flour were higher than the values of the control group.
引用
收藏
页数:8
相关论文
共 11 条
[1]  
[Anonymous], 1977, J Am Dent Assoc, V95, P991
[2]  
Calikkocaoglu S., 1998, PROTEZ AKAD GNATOLOJ, V2
[3]  
Crosa G., 1993, TRIBOLOGY POLYM COMP
[4]  
Frederick A., 2002, RUEGGEBERG, V87, P364
[5]  
Gur A.K., 2004, DOGU ANADOLU BOLGESI, P106
[6]  
Ozdemir A.K., 2002, CUMHURIYET U YAYINLA, V1
[7]  
Phoenix R D, 1996, Dent Clin North Am, V40, P113
[8]  
Polat T., 2002, CUMHURIYET U DISHEKI, V5, P41
[9]  
Sahin O., 2010, FARKLI POLIMERIZASYO
[10]  
Sarsilmaz F, 2003, DOGU ANADOLU BOLGESI, V3, P117